# US 2025/0149348 A1 · Method for reducing warpage occurred to substrate during packaging process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149348 A1
- Document ID: US20250149348A1
- Status: Published application
- Kind: A1
- Application number: 18/405,740
- Filed: 2024-01-05
- Published: 2025-05-08
- Earliest claimed: 2023-11-08
- Assignees: Tong Hsing Electronic Industries, Ltd.
- Applicants: Tong Hsing Electronic Industries, Ltd.
- Inventors: Yu-Hsiang Liu; Li-Chun Hung
- Web page: https://patentgrep.com/patent/US20250149348A1

## CPC

- H10W 74/016: {using moulds}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10W 42/121: {protecting against mechanical damage (H10W76/00, H10W74/00 take precedence)}
- H10W 74/014: {using batch processing}
- H10W 74/114: {by a substrate and the encapsulations}
- H10W 90/00: Package configurations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for reducing warpage occurred to a substrate during a packaging process includes attaching a plurality of dies to an upper surface of the substrate; attaching an adhesive material having a first curing temperature to a lower surface of the substrate; applying a liquid-packaging material having a second curing temperature to surroundings of the dies; heating the substrate, the adhesive material, and the liquid-packaging material to a heating temperature not less than the first curing temperature and the second curing temperature; and cooling the substrate, the adhesive material, and the liquid-packaging material to a room temperature. When being cooled to the room temperature, the liquid-packaging material applies an upper-surface shrinkage stress to the upper surface of the substrate, the adhesive material applies a lower-surface shrinkage stress to the lower surface of the substrate, and the lower-surface shrinkage stress is substantially equal to the upper-surface shrinkage stress.

## Claims

### Claim 1

A method for reducing warpage occurred to a substrate during a packaging process, comprising:
attaching a plurality of dies to an upper surface of the substrate;
attaching an adhesive material to a lower surface of the substrate, wherein the adhesive material has a first curing temperature;
applying a liquid-packaging material to surroundings of the dies, wherein the liquid-packaging material has a second curing temperature;
heating the substrate, the adhesive material, and the liquid-packaging material to a heating temperature not less than the first curing temperature and the second curing temperature; and
cooling the substrate, the adhesive material, and the liquid-packaging material to a room temperature;
wherein when being cooled to the room temperature, the liquid-packaging material applies an upper-surface shrinkage stress to the upper surface of the substrate, the adhesive material applies a lower-surface shrinkage stress to the lower surface of the substrate, and the lower-surface shrinkage stress is substantially equal to the upper-surface shrinkage stress.

### Claim 2 (depends on 1)

The method according to claim 1, wherein after cooling the substrate, the adhesive material, and the liquid-packaging material to the room temperature, the method further comprises:
removing the adhesive material.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the adhesive material is removed through hydrolysis and/or pyrolysis.

### Claim 4 (depends on 2)

The method according to claim 2, wherein after removing the adhesive material, the method further comprises:
cutting the substrate to separate the dies from each other.

### Claim 5 (depends on 1)

The method according to claim 1, wherein after cooling the substrate, the adhesive material, and the liquid-packaging material to the room temperature, the method further comprises:
cutting the substrate along a cutting line to separate the dies from each other.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the adhesive material is attached to the cutting line, the adhesive material has an adhesive-material width, and the cutting line has a cutting-line width substantially equal to the adhesive-material width to remove the adhesive material through cutting the substrate along the cutting line.

### Claim 7

A method for reducing warpage occurred to a substrate during a packaging process, comprising:
attaching a plurality of dies to an upper surface of the substrate;
attaching an adhesive material to a lower surface of the substrate, wherein the adhesive material has a first curing temperature;
heating a molding material to a molding temperature and applying the molding material to surroundings of the dies, wherein the molding material has a third curing temperature;
heating the substrate, the adhesive material, and the molding material to a heating temperature not less than the first curing temperature and the third curing temperature; and
cooling the substrate, the adhesive material, and the molding material to a room temperature;
wherein when being cooled to the room temperature, the molding material applies an upper-surface shrinkage stress to the upper surface of the substrate, the adhesive material applies a lower-surface shrinkage stress to the lower surface of the substrate, and the lower-surface shrinkage stress is substantially equal to the upper-surface shrinkage stress.

### Claim 8 (depends on 7)

The method according to claim 7, wherein after cooling the substrate, the adhesive material, and the molding material to the room temperature, the method further comprises:
removing the adhesive material.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the adhesive material is removed through hydrolysis and/or pyrolysis.

### Claim 10 (depends on 8)

The method according to claim 8, wherein after removing the adhesive material, the method further comprises:
cutting the substrate to separate the dies from each other.

### Claim 11 (depends on 7)

The method according to claim 7, wherein after cooling the substrate, the adhesive material, and the molding material to the room temperature, the method further comprises:
cutting the substrate along a cutting line to separate the dies from each other.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the adhesive material is attached to the cutting line, the adhesive material has an adhesive-material width, and the cutting line has a cutting-line width substantially equal to the adhesive-material width to remove the adhesive material through cutting the substrate along the cutting line.