# US 2025/0149337 A1 · High selectivity cryogenic tungsten-boron-carbide etch

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149337 A1
- Document ID: US20250149337A1
- Status: Published application
- Kind: A1
- Application number: 18/913,143
- Filed: 2024-10-11
- Published: 2025-05-08
- Earliest claimed: 2023-11-07
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Jing ZHANG; Gene LEE; Kenji TAKESHITA; Anatoli CHLENOV
- Web page: https://patentgrep.com/patent/US20250149337A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 50/283: {by chemical means}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of selectively etching a hardmask layer formed on a device substrate. The method includes supplying an etching gas mixture to a process region of a processing chamber, where a device substrate is disposed in the process region when the etching gas mixture is supplied to the process region, where the device substrate may include a substrate, at least one cavity formed in the substrate, and a hardmask layer formed over the at least one cavity and over the substrate. The method also includes providing radio frequency (rf) power to the etching gas mixture to form a plasma in the process region.

## Claims

### Claim 1

A method of selectively etching a hardmask layer formed on a device substrate, comprising:
supplying an etching gas mixture to a process region of a processing chamber, wherein
a device substrate is disposed in the process region when the etching gas mixture is supplied to the process region, wherein
the device substrate comprises:
a substrate,
at least one cavity formed in the substrate, and
a hardmask layer formed over the at least one cavity and over the substrate; and
the etching gas mixture comprises at least a fluorine-containing gas and a hydrogen-containing gas;
maintaining the device substrate at a cryogenic temperature;
delivering radio frequency (RF) power to the etching gas mixture to form a plasma in the process region; and
selectively etching exposed portions of the hardmask layer relative to the substrate at a ratio greater than 10:1 while in a presence of the plasma.

### Claim 2 (depends on 1)

The method of claim 1, wherein the substrate is further comprised of silicon dioxide.

### Claim 3 (depends on 1)

The method of claim 1, wherein the etching gas mixture has a ratio of the fluorine-containing gas to the hydrogen-containing gas between about 5:1 to about 1:5.

### Claim 4 (depends on 3)

The method of claim 3, wherein the fluorine-containing gas is nitrogen trifluoride (NF3).

### Claim 5 (depends on 3)

The method of claim 3, wherein the hydrogen-containing gas is a diatomic hydrogen (H2).

### Claim 6 (depends on 1)

The method of claim 1, wherein the hardmask layer is deposited by chemical vapor deposition.

### Claim 7 (depends on 1)

The method of claim 1, wherein the hardmask layer comprises a tungsten-boron-carbide (WBC) material, wherein the WBC material further comprises at least tungsten, boron, and carbon.

### Claim 8 (depends on 7)

The method of claim 7, wherein tungsten comprises between about 50% to about 90% of the WBC material by weight.

### Claim 9 (depends on 7)

The method of claim 7, wherein the percentage of boron is between about 5% to about 20% of the WBC material by weight.

### Claim 10 (depends on 7)

The method of claim 7, wherein the percentage of carbon is between about 5% to about 30% of the WBC material by weight.

### Claim 11 (depends on 1)

The method of claim 1, wherein the hardmask layer comprises a tungsten containing material, wherein the tungsten containing material includes a percentage of tungsten greater than about 50% by weight.

### Claim 12 (depends on 1)

The method of claim 1, wherein maintaining the device substrate at the cryogenic temperature further comprises:
maintaining the device substrate between about −10° C. to about −200° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein etching exposed portions of the hardmask layer further comprises:
exposing at least a portion of the cavity through the hardmask layer.

### Claim 14 (depends on 1)

The method of claim 1, wherein providing radio frequency (RF) power to the etching gas mixture further comprises:
inductively coupling the RF power to the etching gas mixture.

### Claim 15 (depends on 1)

The method of claim 1, wherein selectively etching exposed portions of the hardmask layer relative to the substrate reduces the throughput of the etch process.