# US 2025/0149334 A1 · Lattice polarity control in iii-nitride semiconductor heterostructures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149334 A1
- Document ID: US20250149334A1
- Status: Published application
- Kind: A1
- Application number: 18/837,812
- Filed: 2023-02-13
- Published: 2025-05-08
- Earliest claimed: 2022-02-11
- Assignees: The Regents of the University of Michigan
- Applicants: The Regents of the University of Michigan
- Inventors: Ping Wang; Ding Wang; Zetian Mi
- Web page: https://patentgrep.com/patent/US20250149334A1

## CPC

- H10P 14/3216: {Nitrides}
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 29/403: {AIII-nitrides}
- C30B 29/406: {Gallium nitride}
- C30B 29/68: Crystals with laminate structure, e.g. "superlattices"
- H10D 30/472: {having lower bandgap active layer formed on top of wider bandgap layer, e.g. inverted HEMT}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3202: {Materials thereof}
- H10P 14/3416: {Nitrides}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of fabricating a heterostructure includes growing epitaxially, in a growth chamber, a first semiconductor layer of the heterostructure, the first semiconductor layer including a first III-nitride semiconductor material, the first semiconductor layer being supported by a substrate, after growing the first semiconductor layer, growing epitaxially, in the growth chamber, a second semiconductor layer of the heterostructure such that the second semiconductor layer is supported by the first semiconductor layer, the second semiconductor layer including a second III-nitride semiconductor material, and between growing the first semiconductor layer and growing the second semiconductor layer, controlling an extent to which a eutectic layer disposed on the first semiconductor layer is consumed to control a lattice polarity of the second semiconductor layer

## Claims

### Claim 1

A method of fabricating a heterostructure, the method comprising:
growing epitaxially, in a growth chamber, a first semiconductor layer of the heterostructure, the first semiconductor layer comprising a first III-nitride semiconductor material, the first semiconductor layer being supported by a substrate;
after growing the first semiconductor layer, growing epitaxially, in the growth chamber, a second semiconductor layer of the heterostructure such that the second semiconductor layer is supported by the first semiconductor layer, the second semiconductor layer comprising a second III-nitride semiconductor material; and
between growing the first semiconductor layer and growing the second semiconductor layer, controlling an extent to which a eutectic layer disposed on the first semiconductor layer is consumed to control a lattice polarity of the second semiconductor layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein controlling the extent to which the eutectic layer is consumed controls the lattice polarity of the second semiconductor layer based on whether an intermediate layer is formed from the eutectic material between the first and second semiconductor layers.

### Claim 3 (depends on 2)

The method of claim 2, wherein presence of the intermediate layer between the first and second semiconductor layers toggles the lattice polarity of the second semiconductor layer from a lattice polarity of the first semiconductor layer.

### Claim 4 (depends on 2)

The method of claim 2, wherein absence of the intermediate layer between the first and second semiconductor layers allows a lattice polarity of the first semiconductor layer to persist in the second semiconductor layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the eutectic layer comprises silicon and a Group III cation species of the first III-nitride semiconductor material.

### Claim 6 (depends on 1)

The method of claim 1, wherein:
consumption of the eutectic layer forms an intermediate layer between the first and second semiconductor layers;
the intermediate layer is doped with silicon; and
the intermediate layer establishes an interface between the first and second semiconductor layers.

### Claim 7 (depends on 1)

The method of claim 1, wherein controlling the extent to which the eutectic layer is consumed comprises suppressing consumption of the eutectic layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein suppressing the consumption comprises annealing the first semiconductor layer in an active-nitrogen-free environment.

### Claim 9 (depends on 8)

The method of claim 8, wherein annealing the first semiconductor layer is implemented without flux of a Group III cation species.

### Claim 10 (depends on 7)

The method of claim 7, wherein the first and second semiconductor layers are nitrogen polar.

### Claim 11 (depends on 1)

The method of claim 1, wherein controlling the extent to which the eutectic layer is consumed comprises facilitating consumption of the eutectic layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein facilitating consumption of the eutectic layer comprises:
exposing the eutectic layer to an active nitrogen environment; and
growing the second semiconductor layer in a nitrogen-rich environment.

### Claim 13 (depends on 11)

The method of claim 11, wherein one of the first and second semiconductor layers is nitrogen polar, and the other of the first and second semiconductor layers is metal polar.

### Claim 14 (depends on 1)

The method of claim 1, further comprising forming the eutectic layer on a surface of the substrate before growing the first semiconductor layer.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
forming a further eutectic layer on a surface of the second semiconductor layer;
growing epitaxially, in the growth chamber, a III-nitride semiconductor layer of the heterostructure such that the III-nitride semiconductor layer is supported by the second semiconductor layer; and
controlling an extent to which the further eutectic layer disposed on the second semiconductor layer is consumed to control a lattice polarity of the III-nitride semiconductor layer supported by the second semiconductor layer.

### Claim 16 (depends on 1)

The method of claim 1, wherein the first semiconductor material is aluminum nitride (AlN).

### Claim 17 (depends on 1)

The method of claim 1, wherein the second semiconductor material is gallium nitride (GaN).

### Claim 18 (depends on 1)

The method of claim 1, wherein the substrate comprises silicon such that the eutectic layer comprises silicon.

### Claim 19 (depends on 1)

The method of claim 1, wherein growing epitaxially the first semiconductor layer is implemented in a metal-rich environment.

### Claim 20 (depends on 1)

The method of claim 1, wherein growing epitaxially the second semiconductor layer is implemented in a metal-rich environment.

### Claim 21 (depends on 1)

The method of claim 1, wherein growing the second semiconductor layer is implemented without removal of the substrate from the growth chamber after growth of the first semiconductor layer.

### Claim 22

A method of fabricating a heterostructure, the method comprising:
growing epitaxially a first semiconductor layer of the heterostructure, the first semiconductor layer comprising a first III-nitride semiconductor material, the first semiconductor layer being supported by a substrate;
growing epitaxially a second semiconductor layer of the heterostructure such that the second semiconductor layer is supported by the first semiconductor layer, the second semiconductor layer comprising a second III-nitride semiconductor material; and
between growing the first semiconductor layer and growing the second semiconductor layer, annealing the first semiconductor layer in an active nitrogen-free environment to evaporate Group IIIA metal atoms of a eutectic layer disposed on the first semiconductor layer to maintain a lattice polarity of the first semiconductor layer in the second semiconductor layer.

### Claim 23

A method of fabricating a heterostructure, the method comprising:
growing epitaxially a first semiconductor layer of the heterostructure, the first semiconductor layer comprising a first III-nitride semiconductor material, the first semiconductor layer being supported by a substrate;
growing epitaxially a second semiconductor layer of the heterostructure such that the second semiconductor layer is supported by the first semiconductor layer, the second semiconductor layer comprising a second III-nitride semiconductor material; and
between growing the first semiconductor layer and growing the second semiconductor layer, exposing an incidental eutectic coating on the first semiconductor layer to an active nitrogen environment, the incidental eutectic coating comprising silicon and a cation species of the first III-nitride semiconductor material;
wherein growing the second semiconductor layer is implemented in a nitrogen-rich environment such that exposing the incidental eutectic coating forms an intermediate layer at an interface between the first and second semiconductor layers from the incidental eutectic coating such that a lattice polarity of the second semiconductor layer is toggled relative to the first semiconductor layer.

### Claim 24

A device comprising:
a substrate; and
a semiconductor heterostructure supported by the substrate, the semiconductor heterostructure comprising:
a first semiconductor layer supported by the substrate and comprising a first III-nitride semiconductor material; and
a second semiconductor layer supported by, and in contact with, the first semiconductor layer and comprising a second III-nitride semiconductor material differing from the first III-nitride semiconductor material;
wherein the first and second semiconductor layers are nitrogen polar.

### Claim 25 (depends on 24)

The device of claim 24, wherein:
the first semiconductor material is aluminum nitride (AlN);
the second semiconductor material is gallium nitride (GaN); and
the substrate comprises silicon.

### Claim 26 (depends on 24)

The device of claim 24, wherein:
the first semiconductor layer is configured as a buffer layer of a transistor device; and
the second semiconductor layer is configured as a channel layer of the transistor device.

### Claim 27 (depends on 26)

The device of claim 26, wherein the semiconductor heterostructure further comprises a barrier layer supported by the buffer layer and comprising a compound semiconductor material, wherein the barrier layer is nitrogen polar.

### Claim 28

A device comprising:
a substrate; and
a semiconductor heterostructure supported by the substrate;
wherein:
the semiconductor heterostructure comprises a plurality of III-nitride semiconductor layers supported by the substrate;
the semiconductor heterostructure further comprises a plurality of intermediate layers, each intermediate layer of the plurality of intermediate layers being disposed between a respective pair of adjacent III-nitride semiconductor layers of the plurality of III-nitride semiconductor layers;
each intermediate layer of the plurality of intermediate layers comprises silicon; and
the adjacent III-nitride semiconductor layers of each pair of adjacent III-nitride semiconductor layers of the plurality of III-nitride semiconductor layers have different lattice polarities.

### Claim 29 (depends on 28)

The device of claim 28, wherein:
each intermediate layer of the plurality of intermediate layers comprises a doped crystalline material; and
the doped crystalline layer is doped with silicon.

### Claim 30 (depends on 28)

The device of claim 28, wherein each intermediate layer of the plurality of intermediate layers comprises AlSiN.

### Claim 31 (depends on 28)

The device of claim 28, wherein each semiconductor layer the plurality of semiconductor layers is composed of a same III-nitride semiconductor material.

### Claim 32 (depends on 28)

The device of claim 28, wherein at least two of the plurality of semiconductor layers are composed of different III-nitride semiconductor materials.

### Claim 33

A device comprising:
a substrate; and
a semiconductor heterostructure supported by the substrate;
wherein:
the semiconductor heterostructure comprises a plurality of III-nitride semiconductor layers supported by the substrate; and
a first III-nitride semiconductor layer of the plurality of III-nitride semiconductor layers comprises:
a first section having a first lattice polarity; and
a second section laterally adjacent to the first section and having a second lattice polarity differing from the first lattice polarity.

### Claim 34 (depends on 33)

The device of claim 33, wherein:
the plurality of III-nitride semiconductor layers comprises a second III-nitride semiconductor layer supported by the first III-nitride semiconductor layer;
the first and second III-nitride semiconductor layers have different compositions;
the second III-nitride semiconductor layer comprises first and second sections supported by the first and second sections of the first III-nitride semiconductor layer, respectively, and having the first and second lattice polarities, respectively.

### Claim 35 (depends on 33)

The device of claim 33, wherein:
the first III-nitride semiconductor layer comprises a set of N-polar sections and a set of metal-polar sections; and
the set of N-polar sections and the set of metal-polar sections are disposed in a periodic, alternating arrangement.