# US 2025/0149255 A1 · Solid electrolyte capacitor and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149255 A1
- Document ID: US20250149255A1
- Status: Published application
- Kind: A1
- Application number: 18/695,019
- Filed: 2022-09-29
- Published: 2025-05-08
- Earliest claimed: 2021-09-30
- Assignees: Nippon Chemi-Con Corporation
- Applicants: Nippon Chemi-Con Corporation
- Inventors: Atsushi TANAKA; Toshiki WAKABAYASHI; Tomoyuki GOUTSU; Kyohei YOSHIOKA; Kenji MACHIDA; Nozomu KAMIYAMA; Kazuya KOSEKI; Kazuhiro NAGAHARA; Kenta SATO
- Web page: https://patentgrep.com/patent/US20250149255A1

## CPC

- H01G 9/055: Etched foil electrodes
- H01G 9/0032: {formation of the dielectric layer}
- H01G 9/0036: {Formation of the solid electrolyte layer}
- H01G 9/028: Organic semiconducting electrolytes, e.g. TCNQ
- H01G 9/07: Dielectric layers
- H01G 9/15: Solid electrolytic capacitors (H01G11/00 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A solid electrolytic capacitor that exhibits both high withstand voltage and large capacity and a manufacturing method of the solid electrolytic capacitor are provided. The solid electrolytic capacitor includes anode foil, cathode foil facing the anode foil, and conductive polymers intervening between the anode foil and the cathode foil. The anode foil has tunnel-shaped etching pits formed on a surface layer of the anode foil, a dielectric oxide film layer formed on the surface layer of the anode foil, and a pseudo boehmite layer on the dielectric oxide film layer and formed on the surface layer of the anode foil. An amount of the pseudo boehmite layer is adjusted to be 0.4 mg·cm−2 to 1.8 mg·cm−2.

## Claims

### Claim 1

A solid electrolytic capacitor comprising:
anode foil;
a cathode body facing the anode foil; and
a conductive polymer layer intervening between the anode foil and the cathode body,
wherein:
the anode foil has tunnel-shaped etching pits formed on a surface layer of the anode foil, a dielectric oxide film layer formed on the surface layer of the anode foil, and a pseudo boehmite layer on the dielectric oxide film layer and formed on the surface layer of the anode foil, and
an amount of the pseudo boehmite layer is 0.4 mg·cm−2 to 1.8 mg·cm−2.

### Claim 2 (depends on 1)

The solid electrolytic capacitor according to claim 1, wherein the conductive polymer layer is formed by conductive polymer solution including the conductive polymer.

### Claim 3 (depends on 2)

The solid electrolytic capacitor according to claim 2, wherein the conductive polymer layer includes the conductive polymer, a solvent of the conductive polymer solution that disperses or dissolves the conductive polymer, and an additive to which the conductive polymer is added.

### Claim 4 (depends on 1)

The solid electrolytic capacitor according to claim 1, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein a weight of the conductive polymer layer is 30 mg·cm−3 to 250 mg·cm−3 per unit volume of the capacitor element.

### Claim 5 (depends on 1)

The solid electrolytic capacitor according to claim 1, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein a weight of the conductive polymer layer may be 120 mg·cm−3 to 150 mg·cm−3 per unit volume of the capacitor element.

### Claim 6 (depends on 1)

The solid electrolytic capacitor according to claim 1, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein the conductive polymer is included in a ratio of 11 mg·cm−3 per unit volume of the capacitor element.

### Claim 7 (depends on 1)

The solid electrolytic capacitor according to claim 1, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein the conductive polymer is included in a ratio of 6.2 mg·cm−3 to 9.0 mg·cm−3 per unit volume of the capacitor element.

### Claim 8 (depends on 1)

The solid electrolytic capacitor according to claim 1, further comprising electrolytic solution between the anode foil and the cathode body.

### Claim 9

A manufacturing method of a solid electrolytic capacitor comprising:
an anode foil formation process of forming anode foil; and
a conductive polymer layer formation process of forming a conductive polymer layer between the anode foil and a cathode body,
wherein:
the anode foil formation process includes an enlargement process of forming tunnel-shaped etching pits on a surface layer of the anode foil, and a chemical treatment process of forming a dielectric oxide film layer on a surface layer of the anode foil and a pseudo boehmite layer on the dielectric oxide film layer,
in the chemical treatment process, an amount of the pseudo boehmite layer is adjusted to 0.4 mg·cm−2 to 1.8 mg·cm−2, and
in the conductive polymer layer formation process, conductive polymer solution including the conductive polymer is attached to at least the anode foil.

### Claim 10 (depends on 9)

The manufacturing method of the solid electrolytic capacitor according to claim 9, wherein:
the capacitor element is formed from the anode foil, the cathode body, and the conductive polymer layer, and
in the conductive polymer formation process, the conductive polymer layer may be formed so that a weight of the conductive polymer is 30 mg·cm−3 to 250 mg·cm−3 per unit volume of the capacitor element.

### Claim 11 (depends on 9)

The manufacturing method of the solid electrolytic capacitor according to claim 9, wherein:
the capacitor element is formed from the anode foil, the cathode body, and the conductive polymer layer, and
in the conductive polymer formation process, the conductive polymer layer may be formed to so that the conductive polymer is included in a ratio of 11 mg·cm−3 per unit volume of the capacitor element.

### Claim 12 (depends on 9)

The manufacturing method of the solid electrolytic capacitor according to claim 9, wherein after the conductive polymer formation process, the electrolytic solution is impregnated between the anode foil and the cathode body.

### Claim 13 (depends on 2)

The solid electrolytic capacitor according to claim 2, further comprising electrolytic solution between the anode foil and the cathode body.

### Claim 14 (depends on 3)

The solid electrolytic capacitor according to claim 3, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein a weight of the conductive polymer layer is 30 mg·cm−3 to 250 mg·cm−3 per unit volume of the capacitor element.

### Claim 15 (depends on 3)

The solid electrolytic capacitor according to claim 3, further comprising a capacitor element having the anode foil, the cathode body, and the conductive polymer layer,
wherein the conductive polymer is included in a ratio of 11 mg·cm−3 per unit volume of the capacitor element.

### Claim 16 (depends on 3)

The solid electrolytic capacitor according to claim 3, further comprising electrolytic solution between the anode foil and the cathode body.

### Claim 17 (depends on 14)

The solid electrolytic capacitor according to claim 14, further comprising electrolytic solution between the anode foil and the cathode body.

### Claim 18 (depends on 15)

The solid electrolytic capacitor according to claim 15, further comprising electrolytic solution between the anode foil and the cathode body.

### Claim 19 (depends on 11)

The manufacturing method of the solid electrolytic capacitor according to claim 11, wherein after the conductive polymer formation process, the electrolytic solution is impregnated between the anode foil and the cathode body.