# US 2025/0149068 A1 · Metal-Containing Structures, and Methods of Treating Metal-Containing Material to Increase Grain Size and/or Reduce Contaminant Concentration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149068 A1
- Document ID: US20250149068A1
- Status: Published application
- Kind: A1
- Application number: 19/018,941
- Filed: 2025-01-13
- Published: 2025-05-08
- Earliest claimed: 2019-09-27
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: John D. Hopkins; Jordan D. Greenlee; Peng Xu
- Web page: https://patentgrep.com/patent/US20250149068A1

## CPC

- G11C 5/063: {Voltage and signal distribution in integrated semi-conductor memory access lines, e.g. word-line, bit-line, cross-over resistance, propagation delay}
- H10D 64/037: {comprising charge-trapping insulators}
- C23C 8/06: using gases (C23C8/36 takes precedence)
- C23C 8/10: Oxidising
- C23C 8/12: using elemental oxygen or ozone
- C23C 8/36: using ionised gases, e.g. ionitriding
- C23C 28/322: {only coatings of metal elements only}
- C23C 28/34: {including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates}
- C23C 28/341: {with at least one carbide layer}
- C23C 28/345: {with at least one oxide layer}
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 41/35: with a cell select transistor, e.g. NAND
- H10B 41/41: of a memory region comprising a cell select transistor, e.g. NAND
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 43/35: with cell select transistors, e.g. NAND
- H10B 43/40: characterised by the peripheral circuit region
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Some embodiments include a method of forming a conductive structure. A metal-containing conductive material is formed over a supporting substrate. A surface of the metal-containing conductive material is exposed to at least one radical form of hydrogen and to at least one oxidant. The exposure alters at least a portion of the metal-containing conductive material to thereby form at least a portion of the conductive structure. Some embodiments include a conductive structure which has a metal-containing conductive material with a first region adjacent to a second region. The first region has a greater concentration of one or both of fluorine and boron relative to the second region.

## Claims

### Claim 1

A method of forming a conductive structure, comprising:
forming a metal-containing conductive material over a supporting substrate, the metal-containing conductive structure comprising at least one metal selected from the group consisting of Co, Mo, Nb, and Al; and
exposing a surface of the metal-containing conductive material to at least one radical form of hydrogen and to at least one oxidant; the exposing altering at least a portion of the metal-containing conductive material to thereby form at least a portion of the conductive structure, the altering comprising one or more of a change in crystallinity of the metal-containing conductive material, an increase in a grain size of the metal-containing conductive material, and a reduction of a concentration of at least one contaminant within the metal-containing conductive material.

### Claim 2 (depends on 1)

The method of claim 1 wherein the altering comprises reduction of a concentration of at least one contaminant within the metal-containing conductive material.

### Claim 3 (depends on 2)

The method of claim 2 wherein said at least one contaminant includes one or more of chlorine, carbon, silicon, germanium, boron, oxygen and fluorine.

### Claim 4 (depends on 2)

The method of claim 2 wherein said at least one contaminant includes fluorine.

### Claim 5 (depends on 2)

The method of claim 2 wherein said at least one contaminant includes boron.

### Claim 6 (depends on 1)

The method of claim 1 wherein the altering comprises a change in crystallinity of the metal-containing conductive material.

### Claim 7 (depends on 1)

The method of claim 1 wherein the altering comprises an increase in a grain size of the metal-containing conductive material.

### Claim 8 (depends on 1)

The method of claim 1 wherein the conductive structure is a bitline.

### Claim 9 (depends on 1)

The method of claim 1 wherein the conductive structure is a wordline.

### Claim 10 (depends on 1)

The method of claim 1 wherein the at least one radical form of hydrogen includes H·.

### Claim 11 (depends on 1)

The method of claim 1 wherein the at least one radical form of hydrogen includes one or more of H·, H2+, and H2−.

### Claim 12 (depends on 1)

The method of claim 1 wherein the at least one radical form of hydrogen is generated by a plasma.

### Claim 13 (depends on 1)

The method of claim 1 wherein the at least one oxidant includes one or both of O2 and O3.

### Claim 14 (depends on 1)

The method of claim 1 wherein the at least one oxidant includes one or more of O2, O3, hydrogen peroxide and perchlorate ion.

### Claim 15 (depends on 1)

The method of claim 1 wherein the exposing is conducted while the surface is at a temperature within a range of from about 100° C. to about 1000° C., and within an ambient which is maintained at a pressure of less than or equal to atmospheric pressure.

### Claim 16 (depends on 1)

The method of claim 1 wherein the conductive material is a first conductive material, and further comprising forming a second conductive material directly against the surface after the exposing.

### Claim 17

A method of forming a conductive structure, comprising:
forming a first metal-containing conductive material over a supporting substrate; and
forming a second metal-containing conductive material directly against a surface of the first metal-containing conductive material; and
exposing a surface of the second conductive material to at least one radical form of hydrogen and to at least one oxidant to alter at least a portion of the second conductive material.

### Claim 18 (depends on 17)

The method of claim 17 wherein the first metal-containing conductive material includes titanium and nitrogen, and wherein the second conductive material comprises tungsten.

### Claim 19 (depends on 17)

The method of claim 17 wherein the first metal-containing conductive material includes one or more of tungsten, titanium, cobalt, nickel, molybdenum, niobium, ruthenium, tantalum, copper and aluminum.

### Claim 20 (depends on 19)

The method of claim 19 wherein the metal-containing conductive material includes one or more non-metal constituents selected from the group consisting of nitrogen, silicon, germanium, boron and carbon.