# US 2025/0147424 A1 · Lithography method for positive tone development

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0147424 A1
- Document ID: US20250147424A1
- Status: Published application
- Kind: A1
- Application number: 19/011,395
- Filed: 2025-01-06
- Published: 2025-05-08
- Earliest claimed: 2018-11-21
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Ming-Hui WENG; Chen-Yu LIU; Cheng-Han WU; Ching-Yu CHANG; Chin-Hsiang LIN
- Web page: https://patentgrep.com/patent/US20250147424A1

## CPC

- G03F 7/40: Treatment after imagewise removal, e.g. baking
- G03F 1/82: Auxiliary processes, e.g. cleaning or inspecting
- G03F 7/30: Imagewise removal using liquid means
- G03F 7/322: {Aqueous alkaline compositions}
- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- G03F 7/70925: {Cleaning, i.e. actively freeing apparatus from pollutants, e.g. using plasma cleaning}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method includes illuminating radiation to a resist layer over a substrate to pattern the resist layer. The patterned resist layer is developed by using a positive tone developer. The patterned resist layer is rinsed using a basic aqueous rinse solution. A pH value of the basic aqueous rinse solution is lower than a pH value of the developer, and a rinse temperature of rinsing the patterned resist layer is in a range of about 20° C. to about 40° C.

## Claims

### Claim 1

A lithography method, comprising:
forming a material layer over a substrate;
forming a resist layer over the material layer;
exposing the resist layer;
developing the resist layer;
rinsing the resist layer using a basic aqueous wetting solution with a pH value greater than 7.5; and
etching the material layer using the resist layer as an etch mask.

### Claim 2 (depends on 1)

The lithography method of claim 1, wherein the pH value of the basic aqueous wetting solution is lower than 12.

### Claim 3 (depends on 1)

The lithography method of claim 1, wherein the pH value of the basic aqueous wetting solution is greater than 8.

### Claim 4 (depends on 1)

The lithography method of claim 1, wherein rinsing the resist layer comprises rinsing the resist layer at a temperature in a range of about 20° C. to about 40° C.

### Claim 5 (depends on 1)

The lithography method of claim 1, wherein rinsing the resist layer comprises rinsing the resist layer for a rinsing time shorter than about 3 minute.

### Claim 6 (depends on 1)

The lithography method of claim 1, wherein rinsing the resist layer comprises rinsing the resist layer for a rinsing time in a range of about 15 seconds to about 120 seconds.

### Claim 7 (depends on 1)

The lithography method of claim 1, wherein the basic aqueous wetting solution comprises a water and a base.

### Claim 8 (depends on 7)

The lithography method of claim 7, wherein the base of the basic aqueous wetting solution has a concentration greater than about 0.2 parts per million (ppm).

### Claim 9 (depends on 7)

The lithography method of claim 7, wherein the base of the basic aqueous wetting solution has a concentration in a range of about 0.2 ppm to about 300 ppm.

### Claim 10

A lithography method, comprising:
forming a material layer over a substrate;
forming a resist layer over the material layer;
exposing the resist layer;
applying a first basic aqueous wetting solution with a pH value greater than 7.5 to the resist layer;
developing the resist layer; and
etching the material layer using the resist layer as an etch mask.

### Claim 11 (depends on 10)

The lithography method of claim 10, wherein the first basic aqueous wetting solution is free from tetramethylammonium hydroxide (TMAH).

### Claim 12 (depends on 10)

The lithography method of claim 10, wherein the first basic aqueous wetting solution has a pH value different from tetramethylammonium hydroxide (TMAH).

### Claim 13 (depends on 10)

The lithography method of claim 10,further comrpising:
after developing the resist layer, rinsing the resist layer using a second basic aqueous wetting solution.

### Claim 14 (depends on 13)

The lithography method of claim 13, wherein the second basic aqueous wetting solution and the first basic aqueous wetting solution have the same composition.

### Claim 15

A lithography method, comprising:
forming a target layer over a substrate;
forming a hard mask over the target layer;
forming a multilayer stack over the hard mask, wherein the multilayer stack comprises a bottom layer, a middle layer over the bottom layer and a resist layer over the middle layer;
exposing the resist layer;
developing the resist layer;
rinsing the resist layer using a basic aqueous wetting solution with a pH value greater than 7.5; and
etching the middle layer of the multilayer stack using the resist layer as an etch mask.

### Claim 16 (depends on 15)

The lithography method of claim 15, further comprising:
after rinsing the resist layer, spin dry the resist layer.

### Claim 17 (depends on 15)

The lithography method of claim 15, wherein the hard mask comprise:
a titanium nitride layer over the target layer; and
a silicon-containing layer over the titanium nitride layer.

### Claim 18 (depends on 15)

The lithography method of claim 15, wherein the pH value of the basic aqueous wetting solution is between 8 and 12.

### Claim 19 (depends on 15)

The lithography method of claim 15, wherein the basic aqueous wetting solution includes a base and a deionized (DI) water.

### Claim 20 (depends on 15)

The lithography method of claim 15, wherein rinsing the resist layer comprises rinsing the resist layer at a temperature in a range of about 20° C. to about 40° C.