# US 2025/0147417 A1 · Method of manufacturing a semiconductor device and pattern formation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0147417 A1
- Document ID: US20250147417A1
- Status: Published application
- Kind: A1
- Application number: 19/005,512
- Filed: 2024-12-30
- Published: 2025-05-08
- Earliest claimed: 2020-07-02
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chih-Cheng LIU; Ming-Hui WENG; Jr-Hung LI; Yahru CHENG; Chi-Ming YANG; Tze-Liang LEE; Ching-Yu CHANG
- Web page: https://patentgrep.com/patent/US20250147417A1

## CPC

- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/56: After-treatment
- G03F 7/167: {from the gas phase, by plasma deposition (G03F7/2035 takes precedence)}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F 7/2004: {characterised by the use of a particular light source, e.g. fluorescent lamps or deep UV light}
- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- H10P 76/2041: {Photolithographic processes}
- H10P 76/40: of masks comprising inorganic materials
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device includes forming a photoresist layer over a substrate. A first precursor and a second precursor are combined. The first precursor is an organometallic having a formula: MaRbXc, where M is one or more of Sn, Bi, Sb, In, and Te, R is one or more of a C7-C11 aralkyl group, a C3-C10 cycloalkyl group, a C2-C10 alkoxy group, and a C2-C10 alkylamino group, X is one or more of a halogen, a sulfonate group, and an alkylamino group, and 1≤a≤2, b≥1, c≥1, and b+c≤4, and the second precursor is one or more of water, an amine, a borane, and a phosphine. The photoresist layer is selectively exposed to actinic radiation to form a latent pattern. The latent pattern is developed by applying a developer to the selectively exposed photoresist layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
depositing a resist layer over a substrate by chemical vapor deposition,
wherein the resist layer is a reaction product of a first precursor and second precursor;
wherein the first precursor is selected from the group consisting of
patternwise exposing the resist layer to actinic radiation; and
applying a developer to the patternwise exposed resist layer to form a pattern in the resist layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the developer is a dry developer.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the developer is a plasma or a chemical vapor.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising before patternwise exposing the resist layer to actinic radiation, heating the resist layer at a temperature ranging from 40° C. to 120° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the actinic radiation is extreme ultraviolet radiation.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the actinic radiation is an electron beam.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the second precursor is a gas.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first precursor and the second precursor are introduced into a chamber heated to a temperature ranging from 30° C. to 400° C. during the depositing the resist layer.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the first precursor and the second precursor are maintained at a pressure ranging from 5 mTorr to 100 Torr during the depositing the resist layer.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising after patternwise exposing the resist layer to actinic radiation and before applying a developer, heating the resist layer at a temperature ranging from 50° C. to 300° C.

### Claim 11

A method of manufacturing a semiconductor device, comprising:
depositing a first organometallic material layer over a substrate,
wherein the first organometallic material layer includes an organometallic material selected from the group consisting of
depositing a gaseous material over the first organometallic material layer;
reacting the gaseous material with the first organometallic material layer to form a first layer of reaction product;
depositing a second organometallic material layer of the organometallic material over the first layer of reaction product;
depositing an additional amount of the gaseous material over the second organometallic material layer;
reacting the additional amount of the gaseous material with the second organometallic material layer to form a second layer of reaction product;
selectively exposing the first and second layers of reaction product to actinic radiation; and
developing the selectively exposed first and second layers of reaction product to form a pattern in the resist layer.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the first and second layers of reaction product are formed by atomic layer deposition.

### Claim 13 (depends on 11)

The method according to claim 11, further comprising before selectively exposing the first and second layers of reaction product to actinic radiation, heating the first and second reaction product layers at a temperature ranging from 40° C. to 120° C.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the actinic radiation is extreme ultraviolet radiation.

### Claim 15 (depends on 11)

The method according to claim 11, further comprising after selectively exposing the first and second layers of reaction product to actinic radiation and before developing, heating the first and second layers of reaction product at a temperature ranging from 50° C. to 300° C.

### Claim 16

A method of manufacturing a semiconductor device, comprising:
depositing a layer of a reaction product of an organometallic first precursor and a gaseous second precursor over a target layer to be patterned,
wherein the first precursor is selected from the group consisting of
patterning the layer of the reaction product.

### Claim 17 (depends on 16)

The method according to claim 16, further comprising before patterning the layer of the reaction product, heating the layer of the reaction product to a temperature ranging from 40° C. to 120° C.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the first precursor and the second precursor are introduced into a chamber heated to a temperature ranging from 30° C. to 400° C. during the depositing the layer of the reaction product.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the first precursor and the second precursor are maintained at a pressure ranging from 5 mTorr to 100 Torr during the depositing the layer of the reaction product.

### Claim 20 (depends on 16)

The method according to claim 16, wherein during the patterning the layer of the reaction product, the layer of the reaction product is selectively exposed to extreme ultraviolet radiation.