# US 2025/0147230 A1 · Optical fiber and method for manufacturing optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0147230 A1
- Document ID: US20250147230A1
- Status: Published application
- Kind: A1
- Application number: 19/014,700
- Filed: 2025-01-09
- Published: 2025-05-08
- Earliest claimed: 2023-01-30
- Assignees: Furukawa Electric Co., Ltd.
- Applicants: Furukawa Electric Co., Ltd.
- Inventors: Kuniaki ISHIZUKI; Mitsuhiro IWAYA
- Web page: https://patentgrep.com/patent/US20250147230A1

## CPC

- G02B 6/02395: {Glass optical fibre with a protective coating, e.g. two layer polymer coating deposited directly on a silica cladding surface during fibre manufacture (G02B6/02052, G02B6/02057, G02B6/024, G02B6/032, G02B6/105, G02B6/14 take precedence; coating on fibre gratings G02B6/02104; multilayer core or cladding G02B6/036; reinforcing splice joints G02B6/2558; optical cables, i.e. comprising protective structures external to the protective coating such as a jacket or plural coated optical fibres G02B6/44; coating of glass to obtain optical fibres C03C25/104)}
- C03C 25/1065: Multiple coatings
- G02B 6/02: Optical fibres with cladding {with or without a coating}
- G02B 6/44: Mechanical structures for providing tensile strength and external protection for fibres, e.g. optical transmission cables (cables incorporating electric conductors and optical fibres {where features relating to the optical fibres are not of interest} H01B11/22)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention intends to suppress curing of a primary layer over time after manufacturing an optical fiber and to effectively suppress microbend loss. The optical fiber according to the present invention including a bare optical fiber, a primary layer formed of a first ultraviolet curing resin covering the bare optical fiber and a secondary layer formed of a second ultraviolet curing resin covering the primary layer. A Young's modulus of the primary layer is larger than or equal to 0.2 MPa and smaller than or equal to 2.1 MPa. The primary layer includes at least one of an alkoxysilane-derived chemical structure or a halosilane-derived chemical structure.

## Claims

### Claim 1

An optical fiber comprising:
a bare optical fiber;
a primary layer formed of a first ultraviolet curing resin covering the bare optical fiber; and
a secondary layer formed of a second ultraviolet curing resin covering the primary layer,
wherein a Young's modulus of the primary layer is larger than or equal to 0.2 MPa and smaller than or equal to 2.1 MPa, and
wherein the primary layer includes at least one of an alkoxysilane-derived chemical structure or a halosilane-derived chemical structure.

### Claim 2 (depends on 1)

The optical fiber according to claim 1, wherein the primary layer is acidic.

### Claim 3 (depends on 1)

The optical fiber according to claim 1, wherein a Young's modulus increase amount of the primary layer before and after 29 days of storage in an atmosphere having a temperature of 25±5° C. and a relative humidity of 50±10% is smaller than or equal to 0.09 MPa.

### Claim 4 (depends on 1)

The optical fiber according to claim 1, wherein a pH of the primary layer is smaller than or equal to 6.6.

### Claim 5 (depends on 1)

The optical fiber according to claim 1, wherein the first ultraviolet curing resin includes a photoacid generator.

### Claim 6 (depends on 5)

The optical fiber according to claim 5, wherein an amount of the photoacid generator added to the first ultraviolet curing resin is larger than or equal to 0.25 wt %.

### Claim 7 (depends on 1)

The optical fiber according to claim 1, wherein the first ultraviolet curing resin is crosslinked through at least one of an alkoxysilane-derived chemical structure or a halosilane-derived chemical structure.

### Claim 8 (depends on 1)

The optical fiber according to claim 1, wherein the first ultraviolet curing resin includes a mercapto group and at least one of an alkoxysilane or a halosilane.

### Claim 9 (depends on 4)

The optical fiber according to claim 4,
wherein a pH of the primary layer is smaller than or equal to 6.5, and
wherein a Young's modulus increase amount of the primary layer before and after 29 days of storage in an atmosphere having a temperature of 25±5° C. and a relative humidity of 50±10% is smaller than or equal to 0.05 MPa.

### Claim 10

A method for manufacturing an optical fiber comprising:
a step of drawing a bare optical fiber from an optical fiber preform;
a step of forming a primary layer by applying a first ultraviolet curing resin around the bare optical fiber; and
a step of forming a secondary layer by applying a second ultraviolet curing resin around the primary layer,
wherein a Young's modulus of the primary layer is larger than or equal to 0.2 MPa and smaller than or equal to 2.1 MPa, and
wherein the primary layer includes at least one of an alkoxysilane-derived chemical structure or a halosilane-derived chemical structure.

### Claim 11 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein the primary layer is acidic.

### Claim 12 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein a Young's modulus increase amount of the primary layer before and after 29 days of storage in an atmosphere having a temperature of 25±5° C. and a relative humidity of 50±10% is smaller than or equal to 0.09 MPa.

### Claim 13 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein a pH of the primary layer is smaller than or equal to 6.6.

### Claim 14 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein the first ultraviolet curing resin includes a photoacid generator.

### Claim 15 (depends on 14)

The method for manufacturing the optical fiber according to claim 14, wherein an amount of the photoacid generator added to the first ultraviolet curing resin is larger than or equal to 0.25 wt %.

### Claim 16 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein the first ultraviolet curing resin is crosslinked through at least one of an alkoxysilane-derived chemical structure or a halosilane-derived chemical structure.

### Claim 17 (depends on 10)

The method for manufacturing the optical fiber according to claim 10, wherein the first ultraviolet curing resin includes a mercapto group and at least one of an alkoxysilane or a halosilane.

### Claim 18 (depends on 10)

The method for manufacturing the optical fiber according to claim 10,
wherein a pH of the primary layer is smaller than or equal to 6.5, and
wherein a Young's modulus increase amount of the primary layer before and after 29 days of storage in an atmosphere having a temperature of 25±5° C. and a relative humidity of 50±10% is smaller than or equal to 0.05 MPa.