# US 2025/0146229 A1 · A method and a system for manufacturing a paperboard

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146229 A1
- Document ID: US20250146229A1
- Status: Published application
- Kind: A1
- Application number: 18/836,863
- Filed: 2023-02-09
- Published: 2025-05-08
- Earliest claimed: 2022-02-10
- Inventors: Max MOHAMMADI; Ali MOHAMMADI
- Web page: https://patentgrep.com/patent/US20250146229A1

## CPC

- D21H 19/82: superposed {(D21H19/84 takes precedence)}
- D21H 21/16: Sizing or water-repelling agents
- D21H 23/48: Curtain coaters
- D21H 25/06: of impregnated or coated paper (D21H25/08 takes precedence)
- D21H 27/10: Packing paper (packaging materials of special type or form B65D65/38)
- B65D 3/06: essentially conical or frusto-conical
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES

## Abstract

The present disclosure relates a cost-effective manufacturing method of barrier-based paperboard and paper webs which are recyclable and repulpable and which embody heat-sealing properties and blocking resistance. To incorporate said properties of the paperboard, the method involves several steps like, paper substrate preparation, pre-treatment of the same followed by coating a base barrier coating, a barrier coating, a heat-sealing coating, and a shield coating, and finally culminating in post-treatment of the paperboard and ending up by winding the board in rolls for marketability.

## Claims

### Claim 1

A method of manufacturing paperboard comprising:
a coating step; and
a post-treatment step;
wherein,
said coating step includes coating a paper substrate with multiple layers of coating, the multiple layers including:
a base barrier coating (A);
a barrier coating (B);
an optional heat-sealing coating (C); and
a shield coating (D),
wherein,
the coating step includes:
applying a base barrier coating (A) on the paper;
reducing the moisture content of the paper substrate by drying the base barrier coating (A) by means of a drying unit;
compressing and smoothening of the paper substrate;
applying a barrier coating layer (B);
compressing and smoothening of the paper substrate;
optionally applying a heat-sealing coating (C);
applying a shield coating (D);
moisturizing the resulting paper substrate after coating the paper substrate with multiple layers; and
wherein,
the post-treatment step includes
compressing and smoothening the paper substrate being the result of the coating step; and
drying the resulting paper substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising a web-forming step and a pre-treatment step before the coating step,
wherein the web forming step includes forming a web-shaped paper substrate of paper fibres; and
wherein the pre-treatment step includes:
drying and reducing the moisture content of paper pulp forming the paper substrate;
cooling the resulting paper substrate;
compressing and smoothening of the paper substrate; and
sealing surface fibres by means of surface sizer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the web forming step includes adding an internally sizing agent.

### Claim 4 (depends on 2)

The method of claim 2, wherein the surface sizer is any one of film size press, a spray sizer, pond size press and a nip sizer, with one or more curtain applicators and/or one or more foam applicators.

### Claim 5 (depends on 1)

The method of claim 1, wherein the weight of the base barrier coating ranges between 1-17 g/m2, more preferably between 3-11 g/m2, and most preferably between 3-8 g/m2.

### Claim 6 (depends on 1)

The method of claim 1, wherein the weight of the barrier coating ranges between 1-14 g/m2, more preferably between 2-8 g/m2, and most preferably between 2-4 g/m2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the weight of the heat sealing coating, if present, ranges between 1-11 g/m2, more preferably between 2-11 g/m2, yet more preferably between 2-5 g/m2, and most preferably between 2-4 g/m2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the weight of the shield coating layer ranges between 1-10 g/m2, more preferably between 2-8 g/m2, yet more preferably between 2-6 g/m2, and most preferably between 2-4 g/m2.

### Claim 9 (depends on 1)

The method of claim 1, wherein the method further comprises applying a heat sealing coating (C), wherein preferably a composition of the heat sealing coating (C) is selected from copolymers of ethylene and methacrylic acid or acrylic acid.

### Claim 10 (depends on 1)

The method of claim 1, wherein the action of moisturizing the resulting paper substrate after coating the multiple layers in the coating step is performed by means of a spraying unit spraying a moistening agent onto the paper substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the moistening agent is, mostly, preferably at least 99% by weight, and most preferably only, water.

### Claim 12 (depends on 10)

The method of claim 10, wherein the spraying unit sprays the moistening agent from nozzles with a spraying pressure between 1-100 MPa, preferably between 1-17 MPa, more preferably between 1-12 MPa, as measured at the nozzles.

### Claim 13 (depends on 1)

The method of claim 1, wherein the web-shaped paper substrate is moved at a web speed below 500 m/min while the action of moisturizing the resulting paper substrate after coating the multiple layers in the coating step is performed.

### Claim 14 (depends on 1)

The method of claim 1, wherein the action of drying the resulting paper substrate in the post-treatment step includes drying the paper substrate with a drying unit which is maintained at a temperature range of 95-117° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the barrier coating composition is in the form of aqueous dispersions, preferably aqueous polymer dispersions.

### Claim 16 (depends on 15)

The method of claim 15, wherein said polymers of the barrier coating composition are biodegradable/renewable polymers.

### Claim 17 (depends on 1)

The method of claim 1, further comprising a finishing step after the post-treatment step,
wherein the finishing step includes
cooling the paper substrate being the result of the post-treatment step; and
winding the coated paper substrate into rolls.

### Claim 18

A system of manufacturing paper board, the system comprising:
an internal sizer;
a surface sizer;
a spraying unit;
at least one coating unit configured to apply
a base barrier coating;
a barrier coating;
a heat-sealing coating; and
a shield coating;
at least one drying unit;
at least one cooling unit;
at least one calendaring unit; and
a paperboard roll winding unit.