# US 2025/0146178 A1 · SiC EPITAXIAL WAFER

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146178 A1
- Document ID: US20250146178A1
- Status: Published application
- Kind: A1
- Application number: 18/938,613
- Filed: 2024-11-06
- Published: 2025-05-08
- Earliest claimed: 2023-11-07
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Yoshikazu UMETA; Marie Ohuchi
- Web page: https://patentgrep.com/patent/US20250146178A1

## CPC

- C30B 29/36: Carbides
- C30B 23/02: Epitaxial-layer growth
- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 29/64: Flat crystals, e.g. plates, strips or discs
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

An objective of the present invention is to provide a SiC epitaxial wafer with a large diameter, a low triangular defect density, and high carrier concentration uniformity. According to the present invention, a SiC epitaxial wafer includes a SiC substrate and a SiC epitaxial layer. The SiC substrate has a diameter of 195 mm or more. The SiC epitaxial layer has a triangular defect density of 0.2 pieces/cm2 or less and a carrier concentration variation of 20% or less.

## Claims

### Claim 1

A SiC epitaxial wafer comprising:
a SiC substrate; and
a SiC epitaxial layer,
wherein the SiC substrate has a diameter of 195 mm or more, and
wherein the SiC epitaxial layer has a triangular defect density of 0.2 pieces/cm2 or less and a carrier concentration variation of 20% or less.

### Claim 2 (depends on 1)

The SiC epitaxial wafer according to claim 1,
wherein the SiC epitaxial layer can be divided into a plurality of regions each having a 5 mm square in a planar view in a stacking direction of the SiC epitaxial wafer, and
wherein a proportion of a region not having a triangular defect among the plurality of regions is 98% or more.

### Claim 3 (depends on 1)

The SiC epitaxial wafer according to claim 1, wherein the SiC epitaxial layer has a carrier concentration variation of 20% or less in a first region at a distance of 60 mm or more and 95 mm or less from a center of the SiC epitaxial layer in a planar view in a stacking direction of the SiC epitaxial wafer.

### Claim 4 (depends on 1)

The SiC epitaxial wafer according to claim 1, wherein a variation in a film thickness of the SiC epitaxial layer is 5% or less.

### Claim 5 (depends on 4)

The SiC epitaxial wafer according to claim 4, wherein the SiC epitaxial layer has the film thickness variation of 5% or less in a first region at a distance of 60 mm or more and 95 mm or less from a center of the SiC epitaxial layer in a planar view in a stacking direction of the SiC epitaxial wafer.