# US 2025/0146163 A1 · Electrophoretic deposition of hexagonal boron nitride films and coatings and their applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146163 A1
- Document ID: US20250146163A1
- Status: Published application
- Kind: A1
- Application number: 18/394,504
- Filed: 2023-12-22
- Published: 2025-05-08
- Earliest claimed: 2022-12-22
- Assignees: The Penn State Research Foundation
- Applicants: The Penn State Research Foundation
- Inventors: George Bepete; Nestor Perea-Lopez; Mauricio Terrones
- Web page: https://patentgrep.com/patent/US20250146163A1

## CPC

- C25D 13/02: with inorganic material
- C25D 13/12: characterised by the article coated
- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Embodiments relate to methods for preparing a hexagonal boron nitride (hBN) suspension and forming films, coatings, or membranes via electrophoretic deposition.

## Claims

### Claim 1

A method for preparing a hexagonal boron nitride (hBN) suspension, the method comprising:
performing steps of:
mixing and dissolving a metal in a solvent to form a mixture, wherein the solvent includes (A) a polar aprotic organic solvent, (A′) a mixture of polar aprotic organic solvents, or (B) ammonia; and
dispersing hBN powder containing one or more hBN sheet or exfoliated hBN powder containing one or more hBN sheet in the mixture, wherein the metal provides a counterion to negatively charge the one or more hBN sheet;
or;
performing steps of:
combining hBN powder containing one or more hBN sheet or exfoliated hBN powder containing one or more hBN sheet with a metal to form a mixture, wherein the metal provides a counterion to negatively charge the one or more hBN sheet;
applying heat to the mixture to generate a metal-intercalated hBN material; and
exposing the metal-intercalated hBN material to a solvent, the solvent including (A) a polar aprotic organic solvent, (A′) a mixture of polar aprotic organic solvents, or (B) ammonia;
or;
performing steps of:
combining hBN powder containing one or more hBN sheet or exfoliated hBN powder containing one or more hBN sheet and a polyelectrolyte to form a mixture;
dispersing the mixture in an organic polar aprotic a solvent, the solvent including (A) a polar aprotic organic solvent, (A′) a mixture of polar aprotic organic solvents, or (B) ammonia, wherein the polyelectrolyte adsorbs onto the hBN and to impart a negative charge to the one or more hBN sheet.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the metal is one or more alkali metals, one or more alkaline earth metals, one or more alkali metal electrides, one or more alkaline earth metal electrides, or a combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein:
the metal is Li, K, Na, R, Cs, Fr, Be, Mg, Ca, Ba, Sr, and/or Ra.

### Claim 4 (depends on 1)

The method of claim 1, wherein:
the counterion is Li+, K+, Na, Rb+, Cs+, Fr+, Be2+, Mg2+, Ca2+, Ba2+, Sr2+, and/or Ra2+.

### Claim 5 (depends on 1)

The method of claim 1, wherein:
the polyelectrolyte is a nucleic acid, a protein, a teichoic acid, a polypeptides, and/or a polysaccharide.

### Claim 6 (depends on 1)

The method of claim 1, wherein:
the solvent is tetrahydrofuran (THF), acetone, acetonitrile, dimethoxyethane (DME), sulfolane, dimethyl sulfoxide (DMSO), dimethylformamide (DMF), N-methylpyrrolidone (NMP), N-methylformamide, acetone, acetonitrile, dichloromethane, dimethylformamide (DMF), dimethylpropyleneurea, and/or ethyl acetate, hexamethylphosphoric triamide.

### Claim 7 (depends on 1)

The method of claim 1, wherein:
mixing and dispersing occur for a duration within a range from 0 hours to 96 hours;
mixing and dispersing occur while the mixture is subjected to a temperature within a range from −22° C. to 220° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein:
concentration of the exfoliated hBN in the hBN suspension is within a range from 0.01 g/L to 10 g/L.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
separating the hBN suspension from the mixture via centrifugation.

### Claim 10

A method of depositing hexagonal boron nitride (hBN) on a substrate, the method comprising:
placing an anode electrode in an environment containing an exfoliated hBN suspension, the exfoliated hBN suspension including one or more negatively charged hBN sheets, the anode comprising the substrate;
placing a cathode electrode in the environment;
applying a voltage difference across the anode electrode and the cathode electrode;
forming, via electrophoretic deposition, a hBN film, coating, and/or membrane on at least a portion of the substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein:
the hBN film, coating, and/or membrane is formed directly on a surface of the substrate; and/or
the hBN film, coating, and/or membrane is formed on a layer of material formed on the substrate.

### Claim 12 (depends on 11)

The method of claim 11, wherein:
the material includes any one or combination of graphene, MoS2, or WS2.

### Claim 13 (depends on 10)

The method of claim 10, wherein:
the hBN film, coating, and/or membrane is used as an anticorrosion coating, an antioxidation coating, a lubricant coating, an insulating coating, a thermally or electrically conductive coating, a heat dissipation coating, and/or a dielectric coating for the substrate.