# US 2025/0146150 A1 · Method for electrocatalytic reduction of carbon dioxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146150 A1
- Document ID: US20250146150A1
- Status: Published application
- Kind: A1
- Application number: 19/017,876
- Filed: 2025-01-13
- Published: 2025-05-08
- Earliest claimed: 2023-10-26
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Munzir Hamedelniel Mohamed SULIMAN; Muhammad USMAN
- Web page: https://patentgrep.com/patent/US20250146150A1

## CPC

- C25B 11/077: the compound being a non-noble metal oxide
- C25B 1/23: Carbon monoxide or syngas
- C25B 3/03: Acyclic or carbocyclic hydrocarbons
- C25B 3/25: Reduction
- C25B 3/26: of carbon dioxide
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

A method of forming an electrode including dissolving a copper salt and benzene-1,3,5-tricarboxylate in a solvent and heating to a temperature of 60° C. to 100° C. to form a framework. Further, the method includes mixing a zinc salt and the framework to form a zinc doped framework and heating the zinc doped framework to a temperature of 300° C. to 600° C. under air to form ZnCuO nanoparticles. Furthermore, the method includes mixing the ZnCuO nanoparticles, a binding compound, and a conductive carbon compound in a solvent to form a suspension. Moreover, the method includes coating a substrate with the suspension and drying to form the electrode and the ZnCuO nanoparticles have an oval shape with an average size of 50 nm to 200 nm.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method for electrocatalytically reducing carbon dioxide (CO2), comprising:
applying a potential of less than 0 V to −2.0 V vs RHE to an electrochemical cell,
wherein the electrochemical cell is at least partially submerged in an aqueous solution comprising carbon dioxide,
wherein on applying the potential the carbon dioxide is reduced to a conversion product,
wherein the electrochemical cell comprises:
an electrode; and
a counter electrode;
wherein the electrode is made by:
dissolving a copper salt and benzene-1,3,5-tricarboxylate in a solvent and heating to a temperature of 60-100° C. to form a framework;
mixing a zinc salt and the framework to form a zinc doped framework;
heating the zinc doped framework to a temperature of 300° C. to 600° C. under air to form ZnCuO nanoparticles;
mixing the ZnCuO nanoparticles, a binding compound, and a conductive carbon compound in a solvent to form a suspension; and
coating a substrate with the suspension and drying to form the electrode;
wherein the ZnCuO nanoparticles on the substrate have an oval shape with an average size of 50 nm to 200 nm.

### Claim 16 (depends on 15)

The method of claim 15, wherein the conversion product is selected from ethane and carbon monoxide.

### Claim 17 (depends on 15)

The method of claim 15, wherein the aqueous solution further comprises a base selected from at least one of sodium bicarbonate and potassium bicarbonate.

### Claim 18 (depends on 16)

The method of claim 16, having a faradic efficiency for reducing carbon dioxide to ethane of 35% to 45%.

### Claim 19 (depends on 16)

The method of claim 16, having a faradic efficiency for reducing carbon dioxide to carbon monoxide of 50% to 60%.

### Claim 20 (depends on 15)

The method of claim 15, wherein the aqueous solution is saturated with the carbon dioxide.

### Claim 21 (depends on 15)

The method of claim 15, wherein the ZnCuO nanoparticles comprise 5 mol % to 50 mol % Zn, relative to a total number of Zn and Cu moles in the ZnCuO nanoparticles.

### Claim 22 (depends on 15)

The method of claim 15, wherein the ZnCuO nanoparticles comprise Cu, C, Zn, and O.

### Claim 23 (depends on 15)

The method of claim 15, wherein the ZnCuO nanoparticles comprise 30 wt. % to 40 wt. % Cu, 30 wt. % to 40 wt. % C, 10 wt. % to 20 wt. % Zn, and 10 wt. % to 20 wt. % O.

### Claim 24 (depends on 15)

The method of claim 15, wherein the ZnCuO nanoparticles comprise CuO and ZnO and wherein the CuO has a monoclinic crystal structure and the ZnO has a hexagonal crystal structure.

### Claim 25 (depends on 15)

The method of claim 15, wherein the conductive carbon compound is at least one selected from the group consisting of graphite, activated carbon, reduced graphene oxide, carbon nanotubes, carbon nanofibers, and carbon black.

### Claim 26 (depends on 15)

The method of claim 15, wherein the binding compound is a fluorinated polymer.

### Claim 27 (depends on 15)

The method of claim 15, wherein the substrate is made from at least one material selected from the group consisting of conductive carbon, stainless steel, aluminum, nickel, copper, platinum, zinc, tungsten, and titanium.