# US 2025/0146099 A1 · Removal of impurities contained in iron ores

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146099 A1
- Document ID: US20250146099A1
- Status: Published application
- Kind: A1
- Application number: 18/941,806
- Filed: 2024-11-08
- Published: 2025-05-08
- Earliest claimed: 2023-11-08
- Assignees: Form Energy, Inc.
- Applicants: Form Energy, Inc.
- Inventors: Alex Luyima; Joseph Stephen Manser
- Web page: https://patentgrep.com/patent/US20250146099A1

## CPC

- C22B 1/24: Binding; Briquetting {; Granulating}
- C21B 15/00: Other processes for the manufacture of iron from iron compounds (by electrolysis C25C1/06)
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- C22B 3/10: Hydrochloric acid {, other halogenated acids or salts thereof}
- C22B 3/12: in inorganic alkaline solutions
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C25C 1/06: or iron group metals, refractory metals or manganese
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of removing one or more impurities from an iron-containing feedstock includes grinding the iron-containing feedstock in the presence of a grinding aid to form a pretreated iron-containing feedstock, the grinding aid including an alkali metal chloride, a fluoride salt, or a combination thereof; contacting the pretreated iron-containing feedstock with a flux comprising a metal borate; fusing the pretreated iron-containing feedstock and the flux to form a fused mixture; treating the fused mixture with a leaching solution to form a purified iron-containing feedstock and a used leaching solution; and solid-liquid separating the purified iron-containing feedstock from the used leaching solution, wherein an amount of aluminum, silicon, or a combination thereof is less in the purified iron-containing feedstock than in the iron-containing feedstock. Methods of removing one or more impurities from an iron-containing feedstock also include leaching the pretreated iron-containing feedstock with acid or base without fusion.

## Claims

### Claim 1

A method of removing one or more impurities from an iron-containing feedstock, the method comprising:
grinding the iron-containing feedstock in the presence of a grinding aid to form a pretreated iron-containing feedstock, the grinding aid comprising an alkali metal chloride, a fluoride salt, or a combination thereof;
contacting the pretreated iron-containing feedstock with a flux comprising a metal borate;
fusing the pretreated iron-containing feedstock and the flux to form a fused mixture;
treating the fused mixture with a leaching solution to form a purified iron-containing feedstock and a used leaching solution; and
solid-liquid separating the purified iron-containing feedstock from the used leaching solution,
wherein an amount of aluminum, silicon, or a combination thereof is less in the purified iron-containing feedstock than in the iron-containing feedstock.

### Claim 2 (depends on 1)

The method of claim 1, wherein a weight ratio of the flux to the pretreated iron-containing feedstock is less than or equal to 1.5:1.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal of the metal borate is an alkali metal, an alkaline earth metal, or a combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal borate is Na3BO3, Na3B3O6, NaB(OH)4, Na2B4O7, Na2B4O7·4H2O, Na2B4O7·5H2O, Na2B4O7·10H2O, Na2B8O13, or a combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the flux further comprises a second fluoride salt, a second chloride salt, a hydroxide, or a combination thereof, and optionally wherein the second fluoride salt is ammonium fluoride, an alkali metal fluoride, an alkaline earth metal fluoride, or a combination thereof, and the second chloride salt is ammonium chloride, an alkali metal chloride, an alkaline earth metal chloride, or a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the fusing comprises heating at a temperature of 323° C. to 1500° C. for 1 hour to 24 hours.

### Claim 7 (depends on 1)

The method of claim 1, wherein the leaching solution is water, and optionally the water has a temperature of 25° C. to 300° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the leaching solution is
(i) an acidic aqueous solution; or
(ii) an acidic aqueous solution comprising hydrofluoric acid, hydrochloric acid, nitric acid, sulfuric acid, acetic acid, citric acid, oxalic acid, or a combination thereof.

### Claim 9 (depends on 1)

The method of claim 1, wherein the leaching solution is
(i) a basic aqueous solution; or
(ii) a basic aqueous solution comprising sodium hydroxide, potassium hydroxide, lithium hydroxide, cesium hydroxide, ammonium hydroxide, or a combination thereof.

### Claim 10 (depends on 1)

The method of claim 1, further comprising recycling one or more components of the flux from the used leaching solution.

### Claim 11

A method of removing one or more impurities from an iron-containing feedstock, the method comprising:
grinding the iron-containing feedstock in the presence of a grinding aid to provide a pretreated iron-containing feedstock, the grinding aid comprising an alkali metal chloride, a fluoride salt, or a combination thereof;
contacting the pretreated iron-containing feedstock with an acid solution to form a purified iron-containing feedstock and a used acid solution, the acid solution comprising 1 wt % to 20 wt % of an inorganic acid having a pKa of less than −1, an organic acid, or a combination thereof, based on a total weight of the acid solution; and
solid-liquid separating the purified iron-containing feedstock from the used acid solution,
wherein an amount of aluminum, silicon, or a combination thereof is less in the purified iron-containing feedstock than in the iron-containing feedstock.

### Claim 12

(canceled)

### Claim 13

(canceled)

### Claim 14 (depends on 11)

The method of claim 11, wherein the acid solution comprises hydrochloric acid, nitric acid, sulfuric acid, acetic acid, citric acid, oxalic acid, or a combination thereof.

### Claim 15

(canceled)

### Claim 16

A method of removing one or more impurities from an iron-containing feedstock, the method comprising:
grinding the iron-containing feedstock in the presence of a grinding aid to form a pretreated iron-containing feedstock, the grinding aid comprising an alkali metal chloride, a fluoride salt, or a combination thereof;
contacting the pretreated iron-containing feedstock with a caustic solution having a hydroxide concentration of at least 30 wt % at a temperature of at least 90° C. to form a purified iron-containing feedstock and a used caustic solution, the caustic solution and the iron-containing feedstock having a ratio of at least 2.5 mL/g; and
solid-liquid separating the purified iron-containing feedstock from the used caustic solution,
wherein an amount of aluminum, silicon, or a combination thereof is less in the purified iron-containing feedstock than in the iron-containing feedstock.

### Claim 17 (depends on 16)

The method of claim 16, wherein the contacting is at a temperature of 140° C. to 300° C. for 30 minutes to 24 hours.

### Claim 18 (depends on 16)

The method of claim 16, wherein the caustic solution comprises sodium hydroxide, potassium hydroxide, lithium hydroxide, cesium hydroxide, ammonium hydroxide, or a combination thereof.

### Claim 19 (depends on 16)

The method of claim 16, further comprising purifying the used caustic solution to form a purified caustic solution before further contacting the purified caustic solution with the pretreated iron-containing feedstock.

### Claim 20 (depends on 19)

The method of claim 19, wherein the purifying comprises contacting the used caustic solution with Al2O3, Al(OH)3, CaO, Ca(OH)2, an aluminate compound, or a combination thereof; and optionally wherein the aluminate compound comprises NaAlO2, Al2Si2O5(OH)4, NaAl(OH)4, Na2O·Al2O3, Na2Al2O4, or a combination thereof.

### Claim 21

(canceled)

### Claim 22 (depends on 1)

The method of claim 1, wherein the grinding aid is solid sodium chloride.

### Claim 23 (depends on 1)

The method of claim 1, wherein a weight ratio of the grinding aid to the iron-containing feedstock is 1:8 to 1:1.

### Claim 24 (depends on 1)

The method of claim 1, wherein the grinding releases one or more impurities from a matrix of the iron-containing feedstock.

### Claim 25 (depends on 1)

The method of claim 1, wherein
(i) the pretreated iron-containing feedstock comprises iron-containing feedstock particles having an average particle size of 10 μm to 300 μm;
(ii) the iron-containing feedstock comprises hematite, maghemite, magnetite, goethite, limonite, or a combination thereof;
(iii) the method further comprises washing the purified iron-containing feedstock with an aqueous solution; or
(iv) a combination thereof.

### Claim 26 (depends on 1)

The method of claim 1, wherein
(i) the purified iron-containing feedstock comprises at least 10 weight percent less aluminum than the iron-containing feedstock, based on a total weight of the aluminum in the iron-containing feedstock;
(ii) the purified iron-containing feedstock comprises at least 10 weight percent less silicon than the iron-containing feedstock, based on a total weight of the silicon in the iron-containing feedstock;
(iii) a total content of silicon and aluminum in the purified iron-containing feedstock is less than 6 wt %, based on a total weight of the purified iron-containing feedstock; or
(iv) a combination thereof.

### Claim 27 (depends on 1)

A purified iron-containing feedstock, prepared by the method of claim 1.

### Claim 28 (depends on 1)

A method comprising:
removing one or more impurities from an iron-containing feedstock to form a purified iron-containing feedstock by the method of claim 1; and
electrochemically producing an iron metal from the purified iron-containing feedstock.

### Claim 29 (depends on 28)

The method of claim 28, wherein the iron metal has
a specific total embedded emissions of less than 0.8 tons of CO2 per ton of the iron metal, when determined according to the European Union simplified bubble approach method for determining specific embedded emissions under the Carbon Border Adjustment Mechanism;
a carbon emission intensity of less than 1100 kilograms of CO2 per ton of the iron metal, when determined according to ISO 14404;
a carbon emission intensity of less than 800 kilograms of CO2 per ton of the iron metal, when determined according to the Intergovernmental Panel on Climate Change Methodology 2006 Guidelines for National Greenhouse Gas Inventories;
a carbon emission intensity of less than 1500 kilograms of CO2 per ton of the iron metal, when determined according to the 2017 World Steel Life Cycle Inventory Methodology;
a carbon emission intensity of less than 1300 kilograms of CO2 per ton of the iron metal, when determined according to the 2008 World Resource Institute Iron and Steel Greenhouse Gas Protocol;
a carbon emission intensity of less than 750 kilograms of CO2 per ton of the iron metal, when determined according to European Union Commission Implementing Regulation 2018/2066;
a specific total embedded emissions of less than 0 tons of CO2 per ton of the iron metal, when determined according to the European Union simplified bubble approach method for determining specific embedded emissions under the Carbon Border Adjustment Mechanism, or a combination thereof.