# US 2025/0146096 A1 · Method of producing grain-oriented electrical steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146096 A1
- Document ID: US20250146096A1
- Status: Published application
- Kind: A1
- Application number: 18/838,042
- Filed: 2023-03-02
- Published: 2025-05-08
- Earliest claimed: 2022-03-02
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Rieko IZUMI; Toshito TAKAMIYA; Akio FUJITA; Toru NAKASHIMA; Norihisa OKADA
- Web page: https://patentgrep.com/patent/US20250146096A1

## CPC

- C21D 9/46: for sheet metals
- C21D 6/008: {containing Si}
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1238: {Flattening; Dressing; Flexing}
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/04: containing manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a way to inhibit propagation of edge cracks. A method of producing a grain-oriented electrical steel sheet including, before final annealing, local strain with an indentation amount from the steel sheet surface of 5 μm to 30 μm is applied to a linear region that, when coiled and the coil is charged into a final annealing furnace, is separated from the axial end of the coil that comes into contact with a coil receiving base of the final annealing furnace by 5 mm or more and 20 mm or less in the axial direction of the coil and that extends continuously or discontinuously in a direction on that intersects the axial direction, in order to produce crystal grains having a misorientation angle of 15° or more from Goss orientation grains along 50% or more of the total length of the linear region.

## Claims

### Claim 1

A method of producing a grain-oriented electrical steel sheet, the method comprising:
hot rolling a silicon-containing steel slab; then cold rolling once or two or more times with intermediate annealing; then decarburization annealing; then applying an annealing separator; then winding into a coil; then final annealing; then flattening annealing, wherein
before the final annealing, local strain with an indentation amount from the steel sheet surface of 5 μm to 30 μm is applied to a linear region that, when coiled and the coil is charged into a final annealing furnace, is separated from the axial end of the coil that comes into contact with a coil receiving base of the final annealing furnace by 5 mm or more and 20 mm or less in the axial direction of the coil and that extends continuously or discontinuously in a direction that intersects the axial direction, in order to produce crystal grains having a misorientation angle of 15° or more from Goss orientation grains along 50% or more of the total length of the linear region.

### Claim 2 (depends on 1)

The method of producing a grain-oriented electrical steel sheet according to claim 1, wherein a plurality of linear strain regions apply strain in the linear region.

### Claim 3 (depends on 1)

The method of producing a grain-oriented electrical steel sheet according to claim 1, wherein an average heating rate in a range from 500° C. or more to 800° C. or less in the final annealing is 25° C./h or less.

### Claim 4 (depends on 2)