# US 2025/0146091 A1 · Method for treating steel mill slag

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0146091 A1
- Document ID: US20250146091A1
- Status: Published application
- Kind: A1
- Application number: 18/690,980
- Filed: 2021-09-13
- Published: 2025-05-08
- Earliest claimed: 2021-09-13
- Assignees: Ocs 2 Ug (HaftungsbeschräNkt)
- Applicants: Ocs 2 Ug (HaftungsbeschräNkt); Iron Star GmbH
- Inventors: Günther BELLMANN
- Web page: https://patentgrep.com/patent/US20250146091A1

## CPC

- C21B 3/04: Recovery of by-products, e.g. slag
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/04: Working-up slag
- C21B 2200/00: Recycling of non-gaseous waste material
- C21B 2400/02: Physical or chemical treatment of slags
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

The method according to the invention for treating steel mill slag includes the steps of A) providing steel mill slag in solid form having a fineness such that the steel mill slag has a specific surface area according to BET of 0.1 m2/g or more; step B) treating the steel mill slag by heating it to a temperature of at least 800° Celsius, while adding oxidizing agents and auxiliary agents; and step C) separating iron (III) oxide and iron (II,III) oxide out of the treated steel mill slag.

## Claims

### Claim 1

A method for treating steel mill slag comprising the following steps:
A) providing steel mill slag, which, when solidified, has iron (II) oxide (FeO) and, if solidified, has a fineness such that the steel mill slag has a specific surface area according to BET of 0.1 m2/g or more;
B) treating the steel mill slag at a temperature of at least 600° C., while adding oxidising agents and auxiliary agents,
a) wherein the oxidising agents oxidise at least a part of the iron (II) oxide (FeO) present to iron (III) oxide (Fe2O3) and/or iron (II,III) oxide (Fe3O4) and
b) wherein the auxiliary agents form a bond at least with calcium from calcium-iron compound present and bound in the steel mill slag and
b1) thereby release iron (III) oxide (Fe2O3) and/or iron (II,III) oxide (Fe3O4) and
b2) further increase the proportion of 2 CaO·SiO2 (belite) and/or other calcium silicates, such as alite, wollastonite and/or rankinite, in the treated steel mill slag,
C) separating iron (III) oxide (Fe2O3) and iron (II,III) oxide (Fe3O4) out of the treated steel mill slag.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein
the method further includes:
D) further treating the steel mill slag treated at a temperature of at least 600° C. in a reducing atmosphere by means of adding reducing agents to the heated, treated steel mill slag to reduce iron (III) oxide (Fe2O3) to iron (II,III) oxide (Fe3O4).

### Claim 3 (depends on 2)

The method according to claim 2,
wherein
step D) is carried out after step B) and before step C).

### Claim 4 (depends on 1)

The method according to claim 1,
wherein
the warm, treated steel mill slag is cooled, solidified and crushed, in particular ground up, before step C) so that the cooled, solidified and crushed steel mill slag has a specific surface area according to BET of 0.1 m2/g or more.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein
the separation in step C) is based on magnetic properties, density and/or by means of flotation.

### Claim 6 (depends on 1)

The method according to claim 1,
wherein
the method further includes:
E) treating the treated steel mill slag with CO2 to convert 2 CaO·SiO2 (belite) and/or other calcium silicates, such as alite, wollastonite and/or rankinite, into CaCO3 and SiO2 and/or other corresponding reaction products.

### Claim 7 (depends on 6)

The method according to claim 6,
wherein
step E) is carried out in an aqueous suspension of cooled, solidified and crushed steel mill slag and
a gas, which contains CO2, is injected.

### Claim 8 (depends on 6)

The method according to claim 6,
wherein
the method further includes:
F) separating CaCO3-rich material after step E), in particular by means of flotation.

### Claim 9 (depends on 6)

The method according to claim 6,
wherein
the gas, which contains CO2, originates from steel production.

### Claim 10 (depends on 8)

The method according to claim 8,
wherein
a CaCO3-rich material is separated and/or recovered and fed into the steel or pig iron production process or cement production process for further utilization.

### Claim 11 (depends on 1)

The method according to claim 1,
wherein
an SiO2-rich material is separated and/or recovered and fed into the cement production process for further utilization.

### Claim 12 (depends on 1)

The method according to claim 1,
wherein
the recovered iron (III) oxide (Fe2O3) and/or iron (II,III) oxide (Fe3O4) is fed into the steel production process and/or blast furnace processes for further utilization.

### Claim 13 (depends on 1)

The method according to claim 1,
wherein
a 2 CaO·SiO2 (belite)-rich material and/or a material which is rich in other calcium silicates such as alite, wollastonite and/or rankinite is separated and/or recovered and fed into the cement production process for further utilization.

### Claim 14 (depends on 1)

The method according to claim 1,
wherein
before step A), in a step 0), the steel mill slag is prepared to the desired particle size by means of grinding and/or granulation.

### Claim 15 (depends on 1)

The method according to claim 1,
wherein
in step 0) or after step A) metallic iron (Fe) and/or iron (II,III) oxide (Fe3O4) are separated from the steel mill slag.