# US 2025/0145880 A1 · Graphene based material for corrosion inhibition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145880 A1
- Document ID: US20250145880A1
- Status: Published application
- Kind: A1
- Application number: 19/020,422
- Filed: 2025-01-14
- Published: 2025-05-08
- Earliest claimed: 2022-10-12
- Assignees: Saudi Arabian Oil Company; King Fahd University of Petroleum and Minerals
- Applicants: Saudi Arabian Oil Company; King Fahd University of Petroleum & Minerals
- Inventors: Bader Ghazi Al-Harbi; Tawfik A. Saleh; Norah A. Aljeaban
- Web page: https://patentgrep.com/patent/US20250145880A1

## CPC

- C09K 8/54: Compositions for in situ inhibition of corrosion in boreholes or wells
- C01B 32/194: After-treatment
- C01B 32/198: Graphene oxide
- C01B 32/23: Oxidation
- E21B 37/06: using chemical means for preventing or limiting {, e.g. eliminating,} the deposition of paraffins or like substances
- C09K 2208/32: Anticorrosion additives
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A method includes preparing an alkyl-modified graphene oxide, injecting the modified graphene oxide into a well, and inhibiting acid-induced corrosion of a steel surface in the well with the modified graphene oxide. A composition includes an alkyl-modified graphene oxide having one or more alkyl functional group covalently bonded to a graphene core through an oxygen-containing linking group. A method of preparing modified graphene oxide includes mixing graphite powder with an oxidant to provide a mixture, adding the mixture to an acid solution including H2SO4, H3PO4, or a combination thereof to provide graphene oxide, and reacting the graphene oxide with an alkyl halide by nucleophilic substitution to provide the alkyl-modified graphene oxide.

## Claims

### Claim 1

A method comprising:
preparing an alkyl-modified graphene oxide;
injecting the modified graphene oxide into a well; and
inhibiting acid-induced corrosion of a steel surface in the well with the modified graphene oxide.

### Claim 2 (depends on 1)

The method of claim 1, wherein preparing the alkyl-modified graphene oxide comprises:
mixing graphite powder with an oxidant to provide a mixture;
adding the mixture to an acid solution to provide graphene oxide; and
reacting the graphene oxide with an alkyl halide by nucleophilic substitution to provide the alkyl-modified graphene oxide.

### Claim 3 (depends on 2)

The method of claim 2, wherein the alkyl halide comprises an alkyl group having from 4 to 20 carbon atoms.

### Claim 4 (depends on 3)

The method of claim 3, wherein the alkyl group is selected from the group consisting of hexane, dodecane, octadecane, and combinations thereof.

### Claim 5 (depends on 3)

The method of claim 3, wherein the alkyl halide is an alkyl bromide selected from the group consisting of 1-bromohexane, 1-bromododecane, 1-bromooctadecane, and combinations thereof.

### Claim 6 (depends on 2)

The method of claim 2, wherein the acidic solution comprises one or more of nitric acid, phosphonic acid, sulfuric acid, and hydrochloric acid.

### Claim 7 (depends on 2)

The method of claim 2, wherein the graphene oxide and alkyl halide are reacted in a mole ratio ranging from 1:4 to 4:1 of graphene oxide to alkyl halide.

### Claim 8 (depends on 7)

The method of claim 7, wherein the graphene oxide and alkyl halide are reacted in a mole ratio of about 1:1 of graphene oxide to alkyl halide.

### Claim 9 (depends on 1)

The method of claim 1, wherein the alkyl-modified graphene oxide inhibits the acid-induced corrosion with an inhibition efficiency ranging from 85 to 95%.

### Claim 10 (depends on 1)

The method of claim 1, wherein the alkyl-modified graphene oxide inhibits the acid-induced corrosion such that a corrosion rate of the steel surface is in a range of from 0.30 to 0.55 mm/yr.

### Claim 11

(canceled)

### Claim 12

(canceled)

### Claim 13

(canceled)

### Claim 14

(canceled)

### Claim 15

(canceled)

### Claim 16

(canceled)

### Claim 17

(canceled)

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20

(canceled)