# US 2025/0145860 A1 · Polishing composition for semiconductor process and manufacturing method of substrate using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145860 A1
- Document ID: US20250145860A1
- Status: Published application
- Kind: A1
- Application number: 18/938,878
- Filed: 2024-11-06
- Published: 2025-05-08
- Earliest claimed: 2023-11-06
- Assignees: SK enpulse Co., Ltd.; SK hynix Inc.
- Applicants: SK enpulse Co., Ltd.; SK Hynix Inc.
- Inventors: Deok Su HAN; Jong Young CHO; Woo Joo KIM; Hyun Goo KANG; Dong Kyun LEE
- Web page: https://patentgrep.com/patent/US20250145860A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- C09K 3/1463: {Aqueous liquid suspensions}
- H10P 52/403: {of conductive or resistive materials}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A polishing composition for a semiconductor process includes polishing particles, a polishing pad protectant, and a fluorinated surfactant. The polishing composition for the semiconductor process has an Rm/e value of 2.5% or less, which is a ratio of a number of defects derived from an organic substance as calculated by Equation 1 below. Rm / e = Dm De × 100 ⁢ ( % ) [ Equation ⁢ 1 ] In the Equation 1, a De value is a number of defects detected from a top surface of a substrate after polishing the top surface with the polishing composition for the semiconductor process and etching back the top surface, and a Dm value is a number of defects derived from the organic substance among 100 defects randomly selected from the defects detected from the top surface after the polishing and etching back of the top surface. In these cases, polished and etched surfaces can prevent contamination by particles, especially organic particles.

## Claims

### Claim 1

A polishing composition for a semiconductor process, the polishing composition comprising:
polishing particles;
a polishing pad protectant; and
a fluorinated surfactant,
wherein the polishing composition has an Rm/e value of 2.5% or less, which is a ratio of a number of defects derived from an organic substance as calculated by Equation 1 below;
Rm
/
e
=
Dm
De
×
100
⁢
(
%
)
[
Equation
⁢
1
]
wherein in the Equation 1, a De value is a number of defects detected from a top surface of a substrate after polishing the top surface with the polishing composition for the semiconductor process and etching back the top surface, and
wherein a Dm value is a number of defects derived from the organic substance among 100 defects randomly selected from the defects detected from the top surface after the polishing and etching back of the top surface.

### Claim 2 (depends on 1)

The polishing composition for a semiconductor process of claim 1, wherein the polishing pad protectant comprises a sugar alcohol.

### Claim 3 (depends on 2)

The polishing composition for a semiconductor process of claim 2, wherein the sugar alcohol is one selected from the group consisting of sorbitol, mannitol, galactitol, fucitol, iditol, inositol, arabitol, xylitol, erythritol, threitol, and combinations thereof.

### Claim 4 (depends on 1)

The polishing composition for a semiconductor process of claim 1, wherein the fluorinated surfactant is a compound represented by Formula 1 below;
Rf—(Ren—O)n—H [Formula 1]
In the Formula 1, Rf is a fluoroalkyl group having a carbon number from 3 to 10, Ren is an alkylene group having a carbon number of 2 or 3, and n is an integer from 2 to 15.

### Claim 5 (depends on 1)

The polishing composition for a semiconductor process of claim 1, wherein the polishing composition comprises from 1 wt % to 5 wt % of the polishing pad protectant.

### Claim 6 (depends on 1)

The polishing composition for a semiconductor process of claim 1, wherein the polishing composition comprises from 10 ppm (by weight) to 500 ppm (by weight) of the fluorinated surfactant.

### Claim 7 (depends on 1)

The polishing composition for a semiconductor process of claim 1, further comprising a tungsten inhibitor,
wherein the tungsten inhibitor is one selected from the group consisting of an azole-based compound, an amino acid, and combinations thereof.

### Claim 8 (depends on 1)

The polishing composition for a semiconductor process of claim 1, wherein the polishing composition has a pH of 2.5 to 5.

### Claim 9

A method of manufacturing a substrate, the method comprising:
polishing the substrate by applying a polishing composition for a semiconductor process, the polishing composition comprising:
polishing particles;
a polishing pad protectant; and
a fluorinated surfactant,
wherein the polishing composition has an Rm/e value of 2.5% or less, which is a ratio of a number of defects derived from an organic substance as calculated by Equation 1 below;
Rm
/
e
=
Dm
De
×
100
⁢
(
%
)
[
Equation
⁢
1
]
wherein in the Equation 1, a De value is a number of defects detected from a top surface of the substrate after polishing the top surface with the polishing composition and etching back the top surface, and
wherein a Dm value is a number of defects derived from the organic substance among 100 defects randomly selected from the defects detected from the top surface after the polishing and etching back of the top surface.