# US 2025/0145810 A1 · Polyethylene composition for pipe applications with improved sagging properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145810 A1
- Document ID: US20250145810A1
- Status: Published application
- Kind: A1
- Application number: 19/018,904
- Filed: 2025-01-13
- Published: 2025-05-08
- Earliest claimed: 2013-12-23
- Assignees: Abu Dhabi Polymers Co. Ltd (Borouge) LLC.; Borealis AG
- Applicants: Abu Dhabi Polymers Company Limited (Borouge); Borealis AG
- Inventors: Antti TYNYS; Jarmo HARJUNTAUSTA; Mohana Murali ADHYATMABHATTAR
- Web page: https://patentgrep.com/patent/US20250145810A1

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08K 3/04: Carbon
- C08L 23/06: Polyethylene
- F16L 9/12: of plastics with or without reinforcement (F16L9/16 - F16L9/22 take precedence)
- C08L 2203/18: used for pipes
- C08L 2308/00: Chemical blending or stepwise polymerisation process with the same catalyst
- C08L 2314/02: Ziegler natta catalyst
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

The present invention relates to a polyethylene composition comprising, a base resin (A) comprising a copolymer of ethylene and at least one comonomer selected from alpha-olefins having from three to twelve carbon atoms, wherein the ethylene copolymer comprises a low molecular weight component (A-1) and a high molecular weight component (A-2) with the low molecular weight component (A-1) having a lower weight average molecular weight than the high molecular weight component (A-2), (B) carbon black in an amount of 1.0 to 10 wt % based on the total amount of the polyethylene composition, and (C) optional further additives other than carbon black.

## Claims

### Claim at position 1

1-11. (canceled)

### Claim 12

A polyethylene composition comprising,
a base resin (A) comprising
a copolymer of ethylene and at least one comonomer selected from alpha-olefins having from three to twelve carbon atoms,
wherein the ethylene copolymer comprises a low molecular weight component (A-1) and a high molecular weight component (A-2) with the low molecular weight component (A-1) having a lower weight average molecular weight than the high molecular weight component (A-2),
(B) carbon black in an amount of 1.0 to 10 wt % based on the total amount of the polyethylene composition, and
(C) optional further additives other than carbon black;
wherein the base resin (A) has a density of equal to or more than 943 kg/m3 to equal to or less than 957 kg/m3, determined according to ISO 1183, and
the composition has a melt flow rate MFR5 (190° C., 5 kg) of equal to or more than 0.12 g/10 min to equal to or less than 0.20 g/10 min, determined according to ISO 1133, a shear thinning index SHI2.7/210 of equal to or more than 80 to equal to or less than 130 and a viscosity at a constant shear stress of 747 Pa, eta747, of equal to or more than 700 kPas to equal to or less than 1200 kPas.

### Claim 13 (depends on 12)

The polyethylene composition according to claim 12, wherein the low molecular weight component (A-1) is an ethylene homopolymer.

### Claim 14 (depends on 12)

The polyethylene composition according to claim 12, wherein the low molecular weight component (A-1) has a melt flow rate MFR2 (190° C., 2.16 kg) of 200 g/10 min to 400 g/10 min, determined according to ISO 1133.

### Claim 15 (depends on 12)

The polyethylene composition according to claim 12, wherein the high molecular weight component (A-2) is a copolymer of ethylene and a comonomer selected from alpha-olefins having from three to twelve carbon atoms.

### Claim 16 (depends on 12)

The polyethylene composition according to claim 12, wherein the weight ratio of the low molecular weight component (A-1) to the high molecular component (A-2) is from 45:55 to 55:45.

### Claim 17 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has a melt flow rate MFR21 (190° C., 21.6 kg) of 5.6 g/10 min to 7.0 g/10 min, determined according to ISO 1133.

### Claim 18 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has a density of equal to or more than 953 kg/m3 to equal to or less than 967 kg/m3, determined according to ISO 1183.

### Claim 19 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has a shear thinning index SHI5/200 of equal to or more than 50 to equal to or less than 100.

### Claim 20 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has at least one, preferably both, of the following properties a) a weight average molecular weight, Mw, of 250 to 360 kg/mol, more preferably 260 to 340 kg/mol, and/or b) Mz value of 1600 to 2500 kg/mol, preferably 1700 to 2200 kg/mol, even more preferably 1750 to 2150 kg/mol.

### Claim 21 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has a molecular weight distribution Mw/Mn, of at least 25, preferably 30 to 50, more preferably 30 to 45.

### Claim 22 (depends on 12)

The polyethylene composition according to claim 12, wherein the composition has a tensile modulus of equal to or less than 1250 MPa, determined according to ISO 527-2:1993.

### Claim 23

A polyethylene composition obtainable by a multistage process, the process comprising
a) polymerizing ethylene in the presence of a Ziegler-Natta catalyst for obtaining an intermediate material,
b) transferring the intermediate material to a gas phase reactor
(i) feeding ethylene and an alpha-olefin comonomer having from 3 to 12 carbon atoms to the gas phase reactor
(ii) further polymerizing the intermediate material
to obtain a base resin (A) which comprises the intermediate material polymerized in step a) and a material polymerized in step b) which has a higher weight average molecular weight as the intermediate material of step a), wherein the base resin (A) has a density of equal to or more than 943 kg/m3 to equal to or less than 957 kg/m3, determined according to ISO 1183,
c) extruding the base resin (A) in the presence of 1 to 10 wt % carbon black (B), based on the amount of the polyethylene composition, and optional further additive(s) (C), into a polyethylene composition having a melt flow rate MFR5 (190° C., 5 kg) of equal to or more than 0.12 g/10 min to equal to or less than 0.20 g/10 min, determined according to ISO 1133 (type II), a shear thinning index SHI2.7/210 of equal to or more than 80 to equal to or less than 130 and a viscosity at a constant shear stress of 747 Pa, eta747, of equal to or more than 700 kPas to equal to or less than 1200 kPas.

### Claim 24 (depends on 12)

An article comprising the polyethylene composition according to claim 12.

### Claim 25 (depends on 24)

The article according to claim 24 being a pipe or pipe fitting, preferably pipe having a wall thickness of at least 60 mm.

### Claim 26 (depends on 23)

An article comprising the polyethylene composition of claim 23.

### Claim 27 (depends on 26)

The article according to claim 26 being a pipe or pipe fitting leaving a wall thickness of at least 60 mm.