# US 2025/0145775 A1 · Synthesis of melamine polyphosphate with low residual melamine

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145775 A1
- Document ID: US20250145775A1
- Status: Published application
- Kind: A1
- Application number: 18/837,978
- Filed: 2023-02-09
- Published: 2025-05-08
- Earliest claimed: 2022-02-18
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Jan Eberhardt; Pascal Guyon; Thomas Esche
- Web page: https://patentgrep.com/patent/US20250145775A1

## CPC

- C08J 3/28: Treatment by wave energy or particle radiation
- C08K 5/5205: {Salts of P-acids with N-bases}
- C08G 79/04: Phosphorus linked to oxygen or to oxygen and carbon
- C08K 2201/019: the composition being defined by the absence of a certain additive
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The present invention relates to a method for producing a melamine depleted melamine polyphosphate which comprises heating a crude melamine polyphosphate for a hold time of at least one hour to a hold temperature of above 290° C.; to a melamine depleted melamine polyphosphate which contains a residual melamine and where the residual melamine concentration is below 0.2 wt %; and to a polymer composition comprising the melamine depleted melamine polyphosphate.

## Claims

### Claim 1

A method for producing a melamine depleted melamine polyphosphate which comprises heating a crude melamine polyphosphate for a hold time of at least one hour to a hold temperature of above 290° C.

### Claim 2 (depends on 1)

The method according to claim 1 where the crude melamine polyphosphate has a residual melamine concentration of at least 0.2 wt % melamine.

### Claim 3 (depends on 1)

The method according to claim 1 where the melamine depleted melamine polyphosphate has a residual melamine concentration of below 0.2 wt %, 0.1 wt % or 0.05 wt %.

### Claim 4 (depends on 1)

The method according to claim 1 where the hold temperature is at least 295, 300, 305, 310 or 315° C.

### Claim 5 (depends on 1)

The method according to claim 1 where the hold time is at least 1, 2, 3, 4 or 5 hours.

### Claim 6 (depends on 1)

The method according to claim 1 where during the hold time the crude melamine polyphosphate is purged with an inert gas or subjected to a vacuum.

### Claim 7 (depends on 1)

The method according to claim 1 where the crude melamine polyphosphate is produced by polymerizing a melamine phosphate for a polymerization time of at least 0.5 hour at a polymerization temperature in the range of 200 to 290° C.

### Claim 8 (depends on 7)

The method according to any of claim 7 where the melamine phosphate contains melamine and phosphoric acid in a molar ratio of 1:1 to 2:1, preferably of 1.2:1 to 1.5:1.

### Claim 9 (depends on 7)

The method according to claim 7 where the melamine phosphate is prepared by heating melamine, phosphoric acid and water above 70° C.

### Claim 10 (depends on 7)

The method according to claim 7 where the melamine phosphate is prepared by adding phosphoric acid and water to a powder of melamine.

### Claim 11 (depends on 1)

The method according to claim 1 where the melamine depleted melamine polyphosphate contains 1 to 30 wt % melam polyphosphate.

### Claim 12

A melamine depleted melamine polyphosphate which contains a residual melamine and where the residual melamine concentration is below 0.2 wt %, 0.1 wt % or 0.05 wt %.

### Claim 13 (depends on 12)

The melamine depleted melamine polyphosphate according to claim 12 which contains 1 to 30 wt % melam polyphosphate.

### Claim 14 (depends on 12)

The melamine depleted melamine polyphosphate according to claim 12 which contains 0.01 to 5.0 wt % melem polyphosphate.

### Claim 15 (depends on 1, 12)

The melamine depleted melamine polyphosphate according to claim 12, where the melamine depleted melamine polyphosphate is obtainable by the method as defined in claim 1 comprising heating the crude melamine polyphosphate for the hold time of at least one hour to the hold temperature of above 290° C.

### Claim 16 (depends on 13)

A polymer composition comprising the melamine depleted melamine polyphosphate as defined in claim 13.