# US 2025/0145770 A1 · Polyarylene sulfide resin composition and molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145770 A1
- Document ID: US20250145770A1
- Status: Published application
- Kind: A1
- Application number: 18/693,939
- Filed: 2022-09-12
- Published: 2025-05-08
- Earliest claimed: 2021-09-28
- Assignees: Toray Industries, Inc.
- Applicants: Toray Industries, Inc.
- Inventors: Tomohiro Atarashi; Hisashi Yamanoue; Kei Saito
- Web page: https://patentgrep.com/patent/US20250145770A1

## CPC

- C08G 75/0209: derived from monomers containing one aromatic ring
- C08K 5/5435: containing oxygen in a ring
- C08K 5/5465: containing at least one C=N bond
- C08L 81/02: Polythioethers; Polythioether-ethers
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polyarylene sulfide resin composition includes: 100 parts by weight of (A) a polyarylene sulfide; and 0.1 to 5 parts by weight of (B) an organic silane coupling agent having at least one epoxy group, an amino group, and an isocyanate group, wherein, when a cumulative integral value from a molecular weight of 100 to 10,000 in a molecular weight distribution curve of (A) the polyarylene sulfide is taken as 100, the cumulative integrated value at a molecular weight of 4,000 is 48 to 53, and when a melt flow rate of (A) the polyarylene sulfide is defined as MFR1, and when the melt flow rate obtained after mixing (A) the polyarylene sulfide with an epoxy silane coupling agent at a weight ratio of 100:1, and heating the resulting mixture at 315.5° C. for 5 minutes is defined as MFR2, a rate of change (MFR2/MFR1) is not more than 0.085.

## Claims

### Claim at position 1

-8. (canceled)

### Claim 9

A polyarylene sulfide resin composition comprising:
100 parts by weight of (A) a polyarylene sulfide; and
0.1 to 5 parts by weight of (B) an organic silane coupling agent having at least one functional group selected from the group consisting of an epoxy group, an amino group, and an isocyanate group,
wherein, when a cumulative integral value from a molecular weight of 100 to a molecular weight of 10,000 in a molecular weight distribution curve of (A) the polyarylene sulfide is taken as 100, the cumulative integrated value at a molecular weight of 4,000 is 48 to 53, and
when a melt flow rate of (A) the polyarylene sulfide is defined as MFR1, and when the melt flow rate obtained after mixing (A) the polyarylene sulfide with an epoxy silane coupling agent at a weight ratio of 100:1, and heating the resulting mixture at 315.5° C. for 5 minutes is defined as MFR2, a rate of change represented by MFR2/MFR1 is not more than 0.085.

### Claim 10

A polyarylene sulfide resin composition comprising:
100 parts by weight of (A) a polyarylene sulfide; and
1 to 50 parts by weight of (C) an olefin elastomer,
wherein, when a cumulative integral value from a molecular weight of 100 to a molecular weight of 10,000 in a molecular weight distribution curve of (A) the polyarylene sulfide is taken as 100, the cumulative integrated value at a molecular weight of 4,000 is 48 to 53, and
when a melt flow rate of (A) the polyarylene sulfide is defined as MFR1, and when the melt flow rate obtained after mixing (A) the polyarylene sulfide with an epoxy silane coupling agent at a weight ratio of 100:1, and heating the resulting mixture at 315.5° C. for 5 minutes is defined as MFR2, a rate of change represented by MFR2/MFR1 is not more than 0.085.

### Claim 11 (depends on 10)

The polyarylene sulfide resin composition according to claim 10, wherein, in a phase structure of the polyarylene sulfide resin composition, (A) the polyarylene sulfide is a continuous phase, (C) the olefin elastomer is an island phase, and a number average dispersion particle diameter of (C) the olefin elastomer is 10 to 300 nm.

### Claim 12 (depends on 9)

The polyarylene sulfide resin composition according to claim 9, wherein (A) the polyarylene sulfide has a crosslinked structure.

### Claim 13 (depends on 12)

The polyarylene sulfide resin composition according to claim 12, wherein, when (A) the polyarylene sulfide having a crosslinked structure is dissolved in a 20-fold weight of 1-chloronaphthalene at 250° C. over a period of 5 minutes, and subjected to heat pressure filtration through a PTFE membrane filter having a pore size of 1 μm, the amount of the resulting residue is not more than 4.0% by weight.

### Claim 14 (depends on 9)

A molded article composed of the polyarylene sulfide resin composition according to claim 9.

### Claim 15 (depends on 14)

The molded article according to claim 14, wherein the molded article is any water plumbing part selected from toilet-related parts, water heater-related parts, bath-related parts, pump-related parts, underfloor heating-related parts, and water meter-related parts.

### Claim 16 (depends on 14)

The molded article according to claim 14, wherein the molded article is any one selected from: an insulating plate for a primary battery or a secondary battery; and a sealing gasket.