# US 2025/0145515 A1 · Low lithium, low thermal expansion high recycled content glasses

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145515 A1
- Document ID: US20250145515A1
- Status: Published application
- Kind: A1
- Application number: 18/928,625
- Filed: 2024-10-28
- Published: 2025-05-08
- Earliest claimed: 2023-11-03
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Jaymin Amin; Carol Ann Click; Timothy Michael Gross; Kristy Lynn Smith; Jingshi Wu
- Web page: https://patentgrep.com/patent/US20250145515A1

## CPC

- C03C 3/091: containing aluminium
- C03C 1/002: {Use of waste materials, e.g. slags}
- C03C 3/118: containing aluminium
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass comprising a coefficient of thermal expansion (CTE) of 70×10−7/° C. or less, a liquidus viscosity of at least 150 kP, and Li2O in an amount of 0.1 wt. % or less, wherein the glass is ion-exchangeable. A glass, comprising SiO2 in an amount of 64-73 wt. %, Al2O3 in an amount of 7-15 wt. %, B2O3 in an amount of 9-11 wt. %, Na2O in an amount of 6-9.5 wt. %, K2O in an amount of 0.5-3 wt. %, CaO in an amount of at least 0.05 wt. %, and Li2O in an amount of less than 0.1 wt. %, wherein a weight ratio of Na2O/Al2O3 is less than or equal to 0.9. A method of recycling glass, the method comprising heating a composition to form a melt, the composition comprising glass cullet in an amount of at least 60 wt. %, and raw materials in an amount of 40 wt. % or less.

## Claims

### Claim 1

A glass, comprising:
SiO2 in an amount of 64-73 wt. %;
Al2O3 in an amount of 7-15 wt. %;
B2O3 in an amount of 9-11 wt. %;
Na2O in an amount of 6-9.5 wt. %;
K2O in an amount of 0.5-3 wt. %; and
CaO in an amount of at least 0.05 wt. %;
Li2O in an amount of 0.1 wt. % or less;
wherein a weight ratio of Na2O/Al2O3 is less than or equal to 0.9.

### Claim 2 (depends on 1)

The glass of claim 1, comprising:
SiO2 in an amount of 66-72 wt. %;
Al2O3 in an amount of 8-14 wt. %;
Na2O in an amount of 6.5-9 wt. %;
K2O in an amount of 1-2.5 wt. %; and
CaO in an amount of 0.1-5 wt. %;

### Claim 3 (depends on 1)

The glass of claim 1, comprising:
CaO in an amount of 0.1-2 wt. % MgO in an amount of 0-1 wt. %; and
SnO2 in an amount of 0-1 wt. %.

### Claim 4 (depends on 1)

The glass of claim 1, comprising at least one of:
a coefficient of thermal expansion (CTE) of 70×10−7/° C. or less; and
a liquidus viscosity of at least 150 kP.

### Claim 5 (depends on 1)

The glass of claim 1, wherein the Young's modulus is at least 60 GPa.

### Claim 6 (depends on 1)

The glass of claim 1, wherein the CTE is at least 44×10−7/° C.

### Claim 7 (depends on 1)

The glass of claim 1, comprising a 200 P temperature of 1800° C. or less.

### Claim 8 (depends on 1)

The glass of claim 1, comprising a 35,000 P temperature of at least 1000° C.

### Claim 9 (depends on 1)

The glass of claim 1, comprising a strain point of at least 525° C.

### Claim 10 (depends on 1)

The glass of claim 1, comprising a liquidus temperature of 1000° C. or less.

### Claim 11 (depends on 1)

The glass of claim 1, comprising a liquidus viscosity of 18,000 kP or less.

### Claim 12 (depends on 1)

The glass of claim 1, wherein, when the glass has a thickness of 1 mm and is subjected to a single step ion exchange in a 100 wt. % KNO3 molten salt bath at 430-450° C., the glass achieves a maximum compressive stress of 300-600 MPa and a depth of layer (DOL) of at least 8 μm within 1 hour.

### Claim 13 (depends on 1)

The glass of claim 1, wherein the glass is substantially free of Li2O.

### Claim 14 (depends on 1)

A method of chemically strengthening a glass-based substrate, the method comprising:
ion exchanging the glass-based substrate in a molten salt bath to form a glass-based article;
wherein the glass-based article comprises:
a maximum compressive stress (CS) of 300-600 MPa; and
a depth of layer (DOL) of 5-30 μm;
wherein the glass-based substrate comprises the glass of claim 1.

### Claim 15 (depends on 14)

The method of claim 14, wherein the ion-exchanging takes place for 2 hours or less.

### Claim 16 (depends on 14)

The method of claim 14, wherein the molten salt bath comprises at least 95 wt. % KNO3 and a temperature of at least 400° C.

### Claim 17 (depends on 1)

A glass-based article, comprising:
a maximum compressive stress (CS) of 300-600 MPa;
a depth of layer (DOL) of 5-30 μm; and
a composition at a center of the glass-based article;
wherein the composition at the center of the glass-based article comprises the glass of claim 1.

### Claim 18 (depends on 17)

A consumer electronic device comprising:
a housing having a front surface, a back surface, and side surface;
electrical components provided at least partially within the housing, the electrical components including at least a controller, a memory, and a display, the display being provided at or adjacent to a front surface of the housing; and
a cover glass disposed over the display,
wherein at least one of a portion of the housing or the cover glass comprises the glass-based article of claim 17.

### Claim 19 (depends on 1)

A method of recycling glass, the method comprising:
heating a composition to form a melt, the composition comprising:
glass cullet in an amount of at least 60 wt. %; and
raw materials in an amount of 40 wt. % or less;
based on total weight of the composition;
wherein, when the melt is formed and cooled to form a glass-based substrate, the glass-based substrate is the glass of claim 1.

### Claim 20

A composition, comprising:
glass cullet in an amount of at least 60 wt. %; and
raw materials in an amount of 40 wt. % or less;
based on total weight of the composition
wherein the glass cullet comprises:
SiO2 in an amount of 65-80 wt. %;
Al2O3 in an amount of 1-10 wt. %;
B2O3 in an amount of 5-15 wt. %;
Na2O in an amount of 1-10 wt. %;
K2O in an amount of 0.1-5;
CaO in an amount of 0.05-10 wt. %; and
Li2O in an amount of less than 0.1 wt. %;
based on total weight of glass cullet; and
wherein the raw materials comprise at least one of:
SiO2;
Na2CO3; and
Al2O3.