# US 2025/0145493 A1 · Systems and methods for preparing electrode materials via aerosol decomposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145493 A1
- Document ID: US20250145493A1
- Status: Published application
- Kind: A1
- Application number: 18/933,762
- Filed: 2024-10-31
- Published: 2025-05-08
- Earliest claimed: 2023-11-03
- Assignees: Stratus Materials Inc.
- Applicants: Stratus Materials Inc.
- Inventors: Jared Mitchell; Jay F. Whitacre
- Web page: https://patentgrep.com/patent/US20250145493A1

## CPC

- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 45/1228: of the type (MnO2)-, e.g. LiMnO2 or Li(MxMn1-x)O2
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods and systems for preparing electrode materials such as lithium-rich metal oxide materials, including the decomposition (e.g., via aerosol decomposition) of precursor materials, are generally provided.

## Claims

### Claim 1

A method for synthesizing transition metal oxide electrode materials and/or precursors thereof, the method comprising:
aerosolizing a precursor composition in an environment having a temperature of greater than or equal to 500° C. and less than or equal to 900° C., the precursor composition comprising particles comprising one or more metal cations and one or more anions, such that at least a portion of the one or more anions are removed, thereby forming a decomposed precursor powder
wherein the one or more metal cations are selected from the group consisting of manganese, nickel, cobalt, lithium, sodium, potassium, magnesium, calcium, aluminum, and iron.

### Claim 2 (depends on 1)

The method of claim 1, wherein the one or more anions are selected from the group consisting of carboxylate-containing anions, nitrates, and sulfates.

### Claim 3 (depends on 1)

The method of claim 1, wherein the one or more anions are selected from the group consisting of carboxylate-containing anions and nitrates.

### Claim 4 (depends on 1)

The method of claim 1, further comprising, prior to the aerosolizing, a step of removing at least some liquid from a pre-drying precursor composition comprising a liquid and the metal cations and anions dissolved in the liquid, thereby forming the particles comprising metal cations and anions.

### Claim 5 (depends on 4)

The method of claim 4, wherein the pre-drying precursor composition comprises a homogeneous solution comprising the liquid and the metal cations and anions dissolved in the solution.

### Claim 6 (depends on 4)

The method of claim 4, wherein the pre-drying precursor composition comprises a solvated gel of the metal cations and the anions.

### Claim 7

(canceled)

### Claim 8 (depends on 4)

The method of claim 4, wherein the removing at least some of the liquid comprises atomizing the pre-drying precursor composition and/or passing the pre-drying precursor composition through a spray nozzle.

### Claim 9

(canceled)

### Claim 10 (depends on 4)

The method of claim 4, wherein the removing at least some of the liquid comprises generating first droplets comprising the precursor composition having a first average largest cross-sectional dimension and generating second droplets comprising the precursor composition having a second, different average largest cross-sectional dimension.

### Claim 11 (depends on 4)

The method of claim 4, wherein the liquid comprises water in an amount of greater than or equal to 50 wt %.

### Claim 12 (depends on 1)

The method of claim 1, wherein an amount of the precursor composition subjected to the aerosolizing that is converted to a plasma during any step of the method is less than or equal to 1 wt % or is zero.

### Claim 13 (depends on 1)

The method of claim 1, wherein at least some of the one or more metal cations are Li+.

### Claim 14

(canceled)

### Claim 15 (depends on 1)

The method of claim 1, wherein at least some of the metal cations comprise Mn2+ and/or Ni2+.

### Claim 16 (depends on 1)

The method of claim 1, wherein at least some of the one or more anions are carboxylate-containing anions.

### Claim at position 17

-19. (canceled)

### Claim 20 (depends on 1)

The method of claim 1, wherein at least some of the one or more anions are sulfates.

### Claim at position 19

-22. (canceled)

### Claim 23 (depends on 1)

The method of claim 1, wherein the decomposed precursor powder comprises particles have an average largest cross-sectional dimension that is no greater than the average largest cross-sectional dimension of the particles of the precursor composition.

### Claim 24 (depends on 1)

The method of claim 1, further comprising heating at least some of the decomposed precursor powder in an environment having a temperature of greater than 600° C., thereby forming a thermally-processed powder.

### Claim 25

(canceled)

### Claim 26 (depends on 24)

The method of claim 24, wherein the thermally processed powder comprises a lithium transition metal oxide, wherein the lithium transition metal oxide comprises a lithium-rich metal oxide (LRMO) material.

### Claim 27

(canceled)

### Claim 28 (depends on 26)

The method of claim 26, wherein the LRMO material is represented by the formula:
Lix(MnyNi1-y)2-xO2,
wherein x is greater than 1.0 and less than 1.25, and y is less than or equal to 0.95 and greater than or equal to 0.1.

### Claim 29 (depends on 24)

The method of claim 24, wherein the thermally processed powder comprises a lithium transition metal oxide, wherein the lithium transition metal oxide comprises a substituted lithium-rich metal oxide (S-LRMO) material.

### Claim 30 (depends on 29)

The method of claim 29, wherein the S-LRMO material is represented by the formula:
Li[LixAyMz]Ob,
wherein:
A comprises at least one of Na, K, Ca, or Mg,
(x+y) is greater than 0 and less than 0.3,
y>0.05,
z
=
1
-
(
x
+
y
)
,
M comprises Mn and Ni, and
b is greater than or equal to 1.8 and less than or equal to 2.2.

### Claim 31

(canceled)

### Claim 32 (depends on 24)

The method of claim 24, further comprising quenching the thermally processed powder, thereby forming a quenched powder, optionally wherein the quenching occurs in less than or equal to 500 microseconds, and optionally wherein the quenching comprises exposing the thermally processed powder to a quenching liquid.

### Claim at position 30

-35. (canceled)

### Claim 36 (depends on 32)

The method of claim 32, further comprising incorporating the quenched powder into an electrode.

### Claim 37 (depends on 4)

The method of claim 4, wherein the precursor composition is a first precursor composition, the decomposed precursor powder is a first decomposed precursor powder, the one or more cations are one or more first cations, the one or more anions are one or more first anions, the pre-drying precursor composition is a first pre-drying precursor composition, the liquid is a first liquid, and the method further comprises:
forming a second pre-drying precursor composition comprising a second liquid and one or more second metal cations and one or more second anions dissolved in the second liquid, the second pre-drying precursor composition formed at least in part by exposing a species comprising the one or more second metal cations to a gaseous species formed from at least some of the one or more first anions removed during the aerosolizing the first precursor composition, wherein the one or more second anions are a reaction product resulting from the exposing the species comprising the one or more second metal cations to the gaseous species;
removing at least some of the second liquid from the second pre-drying precursor composition, thereby forming the particles comprising the one or more second metal cations and the one or more second anions; and
aerosolizing the second precursor composition in an environment having a temperature of greater than or equal to 500° C. and less than or equal to 900° C., the second precursor composition comprising the particles comprising the one or more second metal cations and the one or more second anions, such that at least a portion of the one or more second anions are removed, thereby forming a second decomposed precursor powder.

### Claim 38

(canceled)

### Claim 39

A system, comprising:
a dryer comprising an atomizer and/or spray nozzle, the dryer configured to receive a pre-drying precursor composition and produce particles from the pre-drying precursor composition to form a dried composition having less liquid than the pre-drying precursor composition;
an aerosolizer configured to:
receive at least some of the dried composition; and
aerosolize the at least a some of the dried composition in an environment having a temperature of greater than or equal to 500° C. and less than or equal to 900° C. to form a decomposed precursor powder.

### Claim at position 35

40-42. (canceled)

### Claim 43

A method, comprising:
aerosolizing a solid precursor composition in an environment having a temperature of greater than or equal to 500° C. and less than or equal to 900° C., the precursor composition comprising particles comprising one or more metal cations and one or more anions, such that at least a portion of the one or more anions are removed, thereby forming a decomposed precursor powder.