# US 2025/0145492 A1 · Cathode material for sodium-ion batteries, preparation method therefor, and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145492 A1
- Document ID: US20250145492A1
- Status: Published application
- Kind: A1
- Application number: 18/832,651
- Filed: 2023-04-10
- Published: 2025-05-08
- Earliest claimed: 2023-02-27
- Assignees: Jingmen Gem Co., Ltd.; Gem Co., Ltd.
- Applicants: Jingmen Gem Co., Ltd; Gem Co., Ltd
- Inventors: Kaihua XU; Kun ZHANG; Zhaojian SUN; Cong LI; Wenguang WANG
- Web page: https://patentgrep.com/patent/US20250145492A1

## CPC

- C01G 53/51: containing sodium
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/362: {Composites}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- C01P 2002/54: one element only
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are a cathode material for sodium-ion batteries, a preparation method therefor, and an application thereof, and the preparation method comprises the following steps: (1) mixing a nickel source, a manganese source, and a magnesium source to obtain a ternary salt solution, adding the ternary salt solution, a precipitating agent, a complexing agent, a boron source solution, and an organic additive to a reaction vessel in parallel flow, and performing a reaction to obtain a B-doped radially-packed hydroxide precursor; and (2) mixing the B-doped radially-packed hydroxide precursor obtained in step (1) with a sodium source, and performing sintering treatment to obtain the cathode material for sodium-ion batteries. In the present application, the chemical composition (B-doping) and microscopic morphology (radial-packed arrangement of primary particles) of the cathode material are synergistically modified and regulated by optimizing the co-precipitation process, so as to improve the element distribution uniformity, structure stability, cycle performance, rate capability, and production efficiency of the cathode material for sodium-ion batteries simultaneously.

## Claims

### Claim 1

A preparation method for a cathode material for sodium-ion batteries, which comprises the following steps:
(1) mixing a nickel source, a manganese source, and a magnesium source to obtain a ternary salt solution, adding the ternary salt solution, a precipitating agent, a complexing agent, a boron source solution, and an organic additive to a reaction vessel in parallel flow, and performing a reaction to obtain a B-doped radially-packed hydroxide precursor;
the precipitating agent comprises a sodium hydroxide solution with a concentration of 6-10 mol/L;
the complexing agent comprises any one or a combination of at least two of aqueous ammonia, oxalic acid, sodium oxalate, or salicylic acid;
the organic additive comprises any one or a combination of at least two of ethanol, ethylene glycol, or cetyltrimethylammonium bromide;
the reaction is performed at a pH of 9-12;
for a system of the reaction, the complexing agent has a concentration of 1.5-3.0 mmol/L; and
(2) mixing the B-doped radially-packed hydroxide precursor obtained in step (1) with a sodium source, and performing sintering treatment to obtain the cathode material for sodium-ion batteries.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the nickel source in step (1) comprises any one or a combination of at least two of nickel sulfate, nickel chloride, or nickel nitrate.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the manganese source in step (1) comprises any one or a combination of at least two of manganese sulfate, manganese chloride, or manganese nitrate.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the magnesium source in step (1) comprises any one or a combination of at least two of magnesium sulfate, magnesium chloride, or magnesium nitrate.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein metal ions in the ternary salt solution in step (1) have a total concentration of 0.5-2.0 mol/L.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein the complexing agent in step (1) has a concentration of 0.1-0.5 mol/L.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein a solute of the boron source solution in step (1) comprises any one or a combination of at least two of boric acid, boron oxide, or sodium borate.

### Claim 9

(canceled)

### Claim 10 (depends on 1)

The preparation method according to, claim 1, wherein the ternary salt solution in step (1) has a flow rate of 7-9 L/h;
the precipitating agent in step (1) has a flow rate of 2-4 L/h;
the complexing agent in step (1) has a flow rate of 1-1.5 L/h;
the boron source solution in step (1) has a flow rate of 0.05-0.15 L/h;
the organic additive in step (1) has a flow rate of 0.1-0.3 L/h.

### Claim 11 (depends on 1)

The preparation method according to claim 1, wherein the reaction in step (1) is performed at a temperature of 30-60° C.

### Claim 12 (depends on 11)

The preparation method according to claim 11, wherein a washing agent of the washing in step (1) comprises any one or a combination of at least two of hot water, liquid sodium hydroxide, or ethanol.

### Claim 13 (depends on 1)

The preparation method according to claim 1, wherein the B in the B-doped radially-packed hydroxide precursor in step (1) has a doping amount of 2000-10000 ppm.

### Claim 14 (depends on 1)

The preparation method according to claim 1, wherein the sodium source in step (2) comprises sodium hydroxide and/or sodium carbonate.

### Claim 15 (depends on 1)

A cathode material for sodium-ion batteries, which is prepared by the method according to any one of claim 1.

### Claim 16 (depends on 15)

A cathode sheet, which comprises the cathode material for sodium-ion batteries according to claim 15.

### Claim 17 (depends on 16)

A sodium-ion battery, which comprises the cathode sheet according to claim 16.

### Claim 18 (depends on 1)

The preparation method according to claim 1, wherein the boron source solution in step (1) has a concentration of 1-3 mol/L

### Claim 19 (depends on 1)

The preparation method according to claim 1, wherein the reaction in step (1) is performed at a stirring rate of 250-400 rpm.

### Claim 20 (depends on 1)

The preparation method according to claim 1, wherein washing and drying are carried out after the reaction in step (1).

### Claim 21 (depends on 14)

The preparation method according to claim 14, wherein a molar ratio of the sodium source to the hydroxide precursor is 1-1.2 in step (2).

### Claim 22 (depends on 1)

The preparation method according to claim 1, wherein the sintering treatment in step (2) is performed at a temperature of 800-1000° C.;
the sintering treatment in step (2) is performed for a period of 10-20 h.