# US 2025/0145487 A1 · Chlorine Recycle Process for Titanium-Bearing Feedstocks with High Iron Contents for the Production of Titanium Tetrachloride Based on the Conversion of Anhydrous Ferrous Chloride to Ferrous Sulfate with concentrated Sulfuric Acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145487 A1
- Document ID: US20250145487A1
- Status: Published application
- Kind: A1
- Application number: 18/386,903
- Filed: 2023-11-03
- Published: 2025-05-08
- Earliest claimed: 2021-05-06
- Assignees: Kronos International, Inc.
- Applicants: Kronos International, Inc.
- Inventors: Mitja Medved; Thomas Pierau
- Web page: https://patentgrep.com/patent/US20250145487A1

## CPC

- C01G 23/07: Producing by vapour phase processes, e.g. halide oxidation
- C01G 49/10: Halides {(C01G49/0018 takes precedence)}
- C01B 7/04: Preparation of chlorine from hydrogen chloride
- C01G 23/022: {Titanium tetrachloride}
- C01G 23/024: {Purification of tetrachloride}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

The invention relates to a method for recycling chlorine in the production of titanium tetrachloride. Further, the invention refers to the use of this method in the chloride process to produce titanium dioxide.

## Claims

### Claim 1

A method for recycling chlorine in the production of titanium tetrachloride, comprising:
a) contacting chlorine with a titanium-bearing feedstock which comprises iron to obtain a chloride mixture comprising ferrous chloride and titanium tetrachloride,
b) separating the ferrous chloride from the chloride mixture,
c) contacting the ferrous chloride with an aqueous solution of concentrated sulfuric acid to obtain iron sulfate and gaseous hydrochloric acid,
d) converting at least a portion of the obtained gaseous hydrochloric acid into chlorine, and
e) using at least a portion of the chlorine obtained in step d) in step a).

### Claim 2 (depends on 1)

The method of claim 1, wherein step c) is conducted at a temperature of between about 60° C. and about 120° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein the temperature is from about 75° C. to about 105° C.

### Claim 4 (depends on 3)

The method of claim 3, wherein the temperature is from about 90° C. to about 100° C.

### Claim 5 (depends on 1)

The method of claim 1 wherein in step c) water is added to the ferreous chloride to obtain iron sulfate monohydrate.

### Claim 6 (depends on 1)

The method of claim 1, wherein the aqueous solution of concentrated sulfuric acid used in step c) has a sulfuric acid concentration of from about 78.0 wt. % to about 84.5 wt. % based on the total weight of the aqueous solution is used.

### Claim 7 (depends on 1)

The method of claim 1, wherein the titanium-bearing feedstock comprises up to about 70 wt. % iron based on the total weight of titanium-bearing feedstock.

### Claim 8 (depends on 7)

The method of claim 7, wherein the titanium-bearing feedstock comprises up to about 60 wt. % iron based on the total weight of titanium-bearing feedstock.

### Claim 9 (depends on 8)

The method of claim 8, wherein the titanium-bearing feedstock comprises up to about 50 wt. % iron based on the total weight of titanium-bearing feedstock.

### Claim 10 (depends on 1)

The method of claim 1, wherein at least a portion of the gaseous hydrochloric acid obtained in step c) is mixed with the ferrous chloride obtained in step b) to obtain an aqueous ferrous chloride suspension.

### Claim 11 (depends on 1)

The method of claim 1, wherein the titanium-bearing feedstock is selected from the group consisting of ilmenites, perovskites, rutiles, titanites or a mixture thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein step d) is conducted at an elevated temperature in the presence of a catalyst.

### Claim 13 (depends on 1)

The method of claim 1, wherein electrolysis is used in step d).

### Claim 14 (depends on 1)

The method of claim 1, further comprising:
f) reacting the titanium tetrachloride with oxygen to obtain titanium dioxide.

### Claim 15 (depends on 1)

Use of the method of claim 1 in the chloride process to obtain titanium dioxide.

### Claim 16 (depends on 1)

The method of claim 1, wherein:
the titanium-bearing feedstock is selected from the group consisting of ilmenites, perovskites, rutiles, titanites or a mixture thereof and comprises up to about 70 wt. % iron based on the total weight of titanium-bearing feedstock;
the aqueous solution of concentrated sulfuric acid used in step c) has a sulfuric acid concentration of from about 78.0 wt. % to about 84.5 wt. % based on the total weight of the aqueous solution is used;
wherein step c) is conducted at a temperature of between about 60° C. and about 120° C.

### Claim 17 (depends on 16)

The method of claim 16, wherein step c) is conducted at a temperature of between about 90° C. and about 100° C.