# US 2025/0145479 A1 · Methods for making zeolite-y particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145479 A1
- Document ID: US20250145479A1
- Status: Published application
- Kind: A1
- Application number: 18/500,528
- Filed: 2023-11-02
- Published: 2025-05-08
- Earliest claimed: 2023-11-02
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Faisal Alotaibi; Lianhui Ding; Mohammad F. Aljishi
- Web page: https://patentgrep.com/patent/US20250145479A1

## CPC

- C01B 39/24: Type Y {(C01B39/205 takes precedence)}
- B01J 6/001: {Calcining}
- B01J 29/084: {Y-type faujasite}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01P 2004/60: Particles characterised by their size
- C01P 2006/12: Surface area
- C01P 2006/14: Pore volume
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method of making zeolite-Y particles may include dissolving a silica source material into a first solvent to form a first solution and dissolving an alumina source material into a second solvent to form a second solution. The method may also include combining the first solution with the second solution to form a combined mixture. The combined mixture may include a templating agent. The method may include aging the combined mixture for a time period of from 10 hours to 30 hours to form a zeolite precursor solution and heating the zeolite precursor solution at a temperature of from 50° C. to 70° C. to form an intermediate mixture. The method may include heating the intermediate mixture at a temperature of from 80° C. to 120° C. to form the zeolite-Y particles.

## Claims

### Claim 1

A method for making zeolite-Y particles, the method comprising:
dissolving a silica source material into a first solvent to form a first solution;
dissolving an alumina source material into a second solvent to form a second solution;
combining the first solution with the second solution to form a combined mixture, wherein the combined mixture comprises a templating agent;
aging the combined mixture for a time period of from 10 hours to 30 hours to form a zeolite precursor solution;
heating the zeolite precursor solution at a temperature of from 50° C. to 70° C. to form an intermediate mixture; and
heating the intermediate mixture at a temperature of from 80° C. to 120° C. to form the zeolite-Y particles.

### Claim 2 (depends on 1)

The method of claim 1, wherein the templating agent is one or more of tetramethylammonium hydroxide, tetraethylammonium hydroxide, tetrapropylammonium hydroxide, tetraethylammonium bromide, and tetrapropylammonium bromide.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first solution comprises tetramethylammonium hydroxide, water, and the silica source material.

### Claim 4 (depends on 1)

The method of claim 1, wherein the second solution comprises the tetramethylammonium hydroxide, the alumina source material, water, and a basic compound.

### Claim 5 (depends on 4)

The method of claim 4, wherein the basic compound is NaOH.

### Claim 6 (depends on 1)

The method of claim 1, wherein aging the mixture comprises stirring the mixture at a temperature of from 20° C. to 40° C. for a time period of from 15 hours to 25 hours.

### Claim 7 (depends on 1)

The method of claim 1, wherein the zeolite precursor solution is heated for a time period of from 12 hours to 24 hours.

### Claim 8 (depends on 1)

The method of claim 1, wherein the intermediate mixture is heated for a time period of from 12 hours to 24 hours.

### Claim 9 (depends on 1)

The method of claim 1, wherein the alumina source material is chosen from one or more of, Al2(SO4)3, Al(NO3)3, AlCl3, NaAlO2, or Al2O3.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silica source material is chosen from one or more of colloidal silica, fumed silica, tetraethyl orthosilicate, or Na2SiO4.

### Claim 11 (depends on 1)

The method of claim 1, wherein one or both of the zeolite precursor solution and the intermediate mixture are not heated using microwave heating.

### Claim 12 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average particle size of from 30 nm to 100 nm.

### Claim 13 (depends on 1)

The method of claim 1, wherein greater than 95% of the zeolite-Y particles have a particle size of from 30 nm to 100 nm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average pore size of from 6 nm to 8 nm.

### Claim 15 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have a total pore volume of from 0.5 ml/g to 1 ml/g.

### Claim 16 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have a total mesopore volume of from 0.7 ml/g to 0.9 ml/g.

### Claim 17 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average surface area of at least 600 m2/g.

### Claim 18 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average surface area of from 600 m2/g to 800 m2/g.

### Claim 19 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have a relative crystallinity of greater than 80%.

### Claim 20 (depends on 1)

The method of claim 1, further comprising:
washing the zeolite-Y particles;
drying the zeolite-Y particles; and
calcinating the zeolite-Y particles.