# US 2025/0145478 A1 · Methods for making zeolite-y particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145478 A1
- Document ID: US20250145478A1
- Status: Published application
- Kind: A1
- Application number: 18/500,513
- Filed: 2023-11-02
- Published: 2025-05-08
- Earliest claimed: 2023-11-02
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Faisal Alotaibi; Lianhui Ding
- Web page: https://patentgrep.com/patent/US20250145478A1

## CPC

- C01B 39/24: Type Y {(C01B39/205 takes precedence)}
- B01J 6/001: {Calcining}
- B01J 29/084: {Y-type faujasite}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01P 2004/60: Particles characterised by their size
- C01P 2006/12: Surface area
- C01P 2006/14: Pore volume
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for making zeolite-Y particles may include forming an initial zeolite precursor solution including an initial alumina source material and a silica source material in a solvent. The method may also include heating the initial zeolite precursor solution at a temperature of at least 50° C. to form an intermediate mixture. The method may also include adding additional alumina source material to the intermediate mixture. Following the adding of the additional alumina source material to the intermediate mixture, the intermediate mixture may be heated at a temperature of at least 50° C. to form zeolite-Y particles.

## Claims

### Claim 1

A method for making zeolite-Y particles, the method comprising:
forming an initial zeolite precursor solution comprising an initial alumina source material and a silica source material in a solvent;
heating the initial zeolite precursor solution at a temperature of at least 50° C. to form an intermediate mixture;
adding additional alumina source material to the intermediate mixture; and
following the adding of the additional alumina source material to the intermediate mixture, heating the intermediate mixture at a temperature of at least 50° C. to form zeolite-Y particles.

### Claim 2 (depends on 1)

The method of claim 1, wherein the initial alumina source material is chosen from one or more of NaAlO2, Al2(SO4)3, Al(NO3)3, AlCl3, or Al2O3.

### Claim 3 (depends on 1)

The method of claim 1, wherein the additional alumina source material is chosen from one or more of NaAlO2, Al2(SO4)3, Al(NO3)3, AlCl3, or Al2O3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the additional alumina source material has the same composition as the initial alumina source material.

### Claim 5 (depends on 1)

The method of claim 1, wherein the additional alumina source material has a different composition than the initial alumina source material.

### Claim 6 (depends on 1)

The method of claim 1, wherein the method does not utilize an organic structure-directing agent.

### Claim 7 (depends on 1)

The method of claim 1, wherein the heating of the initial zeolite precursor solution is at a temperature of from 50° C. to 70° C. for a time period of from 12 hours to 24 hours.

### Claim 8 (depends on 1)

The method of claim 1, wherein the heating of the intermediate mixture is at a temperature of from 80° C. to 120° C. for a time period of from 12 hours to 24 hours.

### Claim 9 (depends on 1)

The method of claim 1, wherein forming zeolite precursor solution comprises:
mixing a basic compound, the silica source material, and the alumina source material into a solvent to form a mixture; and
aging the mixture by stirring the mixture for at least 10 hours.

### Claim 10 (depends on 9)

The method of claim 9, wherein the solvent is water.

### Claim 11 (depends on 9)

The method of claim 9, wherein aging the mixture comprises stirring the mixture at a temperature of from 20° C. to 40° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein aging the mixture comprises stirring the mixture for from 10 hours to 30 hours.

### Claim 13 (depends on 9)

The method of claim 9, wherein the basic compound is chosen from one or more of NaOH, KOH, or Mg(OH)2.

### Claim 14 (depends on 9)

The method of claim 9, wherein the amount of additional alumina added is the same or different from the amount of alumina source material used to form the mixture.

### Claim 15 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average particle size of from 150 nm to 280 nm.

### Claim 16 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average pore size of from 2 to 5 nm.

### Claim 17 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have a total pore volume of from 0.45 ml/g to 0.7 ml/g.

### Claim 18 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have an average surface area of at least 600 m2/g.

### Claim 19 (depends on 1)

The method of claim 1, wherein the zeolite-Y particles have a relative crystallinity of greater than 75%.

### Claim 20 (depends on 1)

The method of claim 1, further comprising:
washing the zeolite-Y particles;
drying the zeolite-Y particles; and
calcinating the zeolite-Y particles.