# US 2025/0145470 A1 · Synthesis and application of lignin-based carbon materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0145470 A1
- Document ID: US20250145470A1
- Status: Published application
- Kind: A1
- Application number: 18/947,757
- Filed: 2024-11-14
- Published: 2025-05-08
- Earliest claimed: 2022-05-26
- Assignees: University of Tennessee Research Foundation
- Applicants: University of Tennessee Research Foundation
- Inventors: Lu YU; David Paul Harper; David Keffer
- Web page: https://patentgrep.com/patent/US20250145470A1

## CPC

- C01B 32/318: characterised by the starting materials
- C01B 32/342: characterised by non-gaseous activating agents
- B01D 15/165: {Flash chromatography}
- C01B 32/15: Nano-sized carbon materials
- C01B 32/348: Metallic compounds
- C01B 32/354: After-treatment
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- C01P 2002/82: by IR- or Raman-data
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2002/86: by NMR- or ESR-data
- C01P 2004/03: obtained by SEM
- C01P 2006/12: Surface area
- C01P 2006/16: Pore diameter
- C01P 2006/60: Optical properties, e.g. expressed in CIELAB-values
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

This application relates to the development and use of lignin-based carbon materials which can be used for energy storage and environmental applications. Included are methods of preparing microporous activated carbon having a controlled, often high surface area and a controlled often high mesopore ratio, and a method of preparing carbon dots, for example carbon quantum dots.

## Claims

### Claim 1

A method of preparing microporous activated carbon having a controlled surface area, comprising the steps of:
providing a lignin including one or more of softwood lignin, hardwood lignin, and herbaceous lignin;
carbonizing the lignin at an elevated temperature of at least about 700° C. to produce a carbonized lignin; and
activating the carbonized lignin by mixing it with potassium hydroxide at a mass ratio of about 1:3 to about 1:5 and an elevated temperature of at least about 700° C. to yield the microporous activated carbon;
wherein the microporous activated carbon has a controlled surface area of about 50 to about 3500 m2/g and a controlled mesopore ratio of about 10% to about 80%.

### Claim 2 (depends on 1)

The method of claim 1, wherein the lignin comprises the softwood lignin.

### Claim 3 (depends on 2)

The method of claim 2, wherein the softwood lignin is kraft softwood lignin.

### Claim 4 (depends on 1)

The method of claim 1, wherein the microporous activated carbon has a surface area of at least about 3000 m2/g.

### Claim 5 (depends on 4)

The method of claim 4, wherein the microporous activated carbon has a mesopore ratio of at least about 70%.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carbonizing and activating steps occur simultaneously.

### Claim 7 (depends on 6)

The method of claim 6, wherein the simultaneous carbonizing and activating steps comprise mixing the lignin with the potassium hydroxide at a mass ratio of about 1:3 to about 1:5 and heating the mixture in an inert environment at a temperature of about 700° C. to about 900° C. for about 1 hour to about 3 hours.

### Claim 8 (depends on 1)

The method of claim 1, wherein the carbonizing step occurs before the activating step.

### Claim 9 (depends on 8)

The method of claim 8, wherein the carbonizing step comprises heating the lignin to a temperature of about 900° C. to about 1100° C. for at least about 0.5 hour to provide the carbonized lignin and pulverizing the carbonized lignin.

### Claim 10 (depends on 8)

The method of claim 8, wherein the activating step comprises mixing the lignin with the potassium hydroxide at a mass ratio of about 1:3 to about 1:5 and heating the mixture in an inert environment at a temperature of about 700° C. to about 900° C. for about 1 hour to about 3 hours.

### Claim 11 (depends on 8)

The method of claim 8, wherein the microporous activated carbon has a surface area of at least about 1200 m2/g and a mesopore ratio of at least about 25%.

### Claim 12

A method of preparing carbon dots, comprising the steps of:
providing a lignin;
carbonizing the lignin at an elevated temperature of at least about 700° C. in an inert environment for at least about 0.5 hour to produce a carbonized lignin;
physically activating the carbonized lignin at a temperature of about 700° C. to about 800° C. in the presence of steam for at least about 0.5 hour, followed by exposing the activated carbon to carbon dioxide to a temperature of at least about 700° C. for at least about 0.5 hour, to yield activated carbon;
treating the activated carbon with concentrated nitric acid;
washing the activated carbon to obtain neutralized activated carbon;
mixing the neutralized activated carbon with hydrogen peroxide and solvent to yield a mixture;
heating the mixture to at least about 110° C. for at least about 1.5 hours to yield the carbon dots; and
separating the carbon dots from the mixture.

### Claim 13 (depends on 12)

The method of claim 12, wherein the carbon dots comprise carbon quantum dots.

### Claim 14 (depends on 12)

The method of claim 12, wherein the lignin is selected from one or more of softwood lignin, hardwood lignin, and herbaceous lignin.

### Claim 15 (depends on 14)

The method of claim 14, wherein the lignin comprises kraft softwood lignin.

### Claim 16 (depends on 12)

The method of claim 12, wherein the carbonizing step comprises pyrolyzing the lignin in a furnace in an inert atmosphere and the temperature is raised to the elevated temperature using a heating rate of about 10° C. per minute.

### Claim 17 (depends on 12)

The method of claim 12, wherein the separating step comprises centrifuging the mixture to separate the carbon dots.

### Claim 18 (depends on 12)

The method of claim 12, further comprising the step of purifying the carbon dots using flash chromatography.

### Claim 19

A method of preparing microporous activated carbon having a high surface area, comprising the steps of:
providing a softwood lignin;
mixing the softwood lignin with potassium hydroxide at a mass ratio of about 1:3 to about 1:5 and an elevated temperature of about 700° C. to about 900° C. for about 1 hour to about 3 hours to activate the lignin;
simultaneously carbonizing the lignin at the elevated temperature yield the microporous activated carbon;
wherein the microporous activated carbon has a surface area of at least about 2500 m2/g and a mesopore ratio of at least about 70%.

### Claim 20 (depends on 19)

The method of claim 19, wherein the elevated temperature is maintained for about 1.5 hour to about 2.5 hour.

### Claim 21 (depends on 19)

The method of claim 19, wherein the elevated temperature is at least about 800° C.

### Claim 22 (depends on 19)

The method of claim 19, wherein the mass ratio of lignin to potassium hydroxide is about 1:4.

### Claim 23 (depends on 19)

The method of claim 19, wherein the microporous activated carbon has a surface area of at least about 3000 m2/g and a mesopore ratio of at least about 75%.