# US 2025/0144916 A1 · High-strength steel composite galvanized sheet resistant to lme cracking during spot welding, and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0144916 A1
- Document ID: US20250144916A1
- Status: Published application
- Kind: A1
- Application number: 18/838,230
- Filed: 2023-02-17
- Published: 2025-05-08
- Earliest claimed: 2022-02-17
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Ming LEI; Hua PAN; Li WANG; Peng XUE; Zhongqu SUN; Tianhai WU; Chengjie LIU; Yue WU; Zhongling WEN
- Web page: https://patentgrep.com/patent/US20250144916A1

## CPC

- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- B32B 15/18: comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/28: with titanium or zirconium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C25D 3/22: of zinc
- B32B 2311/20: Zinc
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 2251/02: Clad material
- Y02E 30/30: Nuclear fission reactors
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed in the present invention are a high-strength steel composite galvanized sheet resistant to LME cracking during spot welding, and a preparation method therefor. The high-strength steel composite galvanized sheet comprises a high-strength steel body (1), low-carbon steel composite layers (2) and a galvanized layer (3), wherein two low-carbon steel composite layers (2) are respectively compounded and rolled on two surfaces of the high-strength steel body (1), the galvanized layer (3) is formed on the surface of at least one low-carbon steel composite layer (2), and a high-strength steel composite galvanized sheet is thus formed. In the present invention, the low-carbon steel composite layers are compounded and rolled on the surfaces of the high-strength steel body, such that liquid metal is prevented from permeating into a base material along a grain boundary during spot welding; therefore, the sensitivity of the high-strength steel composite galvanized sheet to LME during spot welding is reduced, LME cracking during spot welding is effectively avoided, the problem of LME cracking during spot welding is mitigated, the resistance spot-welding performance of the high-strength steel body is improved, and the mechanical properties of a spot-welded joint are obviously improved.

## Claims

### Claim 1

A composite high-strength galvanized steel plate having resistance to spot-welding LME cracks, which comprises a high-strength steel matrix (1), low carbon steel composite layers (2), and a galvanized layer (3); wherein two low carbon steel composite layers (2) are affixed on two surfaces of the high-strength steel matrix (1) by composite rolling, the galvanized layer (3) is formed on the surface of at least one of the low carbon steel composite layers (2), thereby forming the composite high-strength galvanized steel plate.

### Claim 2 (depends on 1)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, wherein the high-strength steel matrix (1) is a high-strength steel that is sensitive to spot-welding LME having a tensile strength of ≥780 MPa, preferably ≥980 MPa, or ≥1180 MPa.

### Claim 3 (depends on 2)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 2, wherein the high strength steel comprises, by mass percentage, C≥0.1%, Mn≥1.0%, and Si≥0.07%.

### Claim 4 (depends on 2)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 2, wherein the high strength steel comprises, by mass percentage, C: 0.1˜0.3%, Si: 0.4˜2.50%, Mn: 1.0˜11.0% and Al: 0˜2.0%.

### Claim 5 (depends on 2)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 2, wherein the high strength steel is one or more selected from the group consisting of QP steel, TRIP steel, DH steel, 7Mn steel, 10 Mn steel and MS steel.

### Claim 6 (depends on 1)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, wherein the low carbon steel composite layers (2) is a low carbon steel that is not sensitive to spot-welding LME, wherein the low carbon steel comprises C and Mn, by mass percentage, the C content is ≤0.1%, the Mn content is ≤1.1% or Mn≤0.7%, the tensile strength is ≤590 MPa or is in a range of 150˜590 MPa or 150˜340 MPa.

### Claim 7 (depends on 6)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 6, wherein the low carbon steel comprises, by mass percentage, C: 0.001˜0.1%, Si: 0.001˜0.50%, Mn: 0.1˜0.1.1%, Nb: 0˜0.02%, Ti: 0˜0.025%, Ni: 0˜0.025%, Cr: 0˜0.05%, P: ≤0.05%, with a balance of Fe and unavoidable impurities; or the low carbon steel comprises, by mass percentage, C: 0.001˜0.08%, Si: 0.001˜0.05%, Mn: 0.1˜0.7%, Nb: 0˜0.02%, Ti: 0˜0.025%, Ni: 0˜0.025%, Cr: 0˜0.05%, P: ≤0.05%, with a balance of Fe and unavoidable impurities.

### Claim 8 (depends on 6)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 6, wherein the low carbon steel is one or more selected from the group consisting of IF steel, aluminum killed steel, cold-rolled carbon structural steel, phosphorus high-strength steel, bake-hardening steel and low-alloy steel.

### Claim 9 (depends on 1)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, wherein the original slab thickness of the high-strength steel matrix (1) and the original slab thickness of the low carbon steel composite layer (2) satisfy the following formula: L×A+M×B+N×C=T;
wherein, A is the percentage of the original slab thickness of one of the low-carbon steel composite layers (2) to the thickness of the total assembled slab, C is the percentage of the original slab thickness of the other of the low-carbon steel composite layers (2) to the thickness of the total assembled slab, and B is the percentage of the original slab of the high-strength steel matrix (1) to the thickness of the total assembled slab, and A+B+C=100%; wherein the total assembled slab is the total thickness of the original slab comprising the high-strength steel matrix (1) and the two low carbon steel composite layers (2);
wherein L is the tensile strength of one of the low carbon steel composite layers (2) after annealing, N is the tensile strength of the other of the low carbon steel composite layers (2) after annealing, M is the tensile strength of the high-strength steel matrix (1) after annealing;
wherein T is the target tensile strength of the composite high-strength galvanized steel plate;
wherein, the unit of the tensile strength is MPa, and the unit of the thickness is micron.

### Claim 10 (depends on 9)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 9, wherein A:B and C:B are in the range of 1:35.5-1:5.

### Claim 11 (depends on 1)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, wherein:
in the composite high-strength galvanized steel plate, each low carbon steel composite layer (2) has a thickness of 10-200 μm; and/or the galvanized layer (3) has a thickness of 4-26 μm.

### Claim 12 (depends on 1)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, wherein the composite high-strength galvanized steel plate has resistance to spot-welding LME cracks as follows: there are no LME cracks in the joint before the occurrence of welding spatter, and after the occurrence of welding spatter, the length of the Type A LME cracks in the joint does not exceed 10% of the plate thickness and the number is less than 6, the length of the Type D LME cracks does not exceed 3% of the plate thickness, and the number is less than 3, there are no Type B or Type C LME cracks.

### Claim 13 (depends on 1)

A method for preparing the composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 1, which comprises the following steps:
Step 1: taking an original slab of a high-strength steel matrix (1) and original slabs of two low-carbon steel composite layers (2), affixing the original slabs of the two low-carbon steel composite layers (2) to two surfaces of the original slab of the high-strength steel matrix (1), and welding the original slab edges of the two low-carbon steel composite layers (2) with the original slab edge of the high-strength steel matrix (1) to form a total assembled slab;
Step 2: subjecting the total assembled slab to primary rolling after heating through blooming process of thick plate to reduce the thickness of the total assembled slab, and then hot rolling, pickling, cold rolling and annealing, so that the original slab of the high-strength steel matrix and the original slabs of the two low-carbon steel composite layers are metallurgically combined to form a billet having a tensile strength of T;
Step 3: Plating a galvanized layer on at least one side of the billet to form the composite high-strength galvanized steel plate.

### Claim 14 (depends on 13)

The preparing method according to claim 13, wherein in step 1, before the original slab of the two low-carbon steel composite layers (2) and the original slab of the high-strength steel matrix (1) are stacked, the affixing surfaces of the high-strength steel matrix (1) and the two low-carbon steel composite layers (2) need to be polished and cleaned.

### Claim 15 (depends on 2)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 2, wherein the tensile strength of the high-strength steel is 780˜1500 MPa or 1180˜1500 MPa.

### Claim 16 (depends on 3)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 3, wherein the high strength steel comprises, by mass percentage, C≥0.14%, and/or Mn≥1.5%, and/or Si≥0.4%; or
the high strength steel comprises, by mass percentage, C: 0.14˜0.60%, Mn: 1.5˜16%, Si: 0.07˜2.0%; or
the high strength steel comprises, by mass percentage, C: 0.14˜0.30%, Mn: 1.5˜3.5%, Si: 0.4˜2.0%.

### Claim 17 (depends on 6)

The composite high-strength galvanized steel plate having resistance to spot-welding LME cracks according to claim 6, wherein by mass percentage, the low carbon steel comprises C: 0.001˜0.1% and Mn: 0.1˜1.1%.

### Claim 18 (depends on 13)

The preparing method according to claim 13, wherein:
the high-strength steel matrix (1) is a high-strength steel that is sensitive to spot-welding LME having a tensile strength of ≥780 MPa, or ≥980 MPa, or ≥1180 MPa; and/or the high strength steel comprises, by mass percentage, C≥0.1%, Mn≥1.0% and Si≥0.07%, or the high strength steel comprises, by mass percentage, C: 0.14˜0.60%, Mn: 1.5˜16% and Si: 0.07˜2.0%, or the high strength steel comprises, by mass percentage, C: 0.14˜0.30%, Mn: 1.5˜3.5% and Si: 0.4˜2.0%, or the high strength steel comprises, by mass percentage, C: 0.1˜0.3%, Si: 0.4˜2.50%, Mn: 1.0˜11.0% and Al: 0˜2.0%; or
the high strength steel is one or more selected from the group consisting of QP steel, TRIP steel, DH steel, 7Mn steel, 10 Mn steel and MS steel.

### Claim 19 (depends on 13)

The preparing method according to claim 13, wherein the low carbon steel composite layers (2) is a low carbon steel that is not sensitive to spot-welding LME, wherein the low carbon steel comprises C and Mn, by mass percentage, the C content is 0.1%, the Mn content is ≤1.1%, the tensile strength is ≤590 MPa; and/or the low carbon steel comprises, by mass percentage, C: 0.001˜0.1%, Si: 0.001˜0.50%, Mn: 0.1˜0.1.1%, Nb: 0˜0.02%, Ti: 0˜0.025%, Ni: 0˜0.025%, Cr: 0˜0.05%, P: ≤0.05%, with a balance of Fe and unavoidable impurities; or the low carbon steel comprises, by mass percentage, C: 0.001˜0.08%, Si: 0.001˜0.05%, Mn: 0.1˜0.7%, Nb: 0˜0.02%, Ti: 0˜0.025%, Ni: 0˜0.025%, Cr: 0˜0.05%, P: ≤0.05%, with a balance of Fe and unavoidable impurities; or
the low carbon steel is one or more selected from the group consisting of IF steel, aluminum killed steel, cold-rolled carbon structural steel, phosphorus high-strength steel, bake-hardening steel and low-alloy steel.

### Claim 20 (depends on 13)

The preparing method according to claim 13, wherein:
the original slab thickness of the high-strength steel matrix (1) and the original slab thickness of the low carbon steel composite layer (2) satisfy the following formula: L×A+M×B+N×C=T;
wherein, A is the percentage of the original slab thickness of one of the low-carbon steel composite layers (2) to the thickness of the total assembled slab, C is the percentage of the original slab thickness of the other of the low-carbon steel composite layers (2) to the thickness of the total assembled slab, and B is the percentage of the original slab of the high-strength steel matrix (1) to the thickness of the total assembled slab, and A+B+C=100%; wherein the total assembled slab is the total thickness of the original slab comprising the high-strength steel matrix (1) and the two low carbon steel composite layers (2);
wherein L is the tensile strength of one of the low carbon steel composite layers (2) after annealing, N is the tensile strength of the other of the low carbon steel composite layers (2) after annealing, M is the tensile strength of the high-strength steel matrix (1) after annealing;
wherein T is the target tensile strength of the composite high-strength galvanized steel plate;
wherein, the unit of the tensile strength is MPa, and the unit of the thickness is micron.