# US 2025/0144764 A1 · Polishing pad with improved slurry flowability and process for preparing a semiconductor device using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0144764 A1
- Document ID: US20250144764A1
- Status: Published application
- Kind: A1
- Application number: 18/817,224
- Filed: 2024-08-28
- Published: 2025-05-08
- Earliest claimed: 2023-11-06
- Assignees: SK enpulse Co., Ltd.
- Applicants: SK enpulse Co., Ltd.
- Inventors: Yujin SHIN; Jongwook YOON; Joonho AN; Kyunghwan KIM; Jangwon SEO
- Web page: https://patentgrep.com/patent/US20250144764A1

## CPC

- B24B 37/22: characterised by a multi-layered structure
- B24B 37/042: {operating processes therefor}
- B24B 37/24: characterised by the composition or properties of the pad materials
- B24B 37/26: characterised by the shape of the lapping pad surface, e.g. grooved
- H10P 52/402: {of semiconductor materials}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

As specially designed second grooves in a radial form are adopted in addition to first grooves in a concentric form in the polishing pad according to an embodiment, slurry flowability can be improved, and wafer profile and polishing rate can be changed. Accordingly, the polishing pad according to the embodiment can be used in the fabrication of semiconductor devices to enhance process efficiency and product quality.

## Claims

### Claim 1

A polishing pad, which comprises a polishing layer having a polishing surface, wherein the polishing layer comprises a plurality of first grooves having a circular shape and sharing the center of the polishing surface; and a plurality of second grooves formed radially from a position distanced from the center by 10% to 90% of the radius of the polishing surface to the outer periphery, and
when the silicon oxide layer of a silicon wafer is polished using a ceria slurry on the polishing surface, and when the polishing rate is measured at 30 or more random locations, the within-wafer non-uniformity (WIWNU) calculated by the following equation is 15% or less:
W
⁢
I
⁢
W
⁢
N
⁢
U
⁢
(
%
)
=
RR_stdev
RR_avg
×
1
⁢
0
⁢
0
wherein RR_stdev is the standard deviation of the polishing rate (Å/minute) measurements, and RR_avg is the average of the polishing rate (Å/minute) measurements.

### Claim 2 (depends on 1)

The polishing pad of claim 1, wherein the WIWNU is 1% to 8%, and the RR_avg is 2,500 Å/minute to 4,000 Å/minute.

### Claim 3 (depends on 2)

The polishing pad of claim 2, wherein the RR_avg is 3,200 Å/minute to 3,400 Å/minute.

### Claim 4 (depends on 1)

The polishing pad of claim 1, wherein the polishing layer comprises the first grooves in a total of 50 to 150 and the second grooves in a total of 2 to 50.

### Claim 5 (depends on 4)

The polishing pad of claim 4, wherein the width of the first groove is 0.1 mm to 1 mm, and the width of the second groove is 0.5 mm to 1.5 mm.

### Claim 6 (depends on 5)

The polishing pad of claim 5, wherein the depth of the first groove is 0.4 mm to 1.2 mm, and the depth of the second groove is 0.5 mm to 1.5 mm.

### Claim 7 (depends on 1)

The polishing pad of claim 1, wherein the second grooves comprise at least one of (i) to (iii) below:
(i) a plurality of second-A grooves formed radially from a position distanced from the center by 10% to 39% of the radius of the polishing surface to the outer periphery,
(ii) a plurality of second-B grooves formed radially from a position distanced from the center by 40% to 59% of the radius of the polishing surface to the outer periphery, and
(iii) a plurality of second-C grooves formed radially from a position distanced from the center by 60% to 90% of the radius of the polishing surface to the outer periphery.

### Claim 8 (depends on 1)

The polishing pad of claim 1, which further comprises a plurality of third grooves formed radially from the center of the polishing surface to the outer periphery.

### Claim 9 (depends on 8)

The polishing pad of claim 8, wherein the polishing layer comprises the first grooves in a total of 50 to 150, the second grooves in a total of 4 to 50, and the third grooves in a total of 4 5 to 50.

### Claim 10 (depends on 1)

A process for preparing a semiconductor device, which comprises polishing the surface of a semiconductor substrate using the polishing pad of claim 1.