# US 2025/0137165 A1 · Methods and devices for growing crystals with high uniformity without annealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0137165 A1
- Document ID: US20250137165A1
- Status: Published application
- Kind: A1
- Application number: 19/004,488
- Filed: 2024-12-30
- Published: 2025-05-01
- Earliest claimed: 2020-06-05
- Assignees: Meishan Boya Advanced Materials Co., Ltd.
- Applicants: Meishan Boya Advanced Materials Co., Ltd.
- Inventors: Yu WANG; Weiming GUAN; Zhenxing LIANG; Min LI
- Web page: https://patentgrep.com/patent/US20250137165A1

## CPC

- C30B 15/02: adding crystallising materials or reactants forming it in situ to the melt
- C30B 15/002: {Continuous growth}
- C30B 15/10: Crucibles or containers for supporting the melt
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/22: Stabilisation or shape controlling of the molten zone near the pulled crystal; Controlling the section of the crystal
- C30B 29/20: Aluminium oxides
- C30B 29/22: Complex oxides
- C30B 35/007: {Apparatus for preparing, pre-treating the source material to be used for crystal growth}
- C30B 29/28: with formula A3Me5O12 wherein A is a rare earth metal and Me is Fe, Ga, Sc, Cr, Co or Al, e.g. garnets
- C30B 29/34: Silicates
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present disclosure provides a method for crystal growth. The method may include at one of the following operations: weighing reactants for growing an oxide crystal after a first preprocessing operation is performed on the reactants; placing the reactants, on which a second preprocessing operation has been performed, into a crystal growth device after an assembly preprocessing operation is performed on at least one component of the crystal growth device, wherein the at least one component of the crystal growth device includes a crucible, the assembly preprocessing operation includes at least one of a coating operation, an acid soaking and cleaning operation, or an impurity cleaning operation; introducing a protective gas into the crystal growth device after sealing the crystal growth device; activating the crystal growth apparatus to execute the crystal growth; and adding reactant supplements into the crystal growth device in real-time during the crystal growth.

## Claims

### Claim 1

A crystal, wherein
a formula of the crystal is X(1-z)ZzVO4, wherein
X consists of at least one of Ca, Mg, Sr, Mn, Ba, Al, Fe, Re, La, Ce, Rr, Nd, Pm, Sm, Eu, Gd, Td, Dy, Ho, Er, Yb, Tm, Lu, Sc, or Y,
Z consists of at least one of Li, B, Gd, Mg, Ca, Tb, Y, Lu, La, Yb, Sc, Er, or Ga, z=0-1, or
a formula of the crystal is (X1-yYy)3(A1-bBb)5O12, wherein
X consists of at least one of Gd, Lu, Y, La, or Yb,
Y consists of at least one of B, Li, Ga, Gd, Ce, Y, Yb, or Er,
A consists of at least one of Al, Ga, In, or Sc,
B consists of Al, and
y=0-1, b=0-1.

### Claim 2 (depends on 1)

The crystal of claim 1, wherein b=0.1, y=0.003.

### Claim 3 (depends on 1)

The crystal of claim 1, wherein b=0.2, y=0.003.

### Claim 4 (depends on 1)

The crystal of claim 1, wherein
X consists of Y,
Y consists of Yb,
b=1, and
the formula of the crystal is (Y1-yYby)3Al5O12.

### Claim 5 (depends on 4)

The crystal of claim 4, wherein
y=0.0016.

### Claim 6 (depends on 4)

The crystal of claim 4, wherein
y=0.108.

### Claim 7 (depends on 1)

The crystal of claim 1, wherein
X consists of Gd,
Y consists of Ce,
A consists of Ga, and
the formula of the crystal is (Gd1-yCey)3(Ga1-bAlb)5O12.

### Claim 8 (depends on 1)

A method for preparing the crystal of claim 1, comprising:
weighing reactants for growing the crystal after a first preprocessing operation is performed on the reactants;
placing the reactants, on which a second preprocessing operation has been performed, into a crystal growth device after an assembly preprocessing operation is performed on at least one component of the crystal growth device;
introducing a protective gas into the crystal growth device after sealing the crystal growth device;
activating the crystal growth device to execute the crystal growth; and
adding reactant supplements into the crystal growth device in real-time during the crystal growth.

### Claim 9 (depends on 8)

The method of claim 8, wherein the adding the reactant supplements into the crystal growth device in real-time during the crystal growth comprises:
obtaining a weight of the crystal being grown; and
adding the reactant supplements into the crystal growth device at least based on the weight of the crystal being grown.

### Claim 10 (depends on 9)

The method of claim 9, wherein
the reactant supplements include the reactants on which at least the first preprocessing operation has been performed, and
a weight of the reactant supplements is determined at least based on the weight of the crystal being grown and a ratio among the reactants for growing the crystal.

### Claim 11 (depends on 10)

The method of claim 10, wherein
components of the reactant supplements and a ratio among the components of the reactant supplements are respectively consistent with components of the crystal being grown and a ratio among concentrations of the components of the crystal being grown in the crystal growth device when the reactant supplements are added.

### Claim 12 (depends on 8)

The method of claim 8, wherein the reactant supplements are added into the crystal growth device in a seeding process, a necking process, a shouldering process, or a constant diameter growth process of the crystal growth.

### Claim 13 (depends on 8)

The method of claim 8, wherein when the crystal is (X1-yYy)3(A1-bBb)5O12, a reactant containing Y for growing the crystal exceeds 0.01%-10% of a theoretical weight value of the reactant containing Y.

### Claim 14 (depends on 8)

The method of claim 8, wherein
the first preprocessing operation includes a roasting operation under 800-1400° C.

### Claim 15 (depends on 8)

The method of claim 8, wherein
the second preprocessing operation includes at least one of a reactant mixing operation or a pressing operation at room temperature.

### Claim 16 (depends on 8)

The method of claim 8, wherein
when the protective gas is a non-flowing gas, the non-flowing gas includes one of oxygen, nitrogen, and inert gas or a mixed gas of oxygen and one or more of hydrogen, carbon dioxide, carbon monoxide, nitrogen, and inert gas, the non-flowing gas forming a pressure of −0.05 Mpa-0.08 Mpa in the crystal growth device, or
when the protective gas is a flowing gas, the flowing gas includes one of oxygen, nitrogen, and inert gas or a mixed gas of oxygen and one or more of hydrogen, carbon dioxide, carbon monoxide, nitrogen, and inert gas.

### Claim 17 (depends on 16)

The method of claim 16, wherein a flow rate of the flowing gas is 0.01 L/min-50 L/min.

### Claim 18 (depends on 8)

The method of claim 8, wherein the protective gas includes a flowing gas, and
in an early stage of the crystal growth, a volume ratio of oxygen in the flowing gas is 0.001%-20%; and
during a cooling process after the crystal growth,
the volume ratio of oxygen in the flowing gas is 1%-30% when a temperature is in a range of 1400-800° C., and
the volume ratio of oxygen in the flowing gas is 0.001%-20% when the temperature is lower than 800° C.

### Claim 19 (depends on 8)

The method of claim 8, wherein
the at least one component of the crystal growth device includes a crucible;
the assembly preprocessing operation includes at least one of a coating operation, an acid soaking and cleaning operation, or an impurity cleaning operation.

### Claim 20 (depends on 8)

The method of claim 8, wherein
the purity of the reactants is greater than 99%; or
the purity of the reactants is greater than 99.9%; or
the purity of the reactants is greater than 99.99%; or
the purity of the reactants is greater than 99.999%.