# US 2025/0136869 A1 · Robotic liquid crystal elastomers, apparatus, and method of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0136869 A1
- Document ID: US20250136869A1
- Status: Published application
- Kind: A1
- Application number: 18/927,122
- Filed: 2024-10-25
- Published: 2025-05-01
- Earliest claimed: 2023-10-25
- Assignees: Massachusetts Institute of Technology
- Applicants: Massachusetts Institute of Technology
- Inventors: Jack Forman; Ozgun Kilic Afsar; Sarah Nicita; Rosalie Hsin-Ju Lin; Cedric Honnet; Neil Gershenfeld; Hiroshi Ishii
- Web page: https://patentgrep.com/patent/US20250136869A1

## CPC

- C09K 19/3833: {with mesogenic groups in the side chain}
- B01J 27/24: Nitrogen compounds
- B29C 48/022: {characterised by the choice of material}
- B29C 48/05: Filamentary, e.g. strands
- C08F 136/02: the radical having only two carbon-to-carbon double bonds
- B29C 2035/0827: {using UV radiation}
- B29L 2031/48: Wearing apparel
- C09K 2219/01: in the form of fibres, e.g. fibres after polymerisation of LC precursor
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

Liquid Crystal Elastomer (LCE) fibers, an apparatus for manufacturing, and a method for using the apparatus are provided. LCE fibers formed from each of a plurality of resin recipes can undergo reversible temperature driven actuation of the fiber. Each of the resin recipes forms a fiber having a different actuation temperature. The apparatus includes: an extrusion device, a drawing bobbin, a coating basin, a collector bobbin, a first plurality of curing devices, and a second plurality of curing devices, to transform a resin recipe into a LCE fiber. In operation, the extrusion device extrudes the resin through to the first plurality of curing devices for a partial cure. Once in contact with drawing bobbin the resin is coated in a fluid, and then pull through the second plurality of curing devices for a final cure by collector bobbin, where it can be collected and post-processed.

## Claims

### Claim 1

A method of synthesizing a resin used for manufacturing high actuation temperature LCE fibers, the method comprising:
mixing, in a container, about 60-80 wt % of a mesogen, and about 0.4-1 wt % grams of a reaction inhibitor forming a first mixture;
baking, in an oven, the first mixture in the container until the first mixture is melted, wherein the oven an internal temperature of the oven is 110° C.;
mixing, into the container, about 15-30 wt % of a joining molecule and 3-8 wt % of a vinyl cross-linker forming a second mixture;
baking, in the oven, the second mixture in the container until the second mixture is completely clear, or transparent, wherein the internal temperature of the oven is 110° C.;
mixing, into the container, 1-2 wt % of a photoinitiator and 0.2-0.5 wt % of a chemical initiator forming a third mixture; and
centrifuging, the container, for a set time period and at a set rotational speed.

### Claim 2 (depends on 1)

The method of claim 1, wherein the mesogen is 1,4-Bis-[4-(6-acryloyloxyhexyloxy)benzoyloxy]-2methylbenzene (RM82) and the reaction inhibitor is Butylated Hydroxytoluene (BHT).

### Claim 3 (depends on 1)

The method of claim 1, wherein the joining molecule is 2,2-(ethylenedioxy)diethanethiol (EDDET) and the vinyl cross-linker is 1,3,5-triallyl-1,3,5-triazine-2,4,6 (1H,3H,5H)trione (TATATO).

### Claim 4 (depends on 1)

The method of claim 1, wherein the photo-initiator is 2,2-dimethoxy-2-phenylacetophenone (I-651) and the chemical initiator is Dipropylamine (DPA).

### Claim 5 (depends on 1)

The method of claim 1, wherein the set time period is 3 minutes, and the set rotational speed is 3000 revolutions per minute.

### Claim 6 (depends on 1)

A resin made by the method of claim 1.

### Claim 7

A method of synthesizing a resin used for manufacturing low actuation temperature LCE fibers, the method comprising:
mixing, in a first container, about 46 wt % of a mesogen, about 15 wt % of a reactive mesogen, and 2 wt % of a reaction inhibitor, to form a first mixture;
melting, the first mixture in the first container, wherein a heat applied to the first container is 80° C.;
mixing, in a second container, about 28 wt % of a joining molecule and heating the container to 80° C.;
pouring, the first mixture in the first container, into the second container forming a second mixture;
mixing, in the second container, the second mixture, about 1.4 wt % of a photoinitiator, and 6 wt % of a vinyl cross-linker;
mixing, into the second container about 1 wt % of a catalyst; and
centrifuging, the container, for a set time period and at a set rotational speed.

### Claim 8 (depends on 7)

The method of claim 7, wherein the mesogen is 1,4-Bis-[4-(6-acryloyloxyhexyloxy)benzoyloxy]-2methylbenzene (RM82), the reactive mesogen is Bis-[4-(3-acryloyloxypropyloxy)benzoyloxy]-2methylbenzene (RM-257) and the reaction inhibitor is Butylated Hydroxytoluene (BHT).

### Claim 9 (depends on 7)

The method of claim 7, wherein the joining molecule is glycol di(3-mercaptopropionate) (GDMP).

### Claim 10 (depends on 7)

The method of claim 7, wherein the photoinitiator is 2,2-dimethoxy-2-phenylacetophenone (I-651) and the vinyl cross-linker is 1,3,5-triallyl-1,3,5-triazine-2,4,6 (1H,3H,5H)trione (TATATO).

### Claim 11 (depends on 7)

The method of claim 7, wherein the catalyst is Triethylamine (TEA).

### Claim 12 (depends on 7)

A resin made by the method of claim 7.

### Claim 13

An apparatus for manufacturing liquid crystal elastomer fibers from a resin, comprising:
a plurality of manufacturing components, comprising:
an extrusion device configured to extrude the resin;
a first plurality of curing devices configured to partially cure the resin;
a drawing bobbin configured to draw the resin, and to submerge the resin in at least one fluid;
a second plurality of curing devices configured to fully cure the resin; and
a collector bobbin configured to collect the fully cured resin;
and
at least one controller configured to control at least one of the plurality of manufacturing components.

### Claim 14 (depends on 13)

The apparatus of claim 13, further comprising:
a housing configured to house and secure the plurality of manufacturing components, the housing comprising:
a plurality of interconnected components forming a frame; and
a plurality of safety shields coupled to the plurality of interconnected components, wherein each of the plurality of safety shields have a film thereon configured to block Ultra-Violet Light.

### Claim 15 (depends on 13)

The apparatus of claim 13, wherein the extrusion device, further comprises:
a motor configured to provide rotational motion through a drive shaft;
a lead screw coupled to the drive shaft by a coupler;
a plunger coupled to the lead screw;
a mount configured to receive and secure at least one removably securable syringe; and
a heating element coupled to the mount, and configured to heat a contents of the at least one removably securable syringe.

### Claim 16

A method of manufacturing Liquid Crystal Elastomer (LCE) fiber, the method comprising:
extruding a length of liquid crystal elastomer (LCE) resin;
curing the length of LCE resin;
submerging the length of LCE resin in a fluid to form a coated length of LCE resin; and
curing of the coated length of LCE resin to form LCE fiber.

### Claim 17 (depends on 16)

The method of claim 16, wherein curing the length of LCE resin, comprises:
exposing the length of LCE resin to Ultra-Violet (UV) light from at least two sides.

### Claim 18 (depends on 17)

The method of claim 17, wherein curing the coated length of LCE resin, comprises:
exposing the length of LCE resin to Ultra-Violet (UV) light from at least two sides.

### Claim 19 (depends on 18)

The method of claim 18, wherein a wavelength of the UV light is 365 nanometers.

### Claim 20 (depends on 16)

The method of claim 16, wherein the fluid is mineral oil.

### Claim 21

An article of clothing, comprising:
a body configured to be worn by a user, wherein the body is formed from a plurality of liquid crystal elastomer fibers, the plurality of liquid crystal elastomer fibers being reversibly actuatable in response to a range of temperatures.

### Claim 22 (depends on 21)

The article of clothing of claim 21, wherein the range of temperatures are approximately 40 C-60 C.

### Claim 23 (depends on 21)

The article of clothing of claim 21, the liquid crystal elastomer fibers having an actuatable stroke of between 30-40%.

### Claim 24 (depends on 21)

The article of clothing of claim 21, further comprising:
at least one conductive thread disposed around at least one of the plurality of LCE fibers, the at least one conductive thread configured to for electrical routing to act as an input sensor, and to provide heat for actuation of the at least one of the plurality of LCE fibers;
at least one non-conductive thread disposed around the at least one of the plurality of LCE fibers, the at least one non-conductive thread configured to provide insulation;
and
at least one power source configured to provide electrical input to the at least one conductive thread.