# US 2025/0132460 A1 · Ultrahigh-molecular-weight polyethylene powder and molded article prepared by molding same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0132460 A1
- Document ID: US20250132460A1
- Status: Published application
- Kind: A1
- Application number: 18/692,905
- Filed: 2022-09-28
- Published: 2025-04-24
- Earliest claimed: 2021-09-29
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Koichi Tsujimoto; Kazuya Shikata
- Web page: https://patentgrep.com/patent/US20250132460A1

## CPC

- D01F 6/04: from polyolefins
- H01M 50/417: Polyolefins
- C08F 2/04: Polymerisation in solution (C08F2/32 takes precedence)
- C08F 6/10: Removal of volatile materials, e.g. solvents {(C08F6/001, C08F6/003, C08F6/005, C08F6/006, C08F6/008, C08F6/02, C08F6/04 take precedence)}
- C08J 3/12: Powdering or granulating
- C08J 3/124: {Treatment for improving the free-flowing characteristics}
- C08J 5/18: Manufacture of films or sheets
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 110/02: Ethene
- C08F 2410/01: Additive used together with the catalyst, excluding compounds containing Al or B
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F 2500/01: High molecular weight, e.g. >800,000 Da.
- C08F 2500/17: Viscosity
- C08F 2500/24: Polymer with special particle form or size
- C08J 2323/06: Polyethene
- Y02E 60/10: Energy storage using batteries
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is an ultrahigh-molecular-weight polyethylene powder having intrinsic viscosity IV of 1.0 dL/g or more and 33.0 dL/g or less, wherein average value Ts of swelling onset temperatures determined by specific methods is 90° C. or higher and 130° C. or lower.

## Claims

### Claim 1

An ultrahigh-molecular-weight polyethylene powder having intrinsic viscosity IV of 1.0 dL/g or more and 33.0 dL/g or less, wherein
average value Ts of swelling onset temperatures determined by the following methods (i) and (ii) is 90° C. or higher and 130° C. or lower:
Method (i); method for measuring D10, D50, and D90;
particle sizes of the target ultrahigh-molecular-weight polyethylene powder are measured using a laser particle size distribution analyzer with methanol as a dispersion medium, and a cumulative particle size distribution from smaller particle sizes is prepared on the basis of the measurement; Particle sizes that attain cumulative percentages of 10%, 50%, and 90% are defined as D10, D50, and D90, respectively;
Method (ii); method for measuring swelling onset temperatures T10, T50, and T90 and method for calculating average value Ts thereof;
swelling onset temperature T10 of a powder having a particle size of D10 is determined; First, any one particle of an ultrahigh-molecular-weight polyethylene powder having a major axis size and a minor axis size (as for a plane figure of a particle observed under an optical microscope, a distance between parallel lines having the shortest interval is defined as the minor axis size of the particle, and a distance between parallel lines having the longest interval in a direction perpendicular thereto is defined as the major axis size of the particle) within a range of D10±10% is collected while confirming with an optical microscope; the collected one particle of the ultrahigh-molecular-weight polyethylene powder (hereinafter, also referred to as a “measurement particle”) is loaded onto a glass slide, and 0.05 mL of liquid paraffin is dropped to the measurement particle using a 1 ml syringe; then, a glass cover is placed thereon so as to sandwich the measurement particle; then, the glass slide is loaded onto a heat stage and heated from room temperature to 150° C. under heating conditions given below; the appearance of the measurement particle during heating is photographed every 6 seconds under an optical microscope equipped with a camera; an equivalent circle diameter of the measurement particle is calculated from each of the obtained observation images; the lowest temperature at which the equivalent circle diameter of the measurement particle is increased by 1% or more with respect to the equivalent circle diameter of the measurement particle at 80° C. in a temperature range of 80° C. or higher and 150° C. or lower is defined as the swelling onset temperature of the measurement particle; measurement is performed for n=10, and an average value thereof is defined as the swelling onset temperature T10;
next, swelling onset temperature T50 of an ultrahigh-molecular-weight polyethylene powder having a particle size of D50, and swelling onset temperature T90 of an ultrahigh-molecular-weight polyethylene powder having a particle size of D90 are also determined in the same manner as in the swelling onset temperature T10 using respectively an ultrahigh-molecular-weight polyethylene powder having a major axis size and a minor axis size within a range of D50±10%, and an ultrahigh-molecular-weight polyethylene powder having a major axis size and a minor axis size within a range of D90±10%;
finally, average value Ts of the swelling onset temperatures T10, T50, and T90 is determined as follows:
T
S
=
T
1
⁢
0
+
T
5
⁢
0
+
T
9
⁢
0
3
(Heating conditions)
heating rate from room temperature to 35° C.: 5° C./min
heating rate in a range from 35° C. to 80° C.: 8° C./min
heating rate in a range from 80° C. to 150° C.: 5° C./min.

### Claim 2 (depends on 1)

The ultrahigh-molecular-weight polyethylene powder according to claim 1, wherein standard deviation s of the swelling onset temperatures of the powders having particle sizes of D10, D50, and D90 is 5° C. or less.

### Claim 3 (depends on 1)

The ultrahigh-molecular-weight polyethylene powder according to claim 1, wherein the standard deviation s of the swelling onset temperatures of the powders having particle sizes of D10, D50, and D90 is 2.4° C. or less.

### Claim 4 (depends on 1)

The ultrahigh-molecular-weight polyethylene powder according to claim 1, wherein a comonomer content measured by 13C-NMR is 1.0 mol % or less.

### Claim 5 (depends on 1)

The ultrahigh-molecular-weight polyethylene powder according to claim 1, having a titanium (Ti) content of 5.0 ppm or less, an aluminum (Al) content of 5.0 ppm or less, and a silicon (Si) content of 100 ppm or less.

### Claim 6 (depends on 1)

The ultrahigh-molecular-weight polyethylene powder according to claim 1, wherein D90/D10 is 1.2 or more and 4.0 or less.

### Claim 7 (depends on 1)

7 (currently amended): The ultrahigh-molecular-weight polyethylene powder according to claim 1, wherein D10 is 30 μm or larger, and D90 is 425 μm or smaller.

### Claim 8 (depends on 1)

A shaped article obtained by shaping the ultrahigh-molecular-weight polyethylene powder according to claim 1.

### Claim 9 (depends on 8)

The shaped article according to claim 8, wherein the shaped article is a separator for secondary battery.

### Claim 10 (depends on 8)

The shaped article according to claim 8, wherein the shaped article is a fiber.

### Claim 11 (depends on 1)

A method for producing the ultrahigh-molecular-weight polyethylene powder according to claim 1, comprising the steps of:
in producing an ethylene polymer, mixing 0.01 to 0.05 mol % of a comonomer in terms of a gas phase concentration into ethylene, and performing polymerization; and
drying a polymer powder at 100° C. or higher.

### Claim 12 (depends on 1)

A method for producing the ultrahigh-molecular-weight polyethylene powder according to claim 1, comprising
a polymerization step of performing polymerization in a state of a polymerization solvent supplemented with 30 to 50% by mass of a plasticizer.

### Claim 13 (depends on 12)

The method for producing an ultrahigh-molecular-weight polyethylene powder according to claim 12, further comprising:
a removal step of removing the plasticizer from the powder after completion of the polymerization step; and
a drying step of setting catalytic activity during polymerization to 5000 (g-PE/g-catalyst) or less, and drying the polymer powder at 70° C. or lower.

### Claim 14 (depends on 12)

The method for producing an ultrahigh-molecular-weight polyethylene powder according to claim 12, wherein the plasticizer is liquid paraffin.

### Claim 15 (depends on 2)

The ultrahigh-molecular-weight polyethylene powder according to claim 2, wherein the standard deviation s of the swelling onset temperatures of the powders having particle sizes of D10, D50, and D90 is 2.4° C. or less.

### Claim 16 (depends on 2)

The ultrahigh-molecular-weight polyethylene powder according to claim 2, wherein a comonomer content measured by 13C-NMR is 1.0 mol % or less.

### Claim 17 (depends on 2)

The ultrahigh-molecular-weight polyethylene powder according to claim 2, having a titanium (Ti) content of 5.0 ppm or less, an aluminum (Al) content of 5.0 ppm or less, and a silicon (Si) content of 100 ppm or less.

### Claim 18 (depends on 2)

The ultrahigh-molecular-weight polyethylene powder according to claim 2, wherein D90/D10 is 1.2 or more and 4.0 or less.

### Claim 19 (depends on 2)

The ultrahigh-molecular-weight polyethylene powder according to claim 2, wherein D10 is 30 μm or larger, and D90 is 425 μm or smaller.

### Claim 20 (depends on 13)

The method for producing an ultrahigh-molecular-weight polyethylene powder according to claim 13, wherein the plasticizer is liquid paraffin.