# US 2025/0129506 A1 · Process for manufacturing a monocrystalline silicon semiconductor wafer, and monocrystalline silicon semiconductor wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0129506 A1
- Document ID: US20250129506A1
- Status: Published application
- Kind: A1
- Application number: 18/691,466
- Filed: 2022-09-05
- Published: 2025-04-24
- Earliest claimed: 2021-09-16
- Assignees: Siltronic AG
- Applicants: Siltronic AG
- Inventors: Timo MUELLER; Michael BOY; Michael GEHMLICH; Gudrun KISSINGER; Dawid KOT
- Web page: https://patentgrep.com/patent/US20250129506A1

## CPC

- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 29/06: Silicon
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor wafer of monocrystalline silicon is produced, in the following order: growing a single crystal of silicon by the CZ method; dividing off a wafer consisting completely of an N region, in which there are no agglomerates of silicon interstitials or vacancies having a diameter of more than 20 nm, and has an oxygen concentration of not less than 5.3×1017 atoms/cm3 and not more than 5.9×1017 atoms/cm3 and a nitrogen concentration of not more than 1.0×1012 atoms/cm3; executing a three separate rapid thermal annealing (RTA) treatments of the wafer at temperatures within different temperature ranges over different time periods in a different atmospheres of argon with and without ammonia.

## Claims

### Claim at position 1

1: A method for producing a semiconductor wafer of monocrystalline silicon, the method comprising in the following order:
growing a single crystal of silicon by the Czochralski (CZ) method;
dividing at least one semiconductor wafer of monocrystalline silicon from the single crystal, wherein the semiconductor wafer consists completely of an N region, in which there are no agglomerates of silicon interstitials or vacancies having a diameter of more than 20 nm, and has an oxygen concentration of not less than 5.3×1017 atoms/cm3 and not more than 5.9×1017 atoms/cm3 and a nitrogen concentration of not more than 1.0×1012 atoms/cm3;
executing a first rapid thermal annealing (RTA) treatment of the semiconductor wafer at a first temperature in a first temperature range of not less than 750° C. and not more than 1100° C. over a first period of not less than 10 s and not more than 30 s in a first atmosphere of argon and ammonia in a ratio of not less than 1:2 and not more than 1:0.75;
executing a second RTA treatment of the semiconductor wafer at a second temperature in a second temperature range of not less than 1190° C. and not more than 1280° C. over a second period of not less than 20 s and not more than 35 s in a second atmosphere of argon; and
executing a third RTA treatment of the semiconductor wafer at a third temperature in a third temperature range of not less than 1160° C. and not more than 1180° C. over a third period of not less than 15 s and not more than 25 s in a third atmosphere of argon and ammonia in a ratio of not less than 8:10 and not more than 3:2.

### Claim at position 2 (depends on 1)

2: The method as claimed in claim 1, which further comprises a fourth RTA treatment of the semiconductor wafer at a fourth temperature in a fourth temperature range of not less than 1130° C. and not more than 1145° C. over a fourth period of not less than 25 s and not more than 35 s in a fourth atmosphere of argon.

### Claim at position 3

3: A semiconductor wafer of monocrystalline silicon having a front side and a back side, consisting of an N region, comprising
an interstitial oxygen concentration of not less than 5.3×1017 atoms/cm3 and not more than 5.9×1017 atoms/cm3; and
a nitrogen concentration, which decreases from the front side and from the back side into the interior of the semiconductor wafer and in a depth of 50 μm from the front side is not less than 2.0×1015 atoms/cm3.

### Claim at position 4 (depends on 3)

4: The semiconductor wafer as claimed in claim 3, wherein the nitrogen concentration in a near-surface region of the back side is lower than in a near-surface region of the front side.

### Claim at position 5 (depends on 3)

5: The semiconductor wafer as claimed in claim 3, which comprises:
a denuded zone, which extends from the front side to a depth of not less than 10 μm and not more than 20 μm into the interior of the semiconductor wafer, and
an underlying region with BMDs of a density of 5.0×109 cm−3 to 7.0×109 cm−3.