# US 2025/0129442 A1 · Cemented carbide insert with eta-phase core

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0129442 A1
- Document ID: US20250129442A1
- Status: Published application
- Kind: A1
- Application number: 18/570,104
- Filed: 2022-06-14
- Published: 2025-04-24
- Earliest claimed: 2021-06-16
- Assignees: Sandvik Mining and Construction Tools AB
- Applicants: Sandvik Mining and Construction Tools AB
- Inventors: Ioannis ARVANITIDIS; Mirjam LILJA
- Web page: https://patentgrep.com/patent/US20250129442A1

## CPC

- C21D 1/06: Surface hardening
- B22F 3/162: {Machining, working after consolidation}
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C22C 29/005: {comprising a particular metallic binder}
- C22C 29/08: based on tungsten carbide
- E21C 35/1835: {Chemical composition or specific material}
- B22F 2003/248: {Thermal after-treatment}
- B22F 2005/001: {Cutting tools, earth boring or grinding tool other than table ware}
- B22F 2207/03: of the metallic binder phase in cermets
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- E21C: MINING OR QUARRYING

## Abstract

A method of treating a cemented carbide insert for rock drilling and mineral cutting is provided. The insert includes a core of cemented carbide and a surface zone of cemented carbide, wherein the core further contains eta-phase and the surface zone is free of eta-phase. The mining insert is subjected to a surface hardening process, wherein the surface hardening process is executed at an elevated temperature of or above 50° C.

## Claims

### Claim 1

A method of treating a cemented carbide insert for rock drilling and mineral cutting, the insert comprising a core of cemented carbide and a surface zone of cemented carbide surrounding said core, wherein both the surface zone and the core contain WC (alpha-phase) with a binder phase (beta-phase) based upon at least one of cobalt, nickel or iron, and wherein the core further contains eta-phase and the surface zone is free of eta-phase, wherein an inner part of the surface zone situated next to the core has a content of binder phase being greater than a nominal content of the binder phase in the cemented carbide body and the content of the binder phase increases gradually in the surface zone in a direction towards the core up to at least 1.2 times compared to the nominal content of the binder phase of the cemented carbide body, wherein the method comprises:
subjecting the insert to a surface hardening process;
heating the insert to a temperature of or above 50° C. prior to the surface hardening process; and
executing the surface hardening process at an elevated temperature of or above 50° C., wherein the surface hardening is tumbling.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the cemented carbide comprises hard constituents in a metallic binder phase, and wherein the metallic binder phase content in the cemented carbide is 3 to 30 wt %.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the metallic binder phase comprises at least 80 wt % of one or more metallic elements selected from Co, Ni and Fe.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the cemented carbide further comprises Cr, in an amount such that a mass ratio of Cr/binder is of 0.043-0.19.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the content of binder phase in the surface zone increases towards the core to 1.4-2.5 times the nominal content of the binder phase.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the insert is tumbled with media and wherein the media is also heated prior to and during tumbling to a temperature of 50° C. or above.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the insert is kept heated during the surface hardening process.

### Claim 8 (depends on 1)

The method according to claim 1, wherein after the insert has been subjected to the surface hardening process at an elevated temperature, the insert is subjected to a second surface hardening process at room temperature.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the tumbling process is a “High Energy Tumbling” process, wherein post tumbling a homogenous cemented carbide mining insert is deformation hardened such that ΔHV3%≥9.72−0.00543*HV3bulk, wherein the ΔHV3% is the percentage difference between the HV3 measurement at 0.3 mm from the surface compared the HV3 measurement in the bulk.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the surface hardening process is conducted in dry conditions.

### Claim 11 (depends on 1)

A cemented carbide insert for rock drilling and mineral cutting produced according to the method disclosed in claim 1.

### Claim 12

A cemented carbide insert for rock drilling and mineral cutting comprising a core of cemented carbide and a surface zone of cemented carbide surrounding said core, wherein both the surface zone and the core contain WC (alpha-phase) with a binder phase (beta-phase) based upon at least one of cobalt, nickel or iron, and wherein the core further contains eta-phase and the surface zone is free of eta-phase, wherein an inner part of the surface zone situated next to the core has a content of binder phase being greater than a nominal content of the binder phase in the cemented carbide body and the content of the binder phase increases gradually in the surface zone in a direction towards the core up to at least 1.2 times compared to the nominal content of the binder phase of the cemented carbide body, having a profile hardness, HV3p, measured 0.3 mm from the surface across a top, non-cylindrical part of the insert and an eta-phase core hardness, HV3η, which an average of the HV3 hardness measurements taken in the core eta phase region, characterized in that HV3p−HV3η>20.

### Claim 13 (depends on 12)

The cemented carbide insert according to claim 12, wherein HV3η is at least 1450 HV3.