# US 2025/0128247 A1 · Photocatalyst granular material and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0128247 A1
- Document ID: US20250128247A1
- Status: Published application
- Kind: A1
- Application number: 18/723,128
- Filed: 2022-12-22
- Published: 2025-04-24
- Earliest claimed: 2021-12-22
- Assignees: Korea Institute of Civil Engineering and Building Technology
- Applicants: Korea Institute of Civil Engineering and Building Technology
- Inventors: Hyun-Bon KOO; Jong-Won KWARK; Seong-Jun KIM; Yun-jong KI
- Web page: https://patentgrep.com/patent/US20250128247A1

## CPC

- B01D 53/885: {Devices in general for catalytic purification of waste gases}
- B01J 35/39: Photocatalytic properties
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/04: Alkali metals
- B01J 35/20: characterised by their non-solid state
- B01J 35/51: Spheres
- B01J 35/55: Cylinders or rings
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0201: {Impregnation}
- B01J 37/0221: {of particles}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/10: in the presence of water, e.g. steam
- B01J 37/343: {of ultrasonic wave energy}
- A61L 9/16: using physical phenomena
- B01D 2255/2022: Potassium
- B01D 2255/2025: Lithium
- B01D 2255/2027: Sodium
- B01D 2255/20707: Titanium
- B01D 2257/70: Organic compounds not provided for in groups B01D2257/00 - B01D2257/602
- B01D 2257/91: Bacteria; Microorganisms
- B01D 2258/06: Polluted air
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 35/80: characterised by their amorphous structures
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

Described are a photocatalytic reforming method, a photocatalyst granular material comprising photocatalyst crystals reformed thereby, and a preparation method therefor, the photocatalytic reforming method comprising the steps of: in order to separate a monatomic layer of a photocatalyst, hydrothermally synthesizing the photocatalyst by reacting the photocatalyst with an alkaline solution at a temperature of at least 100° C.; and processing the hydrothermally synthesized photocatalyst so that crystals of the photocatalyst have tubular shapes.

## Claims

### Claim 1

A photocatalytic reforming method comprising:
performing hydrothermal synthesis to react a photocatalyst with an alkaline solution at a temperature of 100° C. or higher, so that a monoatomic layer of the photocatalyst is separated; and
treating the hydrothermally synthesized photocatalyst so that a crystal of the photocatalyst has a tubular shape.

### Claim 2 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the performing the hydrothermal synthesis is to react the photocatalyst at a temperature of 100° C. to 130° C. by mixing the photocatalyst with the alkaline solution.

### Claim 3 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the alkaline solution contains at least one of Li, Na, and K.

### Claim 4 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the photocatalyst has an anatase phase.

### Claim 5 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the treating includes drying the hydrothermally synthesized photocatalyst.

### Claim 6 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the treating includes calcining the hydrothermally synthesized photocatalyst.

### Claim 7 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the alkaline solution contains at least one of Na and K, and the photocatalyst has an anatase phase.

### Claim 8 (depends on 7)

The photocatalytic reforming method of claim 7, wherein the alkaline solution contains at least one of NaOH and KOH, and the performing the hydrothermal synthesis is to perform the hydrothermal synthesis by dispersing the photocatalyst with the anatase phase in the alkaline solution through energy equivalent to ultrasonic waves, and then reacting the photocatalyst with the alkaline solution at a temperature of 100° C. to 130° C. for 15 to 20 hours.

### Claim 9 (depends on 1)

The photocatalytic reforming method of claim 1, wherein the photocatalyst is titanium oxide or metatitanic acid.

### Claim 10 (depends on 1)

A photocatalyst granular material comprising a photocatalyst having a plurality of photocatalyst crystals reformed by the photocatalytic reforming method according to claim 1.

### Claim 11 (depends on 1)

A photocatalyst granular material preparation method comprising:
preparing a photocatalyst reformed by the photocatalytic reforming method according to claim 1;
producing a photocatalyst paste by mixing the reformed photocatalyst with distilled water;
molding the photocatalyst paste into a granule; and
drying the molded granule to form a photocatalyst granule.

### Claim 12 (depends on 11)

The photocatalyst granular material preparation method of claim 11, wherein the producing the photocatalyst paste is to further mix an open-cell type circular foam made of a material with a lower melting point than that of the reformed photocatalyst or a piece of yarn made of a material with a lower melting point than that of the photocatalyst.

### Claim 13 (depends on 12)

The photocatalyst granular material preparation method of claim 12, wherein the drying the molded granule is to dry the molded granule at a temperature higher than the melting point of the circular foam or the piece of yarn, such that at least a portion of the circular foam or piece of yarn is melted.

### Claim 14 (depends on 12)

The photocatalyst granular material preparation method of claim 12, wherein the circular foam or the piece of yarn is made of a material containing at least one of polyethylene and polyurethane.

### Claim 15 (depends on 1)

A photocatalyst granular material preparation method comprising:
coating a granule with a liquid photocatalyst; and
drying the granule coated with the liquid photocatalyst to form a photocatalyst granule,
wherein the coating of the granule with the liquid photocatalyst is to immerse the granule in the liquid photocatalyst or spray the liquid photocatalyst on the granule, the liquid photocatalyst includes a photocatalyst reformed by the photocatalytic reforming method according to claim 1, and the granule is a material that does not contain the photocatalyst.