# US 2025/0123559 A1 · Resist Material And Patterning Process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0123559 A1
- Document ID: US20250123559A1
- Status: Published application
- Kind: A1
- Application number: 18/909,129
- Filed: 2024-10-08
- Published: 2025-04-17
- Earliest claimed: 2023-10-13
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Yutaro OTOMO
- Web page: https://patentgrep.com/patent/US20250123559A1

## CPC

- G03F 7/0212: {characterised by the polymeric binder or the macromolecular additives other than the diazo resins or the polymeric diazonium compounds}
- G03F 7/0045: {with organic non-macromolecular light-sensitive compounds not otherwise provided for, e.g. dissolution inhibitors}
- G03F 7/0392: {the macromolecular compound being present in a chemically amplified positive photoresist composition}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The present invention is a resist material containing: a base polymer (P) containing a repeating unit (A) containing a reactive group and represented by the following formula (a1) or (a2), and a repeating unit (B) having an acid-decomposable group; a crosslinking agent having a structure represented by the following formula (1); a thermal acid generator; a photodecomposable quencher represented by the following formula (2); and an organic solvent. This can provide: a resist material having little edge roughness, little size variation, excellent resolution, and excellent heat resistance; and a patterning process.

## Claims

### Claim 1

A resist material comprising:
a base polymer (P) containing a repeating unit (A) containing a reactive group and represented by the following formula (a1) or (a2), and a repeating unit (B) having an acid-decomposable group;
a crosslinking agent having a structure represented by the following formula (1);
a thermal acid generator;
a photodecomposable quencher represented by the following formula (2); and
an organic solvent,
wherein each RA independently represents a hydrogen atom or a methyl group, Ya1 and Ya2 each independently represent a single bond, a phenylene group, a naphthylene group, or a linking group having 1 to 14 carbon atoms and having an ester bond, an ether bond, an amide bond, or a lactone ring, Ra1 represents a hydrogen atom, a fluorine atom, or a saturated hydrocarbyl group having 1 to 6 carbon atoms, Ra1 and Ya1 optionally being bonded to each other to form a ring together with the carbon atoms on the aromatic ring bonded thereto, “p” represents 1 or 2, “q” represents an integer of 0 to 4, 1≤p+q≤5, and “r” represents 0 or 1,
wherein R1a represents an organic group optionally having a substituent, L1 represents a linking group selected from a single bond, an ester bond, and an ether bond, R1b represents a single bond or a divalent organic group, and “n” represents an integer of 2 to 4,
wherein R21 to R23 each independently represent a monovalent hydrocarbon group having 1 to 20 carbon atoms and optionally containing a heteroatom, any two of R21, R22, and R23 optionally being bonded to each other to form a ring together with the sulfur atom bonded thereto, “I” represents an integer of 0 to 4, R2b represents a halogen atom, a hydroxy group, a nitro group, a hydrocarbon group having 1 to 20 carbon atoms and optionally having a substituent, an alkoxy group having 1 to 18 carbon atoms and optionally having a substituent, an amino group optionally having a substituent, or a phenyl group optionally having a substituent, when “I” is 2 or more, the R2bs optionally being different from each other, L2a represents a single bond, an ester bond, or a divalent linking group having 1 to 8 carbon atoms, and R2a represents a hydrogen atom or a hydrocarbon group having 1 to 18 carbon atoms and optionally having a substituent, R2a and R2b optionally being bonded to each other to form a ring together with the carbon atoms bonded thereto.

### Claim 2 (depends on 1)

The resist material according to claim 1, wherein the base polymer (P) contains a repeating unit (C) having a structural site which is decomposed by irradiation with an active ray or a radiant ray to generate an acid.

### Claim 3 (depends on 2)

The resist material according to claim 2, wherein the repeating unit (C) contained in the base polymer (P) is represented by the following formula (c),
wherein Rc1 represents a hydrogen atom or a methyl group; Z1 represents a single bond or an ester bond; Z2 represents a single bond or a divalent organic group having 1 to 20 carbon atoms and optionally containing an ester bond, an ether bond, a lactone ring, an amide bond, a sultone ring, or an iodine atom; Rfc1 to Rfc4 each independently represent a hydrogen atom, a fluorine atom, or a trifluoromethyl group, provided that at least one of Rfc1 to Rfc4 contains a fluorine atom; and Rc2 to Rc4 each independently represent a monovalent hydrocarbon group having 1 to 20 carbon atoms and optionally containing a heteroatom, any two of Rc2, Rc3, and Rc4 optionally being bonded to each other to form a ring together with the sulfur atom bonded thereto.

### Claim 4 (depends on 1)

The resist material according to claim 1, wherein the repeating unit (B) contained in the base polymer (P) is represented by the following formula (b),
wherein Rb represents a hydrogen atom or a methyl group; Lb represents a single bond or a divalent linking group having 1 to 15 carbon atoms and including at least one of a phenylene group, a naphthylene group, an ester bond, an ether bond, a lactone ring, an amide group, and a heteroatom; and RAL represents an acid-labile group.

### Claim 5 (depends on 1)

The resist material according to claim 1, wherein the repeating unit (A) contained in the base polymer (P) is represented by the formula (a1), and is contained at a percentage of 30 mol % or more based on a total amount of the repeating units in the base polymer (P).

### Claim 6 (depends on 1)

A patterning process comprising the steps of:
forming a resist film on a substrate by using the resist material according to claim 1;
exposing the resist film to a high-energy beam; and
developing the exposed resist film by using a developer.

### Claim 7 (depends on 2)

A patterning process comprising the steps of:
forming a resist film on a substrate by using the resist material according to claim 2;
exposing the resist film to a high-energy beam; and
developing the exposed resist film by using a developer.

### Claim 8 (depends on 3)

A patterning process comprising the steps of:
forming a resist film on a substrate by using the resist material according to claim 3;
exposing the resist film to a high-energy beam; and
developing the exposed resist film by using a developer.

### Claim 9 (depends on 4)

A patterning process comprising the steps of:
forming a resist film on a substrate by using the resist material according to claim 4;
exposing the resist film to a high-energy beam; and
developing the exposed resist film by using a developer.

### Claim 10 (depends on 5)

A patterning process comprising the steps of:
forming a resist film on a substrate by using the resist material according to claim 5;
exposing the resist film to a high-energy beam; and
developing the exposed resist film by using a developer.

### Claim 11 (depends on 6)

The patterning process according to claim 6, wherein, in the step of forming the resist film, a baking temperature is set to 130° C. or higher.

### Claim 12 (depends on 7)

The patterning process according to claim 7, wherein, in the step of forming the resist film, a baking temperature is set to 130° C. or higher.

### Claim 13 (depends on 8)

The patterning process according to claim 8, wherein, in the step of forming the resist film, a baking temperature is set to 130° C. or higher.

### Claim 14 (depends on 9)

The patterning process according to claim 9, wherein, in the step of forming the resist film, a baking temperature is set to 130° C. or higher.

### Claim 15 (depends on 10)

The patterning process according to claim 10, wherein, in the step of forming the resist film, a baking temperature is set to 130° C. or higher.