# US 2025/0115684 A1 · Method for Preparing Polyethylene Polymerization Catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0115684 A1
- Document ID: US20250115684A1
- Status: Published application
- Kind: A1
- Application number: 18/419,979
- Filed: 2024-01-23
- Published: 2025-04-10
- Earliest claimed: 2023-10-05
- Assignees: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.
- Applicants: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.
- Inventors: Dong Kou Kim; Mun Hyung Kang; Maeng Sun Eo; Sudevan Sujith
- Web page: https://patentgrep.com/patent/US20250115684A1

## CPC

- C08F 4/16: of silicon, germanium, tin, lead, titanium, zirconium or hafnium
- C08F 2/06: Organic solvent
- C08F 4/10: of alkaline earth metals, zinc, cadmium, mercury, copper or silver
- C08F 110/02: Ethene
- C08F 2410/06: Catalyst characterized by its size
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a method for preparing a polyethylene polymerization catalyst including a first mixed solution preparation step of mixing a magnesium compound, a first hydrocarbon compound, and alcohol to prepare a first mixed solution; a viscosity adjustment step of adding a second hydrocarbon compound to the first mixed solution to adjust a viscosity of the first mixed solution; a second mixed solution preparation step of adding a first internal electron donor to the first mixed solution having an adjusted viscosity to prepare a second mixed solution; and a recrystallization step of adding a transition metal compound to the second mixed solution to perform recrystallization.

## Claims

### Claim 1

A method for preparing a polyethylene polymerization catalyst, the method comprising:
a first mixed solution preparation step of mixing a magnesium compound, a first hydrocarbon compound, and alcohol to prepare a first mixed solution;
a viscosity adjustment step of adding a second hydrocarbon compound to the first mixed solution to adjust a viscosity of the first mixed solution;
a second mixed solution preparation step of adding a first internal electron donor to the first mixed solution having an adjusted viscosity to prepare a second mixed solution; and
a recrystallization step of adding a transition metal compound to the second mixed solution to perform recrystallization.

### Claim 2 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein a viscosity range of the first mixed solution in the viscosity adjustment step is 10 cP to 70 cP.

### Claim 3 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, further comprising: a washing step of washing with the second hydrocarbon compound after the recrystallization step.

### Claim 4 (depends on 3)

The method for preparing a polyethylene polymerization catalyst of claim 3, further comprising: a slurry catalyst preparation step of adding the second hydrocarbon compound to prepare a slurry catalyst after the washing step.

### Claim 5 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein a second internal electron donor is further added after adding the transition metal compound.

### Claim 6 (depends on 5)

The method for preparing a polyethylene polymerization catalyst of claim 5, wherein a mole ratio between the magnesium compound and the second internal electron donor is 1:0.01 to 1:1.

### Claim 7 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein a mole ratio between the magnesium compound and the second hydrocarbon compound is 1:1.5 to 1:5.

### Claim 8 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein the alcohol is at least one selected from the group consisting of 2-ethylhexanol, methanol, ethanol, propanol, butanol, pentanol, cyclopentanol, hexanol, heptanol, octanol, decanol, dodecanol, 2-methylpentanol, 2-ethylbutanol, cyclohexanol, methylcyclohexnaol, methylbenzyl alcohol and mixtures thereof.

### Claim 9 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein the first hydrocarbon compound is a C9 to C30 hydrocarbon.

### Claim 10 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein the second hydrocarbon compound is a C3 to C8 hydrocarbon.

### Claim 11 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein the first internal electron donor or the second internal electron donor is independently of each other at least one selected from the group consisting of ethyl benzoate, methyl benzoate, ethyl p-methoxybenzoate, methyl p-ethoxybenzoate, ethyl p-ethoxybenzoate, ethyl p-chlorobenzoate, diisobutyl phthalate, 9,9-bis(methoxymethyl)fluorene, propyl benzoate, isopropyl benzoate, dibutyl benzoate, dibutyl 4-(2-aminoethyl) benzoate, ethyl 4-(dimethylamino) benzoate, ethyl 4-(butylamino) benzoate, ethyl 4-(bromomethyl) benzoate, ethyl 4-(benzyloxy) benzoate, methyl 4-(hydroxymethyl) benzoate, methyl 4-(aminomethyl) benzoate, methyl 3-(aminocarbonyl) benzoate, methyl 4-(2-hydroxyethoxy) benzoate, methyl 4-(cyanomethyl) benzoate, methyl 4-(bromomethyl) benzoate, methyl 3-(bromomethyl) benzoate, 1,2-dimethoxybenzene, 1,2-diethoxybenzene, 1,2-dibutoxybenzene, 1,2-di-sec-butoxybenzene, 1,2-di-tert-butoxybenzene, tetramethoxysilane, tetraethoxysilane, tetrapropoxysilane, tetrabutoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, vinyltrimethoxysilane, methyltrimethoxysilane, n-propyltriethoxysilane, decyltrimethoxysilane, cyclopentyltrimethoxysilane, 2-methylcyclopentyltrimethoxysilane, 2,3-dimethylcyclopentyltrimethoxysilane, phenyltrimethoxysilane, vinyltriethoxysilane, t-butyltriethoxysilane, n-butyltriethoxysilane, isobutyltriethoxysilane, decyltriethoxysilane, cyclopentyltriethoxysilane, chlorotriethoxysilane, cyclohexyltriethoxysilane, ethyltriisopropoxysilane, vinyltributoxysilane, trimethylphenoxysilane, methyltriallyloxysilane, vinyltriacetoxysilane, dimethylmethoxysilane, diisopropyldimethoxysilane, t-butylmethyldimethoxysilane, dicyclopentyldimethoxysilane, dicyclohexyldimethoxysilane, cyclohexylmethyldimethoxysilane, diphenyldimethoxysilane, cyclopentyldimethoxysilane and mixtures thereof.

### Claim 12 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein a mole ratio between the magnesium compound and the first internal electron donor is 1:0.01 to 1:0.3.

### Claim 13 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein a mole ratio between the magnesium compound and the transition metal compound is 1:2 to 1:5.

### Claim 14 (depends on 1)

The method for preparing a polyethylene polymerization catalyst of claim 1, wherein the recrystallization step is performed at −7 to 7° C.

### Claim 15 (depends on 1)

A method for preparing polyethylene, the method comprising: polymerizing a monomer using a polyethylene polymerization catalyst prepared according to claim 1.