# US 2025/0115532 A1 · Energetic formulations containing epoxy-modified graphene oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0115532 A1
- Document ID: US20250115532A1
- Status: Published application
- Kind: A1
- Application number: 18/293,719
- Filed: 2022-08-01
- Published: 2025-04-10
- Earliest claimed: 2021-08-02
- Assignees: Powder Fuels Ltd
- Applicants: Powder Fuels Ltd.
- Inventors: Abraham WEINREB; Shmuel KENIG; Naum NAVEH; Menahem KIDRON; Micha ASSCHER
- Web page: https://patentgrep.com/patent/US20250115532A1

## CPC

- C06B 23/007: {Ballistic modifiers, burning rate catalysts, burning rate depressing agents, e.g. for gas generating}
- C01B 32/198: Graphene oxide
- C06B 43/00: Compositions characterised by explosive or thermic constituents not provided for in groups C06B25/00 - C06B41/00
- C06D 5/06: by reaction of two or more solids
- C06D 5/10: by reaction of solids with liquids
- C10L 1/12: Inorganic compounds
- C10L 1/14: Organic compounds
- C10L 1/1855: {Cyclic ethers, e.g. epoxides, lactides, lactones}
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C06D: MEANS FOR GENERATING SMOKE OR MIST; GAS-ATTACK COMPOSITIONS; GENERATION OF GAS FOR BLASTING OR PROPULSION (CHEMICAL PART) (fuels C10)
- C10L: FUELS NOT OTHERWISE PROVIDED FOR; NATURAL GAS; SYNTHETIC NATURAL GAS OBTAINED BY PROCESSES NOT COVERED BY SUBCLASSES C10G OR C10K; LIQUIFIED PETROLEUM GAS; USE OF ADDITIVES TO FUELS OR FIRES; FIRE-LIGHTERS

## Abstract

An energetic formulation includes graphene oxide functionalized with a molecule containing at least one epoxy group. The graphene oxide may include at least one functional group containing nitrogen between a graphene sheet and the at least one epoxy group. The epoxy group may be sourced from a hydrocarbon compound containing a plurality of epoxy groups. The functionalized graphene oxide may be coated onto ammonium perchlorate. The functionalized graphene oxide is used as a stand-alone energetic material in powder form, mixed as powder in a liquid fuel, or mixed as a powder in a solid fuel.

## Claims

### Claim 1

An energetic formulation, comprising graphene oxide functionalized with a molecule containing at least one epoxy group.

### Claim 2 (depends on 1)

The energetic formulation of claim 1, wherein the graphene oxide is further functionalized through oxidation with a nitro-group, an amino-group, or an oxoacid at a different location than a location of functionalization with the epoxy group.

### Claim 3 (depends on 1)

The energetic formulation of claim 1, wherein the graphene oxide comprises at least one functional group containing nitrogen between a graphene sheet and the at least one epoxy group.

### Claim 4 (depends on 1)

The energetic formulation of claim 1, wherein the epoxide is sourced from an epoxy silane, and the graphene oxide comprises at least one functional group containing nitrogen between a graphene sheet and the at least one epoxy group.

### Claim 5 (depends on 1)

The energetic formulation of claim 1, wherein the epoxide is sourced from a hydrocarbon compound containing a plurality of epoxy groups.

### Claim 6 (depends on 1)

The energetic formulation of claim 1, wherein the functionalized graphene oxide is coated onto ammonium perchlorate.

### Claim 7 (depends on 1)

The energetic formulation of claim 1, wherein the functionalized graphene oxide is used as a stand-alone energetic material in powder form, mixed as powder in a liquid fuel, or mixed as a powder in a solid fuel.

### Claim 8 (depends on 7)

The energetic formulation of claim 7, wherein the functionalized graphene oxide is mixed in a liquid fuel or solid fuel that is metal-free.

### Claim 9

A method of preparing an energetic formulation, comprising functionalizing graphene oxide with a molecule containing at least one epoxy group.

### Claim 10 (depends on 9)

The method of claim 9, comprising further functionalizing the graphene oxide through oxidation of the graphene oxide with a nitro group, an amino group, or an oxoacid, at a different location than a location of functionalization with the epoxy group.

### Claim 11 (depends on 9)

The method of claim 9, wherein the functionalizing step comprises modifying an epoxy-containing molecule with at least one functional group containing nitrogen, and functionalizing a graphene sheet with the modified epoxy-containing molecule, such that the at least one functional group containing nitrogen is between the graphene sheet and the at least one epoxy group.

### Claim 12 (depends on 9)

The method of claim 9, wherein the epoxide is sourced from an epoxy silane, and functionalizing step comprises functionalizing at least one functional group containing silicon between a graphene sheet and the at least one epoxy group.

### Claim 13 (depends on 9)

The method of claim 9, wherein the epoxy group is sourced from a hydrocarbon compound containing a plurality of epoxy groups.

### Claim 14 (depends on 9)

The method of claim 9, further comprising coating ammonium perchlorate with the functionalized graphene oxide.

### Claim 15 (depends on 9)

The method of claim 9, further comprising using the functionalized graphene oxide as a stand-alone energetic material in powder form, mixing the functionalized graphene oxide within a liquid fuel, or mixing the functionalized graphene oxide as a powder in a solid fuel.

### Claim 16 (depends on 15)

The method of claim 15, further comprising mixing the functionalized graphene oxide in liquid fuel or solid fuel that is metal-free.

### Claim 17 (depends on 9)

The method of claim 9, wherein the functionalizing step is performed when the graphene oxide is suspended in water at a concentration of 0.5% to 10%.

### Claim 18 (depends on 9)

The method of claim 9, wherein the functionalizing step further comprises condensing an epoxy-containing hydrocarbon compound with the graphene oxide using stannous chloride (SnCl2) as a catalyst.

### Claim 19 (depends on 18)

The method of claim 18, wherein the functionalizing step is performed within an acetone solvent at approximately room temperature.

### Claim 20 (depends on 18)

The method of claim 18, wherein the epoxy group is sourced from a hydrocarbon compound containing two or more epoxy groups, and the functionalizing step comprises bonding a first oxygen from a hydroxyl group, attached to a sheet of graphene oxide, to a carbon of a first epoxy group of the hydrocarbon, and thereby converting the first oxygen into an ether and the first epoxy group into a hydroxyl group.