# US 2025/0101230 A1 · Method for manufacturing bamboo plastic composite material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0101230 A1
- Document ID: US20250101230A1
- Status: Published application
- Kind: A1
- Application number: 18/474,896
- Filed: 2023-09-26
- Published: 2025-03-27
- Earliest claimed: 2023-09-26
- Assignees: M.J.International Flooring and Interior Products Inc.
- Applicants: M.J.International Flooring and Interior Products Inc.
- Inventors: BEN-YUAN CHEN
- Web page: https://patentgrep.com/patent/US20250101230A1

## CPC

- C08L 97/02: Lignocellulosic material, e.g. wood, straw or bagasse {(manufacture of articles made from lignocellulosic material by dry processes B27N)}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/07: Flat, e.g. panels
- B29C 48/305: having a wide opening, e.g. for forming sheets
- B29C 48/40: using two or more parallel screws {or at least two parallel non-intermeshing screws}, e.g. twin screw extruders
- C08J 3/005: {Processes for mixing polymers}
- C08J 5/18: Manufacture of films or sheets
- C08K 3/26: Carbonates; Bicarbonates
- C08L 27/06: Homopolymers or copolymers of vinyl chloride
- B29C 2948/92704: Temperature
- B29K 2027/06: PVC, i.e. polyvinylchloride
- B29K 2511/14: Wood, e.g. woodboard or fibreboard
- C08J 2327/06: Homopolymers or copolymers of vinyl chloride
- C08J 2397/02: Lignocellulosic material, e.g. wood, straw or bagasse
- C08J 2423/28: by reaction with halogens or halogen-containing compounds (C08J2423/32 takes precedence)
- C08J 2425/12: with unsaturated nitriles
- C08J 2427/06: Homopolymers or copolymers of vinyl chloride
- C08K 2003/265: {Calcium, strontium or barium carbonate}
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2205/06: having improved processability or containing aids for moulding methods
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for manufacturing bamboo plastic composite material having steps of cutting multiple bamboo stalks into multiple bamboo pieces and grinding the bamboo pieces to form multiple bamboo powders; cleaning the bamboo powders; drying the bamboo powers; modifying the bamboo powders; mixing multiple raw materials to form a bamboo plastic composite material with a composition of PVC 10 to 20 wt %; vinyl chloride/vinyl acetate (VC/VAC) copolymer 10 to 30 wt %; styrene-acrylonitrile copolymer (SAN) 1 to 5 wt %; chlorinated polyethylene (CPE) 1 to 5 wt %; the bamboo powders 10 to 40 wt %; inorganic filler 10 to 40 wt %; internal lubricant 0.1 to 1 wt %; external lubricant 0.1 to 1 wt %; and heat stabilizer 1 to 5 wt %; and forming and molding the bamboo plastic composite material.

## Claims

### Claim 1

A method for manufacturing bamboo plastic composite material comprising steps of:
cutting multiple bamboo stalks into multiple bamboo pieces and grinding the bamboo pieces to form multiple bamboo powders;
cleaning the bamboo powders;
drying the bamboo powders to make water content of the bamboo powders below 12 wt %;
modifying the bamboo powders; and
mixing multiple raw materials to form a bamboo plastic composite material, wherein the raw materials comprise:
the bamboo powders 10 to 40 wt %;
polyvinyl chloride (PVC) 10 to 20 wt %;
vinyl chloride/vinyl acetate (VC/VAC) copolymer 10 to 30 wt %;
styrene-acrylonitrile copolymer (SAN) 1 to 5 wt %;
chlorinated polyethylene (CPE) 1 to 5 wt %;
internal lubricant 0.1 to 1 wt %;
external lubricant 0.1 to 1 wt %; and
heat stabilizer 1 to 5 wt %.

### Claim 2 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1 further comprising steps of:
extruding the bamboo plastic composite material with a twin screw extruder, wherein the twin screw extruder comprises multiple mixing sections; and
molding the bamboo plastic composite material into a sheet or a plate by an extrusion die, wherein the extrusion die comprises an extrusion channel with multiple molding sections.

### Claim 3 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2, wherein the extrusion die comprises nine molding sections with different temperatures and extrusion rates.

### Claim 4 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1, wherein the lengths of the bamboo powders are within a range of 0.1 millimeter to 0.8 millimeter.

### Claim 5 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2, wherein the lengths of the bamboo powders are within a range of 0.1 millimeter to 0.8 millimeter.

### Claim 6 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1, wherein the step of cleaning the bamboo powders comprises soaking the bamboo powders in the alkaline solution for 6 to 12 hours and then rinse with water.

### Claim 7 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2, wherein the step of cleaning the bamboo powders comprises soaking the bamboo powders in the alkaline solution for 6 to 12 hours and then rinse with water.

### Claim 8 (depends on 4)

The method for manufacturing bamboo plastic composite material according to claim 4, wherein the step of cleaning the bamboo powders comprises soaking the bamboo powders in the alkaline solution for 6 to 12 hours and then rinse with water.

### Claim 9 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1, wherein a solvent of the alkaline solution comprises calcium hydroxide, potassium hydroxide, or sodium hydroxide, and the concentration of the solute of the alkaline solution is 3 to 10 wt %.

### Claim 10 (depends on 6)

The method for manufacturing bamboo plastic composite material according to claim 6, wherein a solvent of the alkaline solution comprises calcium hydroxide, potassium hydroxide, or sodium hydroxide, and the concentration of the solute of the alkaline solution is 3 to 10 wt %.

### Claim 11 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1, wherein the step of modifying the bamboo powders comprises placing the bamboo powers into a kiln, wherein the kiln is heated to 150 to 250° C. for 3 to 8 hours with a maximum heating ramp rate of 2° C. per minute with less than 8% of oxygen of atmosphere in the kiln.

### Claim 12 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2, wherein the step of modifying the bamboo powders comprises placing the bamboo powers into a kiln, wherein the kiln is heated to 150 to 250° C. for 3 to 8 hours with a maximum heating ramp rate of 2° C. per minute with less than 8% of oxygen of atmosphere in the kiln.

### Claim 13 (depends on 6)

The method for manufacturing bamboo plastic composite material according to claim 6, wherein the step of modifying the bamboo powders comprises placing the bamboo powers into a kiln, wherein the kiln is heated to 150 to 250° C. for 3 to 8 hours with a maximum heating ramp rate of 2° C. per minute with less than 8% of oxygen of atmosphere in the kiln.

### Claim 14 (depends on 1)

The method for manufacturing bamboo plastic composite material according to claim 1, wherein the step of modifying the bamboo powders comprises immersing the bamboo powders in acetic anhydride within a reactor, wherein the reactor is heated to 100 to 120° C. for 1 hour to 8 hours with the vapor being constantly removed.

### Claim 15 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2, wherein the step of modifying the bamboo powders comprises immersing the bamboo powders in acetic anhydride within a reactor, wherein the reactor is heated to 100 to 120° C. for 1 hour to 8 hours with the vapor being constantly removed.

### Claim 16 (depends on 6)

The method for manufacturing bamboo plastic composite material according to claim 6, wherein the step of modifying the bamboo powders comprises immersing the bamboo powders in acetic anhydride within a reactor, wherein the reactor is heated to 100 to 120° C. for 1 hour to 8 hours with the vapor being constantly removed.

### Claim 17 (depends on 14)

The method for manufacturing bamboo plastic composite material according to claim 14, wherein pyridine is added in the reactor and mixed with acetic anhydride.

### Claim 18 (depends on 2)

The method for manufacturing bamboo plastic composite material according to claim 2 further comprising steps of applying an acrylic coating on the surface of the bamboo plastic composite material and curing with ultraviolet light after extrusion and molding.

### Claim 19 (depends on 3)

The method for manufacturing bamboo plastic composite material according to claim 3 further comprising steps of applying an acrylic coating on the surface of the bamboo plastic composite material and curing with ultraviolet light after extrusion and molding.

### Claim 20 (depends on 4)

The method for manufacturing bamboo plastic composite material according to claim 4 further comprising steps of applying an acrylic coating on the surface of the bamboo plastic composite material and curing with ultraviolet light after extrusion and molding.