# US 2025/0100052 A1 · Multiscale metallic metamaterial, and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0100052 A1
- Document ID: US20250100052A1
- Status: Published application
- Kind: A1
- Application number: 18/523,077
- Filed: 2023-11-29
- Published: 2025-03-27
- Earliest claimed: 2023-09-26
- Assignees: Shanghai Jiao Tong University; Shanghai Yiti Technology Co., Ltd.
- Applicants: Shanghai Jiao Tong University; Shanghai Yiti Technology Co., Ltd.
- Inventors: Haozhang ZHONG; Chuanwei LI; Jianfeng GU
- Web page: https://patentgrep.com/patent/US20250100052A1

## CPC

- B22F 10/62: by chemical means
- B22F 3/11: Making porous workpieces or articles
- B22F 3/1115: {comprising complex forms, e.g. honeycombs}
- B22F 5/10: of articles with cavities or holes, not otherwise provided for in the preceding subgroups
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/36: of energy beam parameters
- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 50/02: for controlling or regulating additive manufacturing processes
- B33Y 80/00: Products made by additive manufacturing
- C22C 1/08: Alloys with open or closed pores
- C22C 22/00: Alloys based on manganese
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 10/366: Scanning parameters, e.g. hatch distance or scanning strategy
- B22F 2301/00: Metallic composition of the powder or its coating
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 1/0425: {Copper-based alloys}
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are a multiscale metallic metamaterial, and a preparation method and use thereof. The preparation method includes: preparing a 3D printed metallic material by 3D printing using a metal alloy powder as a raw material, the 3D printed metallic material having a micron-scale pore-array structure; annealing the 3D printed metallic material to obtain an annealed metallic material; and immersing the annealed metallic material in a chemical etching solution, and performing dealloying, to obtain the multiscale metallic metamaterial.

## Claims

### Claim 1

A method for preparing a multiscale metallic metamaterial,
comprising the steps of preparing a 3D printed metallic material by 3D printing using a metal alloy powder as a raw material, the 3D printed metallic material having a micron-scale pore-array structure;
annealing the 3D printed metallic material to obtain an annealed metallic material; and
immersing the annealed metallic material in a chemical etching solution, and performing dealloying to obtain the multiscale metallic metamaterial.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the annealing is conducted at a temperature of 800° C. to 900° C. for 30 min to 60 min.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the 3D printed metallic material is constructed by unit cells arranged in an array, and each of the unit cells is selected from the group consisting of a square honeycomb unit cell, a simple cubic unit cell, and a gyroid unit cell;
in a hexahedral structure of square honeycomb unit cells, only one pair of opposite faces is provided with a through hole; surfaces with the through hole of two adjacent unit cells in an array of the square honeycomb unit cells are in contact with each other; and the 3D printed metallic material constructed by the square honeycomb unit cells is in a square honeycomb structure; and
in a hexahedral structure of simple cubic unit cells, each pair of three pairs of opposite faces is provided with a through hole; and the 3D printed metallic material constructed by the simple cubic unit cells is in a simple cubic structure.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein each of the square honeycomb unit cells has a dimension (length×width×height) of 1.2×1.2×1.2 mm3 and a strut diameter of 0.58 mm, and the array is in a mode of a 4×4 two-dimensional structure; and the 3D printed metallic material constructed by an array of the square honeycomb unit cells has a dimension (length×width×height) of 4.2 mm×4.2 mm×9 mm and a relative density of 80.0%;
each of the simple cubic unit cells has a dimension (length×width×height) of 1.2×1.2×1.2 mm3 and a strut diameter of 0.78 mm, and the array is in a mode of a 4×4×9 three-dimensional structure; and the 3D printed metallic material constructed by an array of the simple cubic unit cells has a dimension (length×width×height) of 4.3 mm×4.3 mm×10.3 mm and a relative density of 81.0%; and
each of gyroid unit cells has a dimension (length×width×height) of 4×4×4 mm3, and the array is in a mode of a 2×2×3 three-dimensional structure; and the 3D printed metallic material constructed by an array of the gyroid unit cells has a dimension (length×width×height) of 8 mm×8 mm×12 mm and a relative density of 80.0%.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the 3D printing is performed with working parameters comprising
a laser diameter of 50 μm to 60 μm, a laser power of 80 W to 100 W, a scanning speed of 600 mm/s to 800 mm/s, a hatch spacing of 100 μm to 110 μm, and a layer thickness of 20 μm to 30 μm; and the metal alloy powder during the 3D printing is at a temperature of 80° C. to 100° C.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the metal alloy powder has a Dv50 of 40 μm to 45 μm, the metal alloy powder is a CuMn alloy, and the CuMn alloy comprises 44 wt % of Cu and 56 wt % of Mn.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the chemical etching solution is a sulfuric acid solution with a molarity of 0.2 mol/L to 0.3 mol/L; and
the dealloying is conducted at a temperature of 20° C. to 30° C. for greater than or equal to 5 days, during which, the chemical etching solution is replaced once every third hour.

### Claim 8 (depends on 1)

A multiscale metallic metamaterial prepared by the method as claimed in claim 1, wherein the multiscale metallic metamaterial has a hierarchical pore structure, the hierarchical pore structure comprises micron-sized pores and nano-sized pores, and the micro-sized pores are arranged in an array.

### Claim 9 (depends on 8)

The multiscale metallic metamaterial as claimed in claim 8, wherein the multiscale metallic metamaterial has a minimum size of greater than 2 mm in three-dimensional dimensions.

### Claim 10 (depends on 8)

A method for preparing a drug-loading implantable medical device, comprising using the multiscale metallic metamaterial as claimed in claim 8.

### Claim 11 (depends on 5)

The method as claimed in claim 5, wherein the metal alloy powder has a Dv50 of 40 μm to 45 μm, the metal alloy powder is a CuMn alloy, and the CuMn alloy comprises 44 wt % of Cu and 56 wt % of Mn.