# US 2025/0100049 A1 · Polycrystalline diamond composite sheet having continuous gradient transition layer and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0100049 A1
- Document ID: US20250100049A1
- Status: Published application
- Kind: A1
- Application number: 18/604,434
- Filed: 2024-03-13
- Published: 2025-03-27
- Earliest claimed: 2023-09-25
- Assignees: Central South University; Sf Diamond Co., Ltd.
- Applicants: Central South University; Sf Diamond Co., Ltd.
- Inventors: Shaohe ZHANG; Xiangwang KONG; Dongpeng ZHAO; Yulu LI; Linglong RONG; Haoyang ZHANG; Qingyuan FANG; Hua GAO; Jincheng LI; Jingjing WU; Mengyao SHAO; Changjian GENG
- Web page: https://patentgrep.com/patent/US20250100049A1

## CPC

- B22F 7/02: of composite layers {(B22F7/002 takes precedence)}
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- B22F 1/103: containing an organic binding agent comprising a mixture of, or obtained by reaction of, two or more components other than a solvent or a lubricating agent
- B22F 10/18: by mixing binder with metal in filament form, e.g. fused filament fabrication [FFF]
- B22F 10/32: of the atmosphere, e.g. composition or pressure in a building chamber
- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B22F 12/55: Two or more means for feeding material
- B28B 1/001: {Rapid manufacturing of 3D objects by additive depositing, agglomerating or laminating of material (selective deposition modelling of metallic powder B22F10/00; rapid manufacturing of 3D objects in general and in particular of plastics B29C64/00)}
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- B33Y 80/00: Products made by additive manufacturing
- C04B 35/52: based on carbon, e.g. graphite
- C04B 35/56: based on carbides {or oxycarbides (containing free metal binder C22C29/00)}
- C04B 35/645: Pressure sintering
- C22C 29/08: based on tungsten carbide
- B22F 3/1021: {Removal of binder or filler (removal of binder from ceramics C04B35/638)}
- B22F 2201/20: Use of vacuum
- B22F 2203/11: temperature, temperature profile
- B22F 2207/15: Temperature gradients
- B22F 2302/10: Carbide
- B22F 2302/406: Diamond
- B22F 2303/40: Layer in a composite stack of layers, workpiece or article
- C04B 2235/3847: Tungsten carbides
- C04B 2235/427: Diamond
- C22C 2026/006: {with additional metal compounds being carbides}
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The disclosure discloses a polycrystalline diamond composite sheet having a continuous gradient transition layer and a 3D printing preparation method thereof. The polycrystalline diamond composite sheet consists of a polycrystalline diamond layer, a continuous gradient transition layer, and a cemented carbide substrate from top to bottom, in which the continuous gradient transition layer consists of diamond and cemented carbide. Along a direction from the cemented carbide substrate to the polycrystalline diamond layer, a content of the cemented carbide in the continuous gradient transition layer decreases from 100% to 0, and a content of the diamond increases from 0 to 100%. By designing and combining the continuous gradient transition layer with 3D printing technology, the disclosure realizes a continuous change in the two materials of diamond and cemented carbide, thereby eliminating the sudden change interface of the materials inside the diamond composite sheet.

## Claims

### Claim 1

A polycrystalline diamond composite sheet having a continuous gradient transition layer, wherein the polycrystalline diamond composite sheet consists of a polycrystalline diamond layer, a continuous gradient transition layer, and a cemented carbide substrate from top to bottom, wherein the continuous gradient transition layer consists of diamond and cemented carbide, a content of the cemented carbide in the continuous gradient transition layer decreases from 100% to 0, and a content of the diamond increases from 0 to 100%, along a direction from the cemented carbide substrate to the polycrystalline diamond layer.

### Claim 2 (depends on 1)

The polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 1, wherein the cemented carbide is WC—Co, a mass fraction of Co is 3 to 20%, and a mass fraction of WC is 80% to 97%.

### Claim 3 (depends on 1)

The polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 1, wherein a thickness of the continuous gradient transition layer is 0.1 mm to 3 mm.

### Claim 4 (depends on 1)

A preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 1, comprising:
mixing, granulating, and drawing sequentially a diamond micropowder and a binder A to obtain a diamond polymer composite filament material;
mixing, granulating, and drawing sequentially a WC powder, a Co powder, and a binder B to obtain a cemented carbide polymer composite filament material;
putting the diamond polymer composite filament material and the cemented carbide polymer composite filament material into two feed inlets of a 3D printer respectively;
controlling feeding speeds of two filament materials through a feeding system according to a model of the polycrystalline diamond composite sheet so that the two filament materials enter a mixing chamber individually or in different proportions;
obtaining a polycrystalline diamond composite sheet green body after being extruded through a nozzle to perform deposition printing; and
performing degreasing and synthesizing under a high temperature and a high pressure on the polycrystalline diamond composite sheet green body to obtain the polycrystalline diamond composite sheet with a gradient structure.

### Claim 5 (depends on 4)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 4, wherein
a mass ratio of the diamond micropowder and the binder A is 2:1 to 20:1;
a composition of the binder A is, in terms of a mass percentage, as follows: 20 to 65% of ethylene-vinyl acetate copolymer, 5 to 35% of polystyrene, 5 to 35% of styrene-butadiene block copolymer, 3 to 10% of dodecyltrimethylammonium chloride, and 1 to 5% of oleic acid; and
a diameter of the diamond polymer composite filament material is 1.65 to 1.85 mm.

### Claim 6 (depends on 4)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 4, wherein
a mass ratio of a sum of masses of the WC powder and the Co powder to the binder B is 2:1 to 20:1;
a composition of the binder B is, in terms of a mass percentage, as follows: 30 to 75% of styrene-butadiene block copolymer, 5 to 35% of polyurethane, 5 to 10% of polyvinyl butyral, 3 to 6% of acrylonitrile-butadiene-styrene copolymer, 3 to 6% of trimellitate, and 1 to 5% of stearic acid;
a diameter of the cemented carbide polymer composite filament material is 1.65 to 1.85 mm.

### Claim 7 (depends on 4)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 4, comprising:
setting a thickness end point of the cemented carbide substrate as a gradient starting point and setting a thickness end point of the continuous gradient transition layer as a gradient end point according to the model of the polycrystalline diamond composite sheet;
controlling the feeding system first so that only the cemented carbide polymer composite filament material enters the mixing chamber,
when reaching the gradient starting point, a proportion of the cemented carbide polymer composite filament material entering the mixing chamber decreases uniformly, and a proportion of the diamond polymer composite filament material entering the mixing chamber increases uniformly, according to a thickness of the continuous gradient transition layer; and
until the gradient end point is reached, only the diamond polymer composite filament material enters the mixing chamber.

### Claim 8 (depends on 7)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 7, wherein during the deposition printing, a position of the gradient starting point is 4 to 13 mm, a position of the gradient end point is 4.1 to 16 mm, a printing layer thickness is 0.05 to 0.3 mm, and a printing speed is 10 to 100 mm/s.

### Claim 9 (depends on 4)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 4, wherein the degreasing is performed under a vacuum condition, and a vacuum degree is 2.0×10−2 Pa to 8.0×10−4 Pa; and a temperature rising process is as the following: first, raising a temperature from a room temperature to 80° C. to 100° C. at 5 to 15° C./min and maintaining for 0.5 to 1 hour; next, raising temperature to 180° C. to 230° C. at 3 to 10° C./min and maintaining for 1 to 2.5 hours; then, raising temperature to 300° C. to 330° C. at 1 to 5° C./min and maintaining for 0.5 to 1.5 hour; and then, raising temperature to 400° C. to 430° C. at 1 to 5° C./min and maintaining for 0.5 to 1.5 hour; and finally, raising temperature to 550° C. to 620° C. at 2 to 6° C./min and maintaining for 0.5 to 1 hour, and then finally cooling with a furnace.

### Claim 10 (depends on 4)

The preparation method of the polycrystalline diamond composite sheet having the continuous gradient transition layer as claimed in claim 4, wherein during the synthesizing under the high temperature and the high pressure, a temperature is 1200° C. to 1800° C., a synthesis pressure is 4 to 8 GPa, and a temperature and pressure maintaining time is 100 s to 900 s.