# US 2025/0098553 A1 · Ferroelectric tunnel junction with multilevel switching

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0098553 A1
- Document ID: US20250098553A1
- Status: Published application
- Kind: A1
- Application number: 18/291,551
- Filed: 2022-07-21
- Published: 2025-03-20
- Earliest claimed: 2021-07-23
- Assignees: Intermolecular, Inc.
- Applicants: Intermolecular, Inc.
- Inventors: RAISUL ISLAM; MARIO LAUDATO; RUBEN WALDMAN
- Web page: https://patentgrep.com/patent/US20250098553A1

## CPC

- H10N 70/023: {by chemical vapor deposition, e.g. MOCVD, ALD}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10D 1/68: Capacitors having no potential barriers
- H10N 70/028: {by conversion of electrode material, e.g. oxidation}
- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/25: {based on bulk electronic defects, e.g. trapping of electrons}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/69395: {the material containing zirconium, e.g. ZrO2}
- H10P 14/69397: {the material containing two or more metal elements}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The disclosed and claimed subject matter relates to a ferroelectric tunnel junction that is BEOL compatible having a film comprising crystalline ferroelectric materials that include a mixture of hafnium oxide and zirconium oxide having a substantial (i.e., approximately 40% or more) or majority portion of the material in a ferroelectric phase as deposited (i.e., without the need for further processing, such as a subsequent capping or annealing) and methods for preparing and depositing these materials. An interfacial layer is formed by oxidizing one or more of a first electrode and a second electrode. The FTJ has a memory window of between about 2× and 10× and is stable over 4 resistance states for at least 10's. The FTJ is produced at temperatures less than or equal to 400 degrees Celsius.

## Claims

### Claim 1

A ferroelectric tunnel junction comprising:
a substrate;
a first electrode and a second electrode, wherein a portion of the first electrode or the second electrode has been oxidized to form an interfacial layer;
a film comprising crystalline material disposed between the first electrode and the second electrode, the crystalline material comprising hafnium oxide and zirconium oxide, wherein the crystalline material exhibits ferroelectric behavior as deposited, wherein the film has a thickness of approximately 0.2 nm to approximately 5 nm; and
a voltage source connected to the first electrode or the second electrode.

### Claim 2 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein the first electrode and the second electrode are independently selected from TIN, W, Ni, Ru, Pt, and Al.

### Claim 3 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein the first electrode and the second electrode are independently selected from TIN and W.

### Claim 4 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein the ferroelectric tunnel junction is capable of switching between at least 4 distinct resistive states.

### Claim 5 (depends on 4)

The ferroelectric tunnel junction of claim 4, wherein the at least four distinct resistive states are stable for at least 103 seconds.

### Claim 6 (depends on 1)

The ferroelectric tunnel junction of claim 1, having a memory window of between about 1.5× and about 10× in a DC domain.

### Claim 7 (depends on 1)

The ferroelectric tunnel junction of claim 1, having a memory window of between about 2× and about 5×.

### Claim 8 (depends on 1)

The ferroelectric tunnel junction of claim 1, capable of exhibiting ferroelectric activity.

### Claim 9 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein the first electrode comprises tungsten and the second electrode comprises titanium nitride.

### Claim 10 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein less than 50% of the total volume of the crystalline material constitutes a non-ferroelectric phase component.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein less than 4950% of the total volume of the crystalline material constitutes a monoclinic phase component.

### Claim 13 (depends on 12)

The ferroelectric tunnel junction of any claim 12, wherein less than 6040% of the total volume of the crystalline material constitutes a monoclinic phase component.

### Claim 14

(canceled)

### Claim 15 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein a molar ratio of hafnium oxide to zirconium oxide is between approximately 1:3 and approximately 3:1.

### Claim 16 (depends on 1)

The ferroelectric tunnel junction of claim 1, wherein the crystalline material has a carbon content below approximately 6 atomic percent.

### Claim at position 17

17-50. (canceled)

### Claim 51

A method of creating a ferroelectric tunnel junction comprising:
(i) providing a substrate;
(ii) depositing a first electrode onto the substrate;
(iii) pulsing a plasma comprising oxygen and ozone to oxidize a portion of the first electrode to form an interfacial layer;
(iv) depositing a ferroelectric layer onto the first electrode at a deposition temperature, the step of depositing the ferroelectric layer comprising:
(a) exposing the first electrode to a first precursor that does not decompose at the deposition temperature;
(b) exposing the substrate to a first reaction gas;
(c) exposing the substrate to a second precursor that does not decompose at the deposition temperature; and
(d) exposing the substrate to a second reaction gas,
wherein one of the first precursor and the second precursor comprises zirconium and the other of the first precursor and the second precursor comprises hafnium; and
(v) depositing a second electrode onto the ferroelectric layer.

### Claim 52 (depends on 51)

The method of claim 51, wherein the first reaction gas and the second reaction gas are each independently a gas containing one or more of oxygen, water, hydrogen peroxide and nitrous oxide.

### Claim 53 (depends on 51)

The method of claim 51, wherein the first reaction gas and the second reaction gas are each independently a gas containing oxygen, a gas containing ozone, or a gas containing water.

### Claim 54 (depends on 51)

The method of claim 51, wherein an annealing step is conducted at a temperature greater than or equal to about 350 degrees Celsius.

### Claim 55 (depends on 51)

The method of claim 51, wherein no process steps take place at a temperature greater than about 400 degrees Celsius.

### Claim 56 (depends on 51)

The method of claim 51, wherein no interfacial layer is deposited between the ferroelectric layer and the first electrode or between the ferroelectric layer and the second electrode.

### Claim 57 (depends on 51)

The method of claim 51, wherein the first reaction gas or the second reaction gas comprises ozone delivered a volumetric fraction of between about 2% and about 50%.

### Claim 58 (depends on 51)

The method of claim 51, further comprising an ozone pulsing step prior to depositing the second electrode.

### Claim 59 (depends on 51)

The method of claim 51, wherein the ozone pulsing step delivers a gas stream comprising between about 2% and about 50% of ozone by volume.

### Claim 60 (depends on 51)

The method of claim 51, wherein the ferroelectric layer exhibits remanent polarization without additional thermal processing.

### Claim 61 (depends on 51)

The method of claim 51, wherein the deposited ferroelectric I has a remanent polarization (Pr) of greater than 8 μC/cm2 or a total loop opening of greater than 16 μC/cm2.

### Claim 62 (depends on 51)

The method of claim 51, wherein the first electrode comprises TiN and the interfacial layer comprises TiOxNy, wherein x and y are integers.

### Claim 63 (depends on 51)

The method of claim 51, wherein the first electrode comprises Tungsten (W) and the interfacial layer comprises WOx, wherein x is a non-negative integer.

### Claim 64 (depends on 51)

The method of claim 51, wherein the first electrode comprises Ruthenium (Ru) and the interfacial layer comprises RuOx, wherein x is a non-negative integer.

### Claim 65 (depends on 51)

The method of claim 51, wherein the first electrode comprises tungsten and the second electrode comprises titanium nitride.

### Claim 66 (depends on 54)

The method of claim 54, wherein the annealing step is conducted at a temperature lower than or equal to about 400 degrees Celsius.

### Claim 67

(canceled)

### Claim 68

(canceled)

### Claim 69

(canceled)

### Claim 70 (depends on 1)

The ferroelectric tunnel junction of claim 1 having a critical dimension of about 300 nm or less.