# US 2025/0098411 A1 · Method for preparing pixel define layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0098411 A1
- Document ID: US20250098411A1
- Status: Published application
- Kind: A1
- Application number: 18/891,816
- Filed: 2024-09-20
- Published: 2025-03-20
- Earliest claimed: 2023-09-20
- Assignees: Duk San Neolux Co., Ltd.
- Applicants: Duk San Neolux Co., Ltd.
- Inventors: Jun BAE; Jun Ki KIM; Kyung Soo KIM; Changmin LEE; Yeon Soo LEE; Jin Hyun KIM; Hanwook SEO; Ju Cheol KWON; Seo Jeong JEON; Hak Young LEE; Soung Yun MUN
- Web page: https://patentgrep.com/patent/US20250098411A1

## CPC

- H10K 59/1201: {Manufacture or treatment}
- H10K 59/122: Pixel-defining structures or layers, e.g. banks
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

Provided is a method for ensuring vivid colors and increasing display reliability and lifespan by implementing a colored pattern with high optical density on an electrode substrate, where the method uses a pigment dispersion in which a pigment having a size of 100 nm or less is used in order to increase the optical density and reduce roughness after completing the post-heat treatment process by including a colorant according to the present disclosure, and the method can minimize the reduction in the lifespan due to moisture in the panel state by minimizing the moisture content after completing the post-heat treatment process.

## Claims

### Claim 1

A method for preparing a pixel defining layer, the method comprising steps of: applying and coating a photosensitive resin composition containing a colorant having a mean pigment particle size of 100 nm or less; performing prebaking; performing exposure; performing development; and performing post-heat treatment, wherein after the post-heat treatment step, the moisture content of the coating film is 50 ppm or less, the optical density is 0.8/μm to 2.0/μm, the roughness is 3.0 nm or less, and there is no residue.

### Claim 2 (depends on 1)

The method of claim 1, wherein the oven temperature of the post-heat treatment step is 210 to 300° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the oven temperature of the post-heat treatment step is 250 to 270° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the post-heat treatment step is performed for 30 to 120 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the post-heat treatment step is performed for 60 to 120 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the optical density of the coating film after the post-heat treatment is 0.9/μm to 1.5/μm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the roughness of the coating film after the post-heat treatment is 2.5 nm or less.

### Claim 8 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a colorant.

### Claim 9 (depends on 8)

The method of claim 8, wherein the colorant includes one or more of an inorganic dye, an organic dye, an inorganic pigment, and an organic pigment.

### Claim 10 (depends on 1)

The method of claim 1, wherein the colorant is contained in an amount of 1 to 40% by weight based on the total amount of the photosensitive resin composition.

### Claim 11 (depends on 1)

The method of claim 1, wherein the colorant is pretreated using: a dispersant; or a water-soluble inorganic salt and a wetting agent.

### Claim 12 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a patterning resin which includes an acrylic binder resin, a cardo-based binder resin, or a combination thereof.

### Claim 13 (depends on 12)

The method of claim 12, wherein the acrylic binder resin has a weight average molecular weight of 3,000 g/mol to 150,000 g/mol.

### Claim 14 (depends on 12)

The method of claim 12, wherein the cardo-based resin has a weight average molecular weight of 1,000 to 100,000 g/mol.

### Claim 15 (depends on 12)

The method of claim 12, wherein the cardo-based resin is contained in an amount of 1 to 30% by weight based on the total amount of the photosensitive resin composition.

### Claim 16 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a reactive unsaturated compound in an amount of 1 to 40% by weight based on the total amount of the photosensitive resin composition.

### Claim 17 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a photoinitiator in an amount of 0.01 to 10% by weight based on the total amount of the photosensitive resin composition.

### Claim 18 (depends on 1)

A pixel defining layer prepared by the preparation method according to claim 1.

### Claim 19 (depends on 18)

An organic light emitting display device comprising the pixel defining layer according to claim 18.

### Claim 20 (depends on 19)

An electronic device comprising the display device of claim 19 and a control unit for driving the display device.