# US 2025/0098205 A1 · Non-conformal oxide liner and manufacturing methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0098205 A1
- Document ID: US20250098205A1
- Status: Published application
- Kind: A1
- Application number: 18/967,154
- Filed: 2024-12-03
- Published: 2025-03-20
- Earliest claimed: 2018-05-18
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Ming-Ho Lin; Chun-Heng Chen; Xiong-Fei Yu; Chi On Chui
- Web page: https://patentgrep.com/patent/US20250098205A1

## CPC

- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method includes forming a fin protruding over a substrate; forming a conformal oxide layer over an upper surface and along sidewalls of the fin; performing an anisotropic oxide deposition or an anisotropic plasma treatment to form a non-conformal oxide layer over the upper surface and along the sidewalls of the fin; and forming a gate electrode over the fin, the conformal oxide layer and the non-conformal oxide layer being between the fin and the gate electrode.

## Claims

### Claim 1

A method comprising:
forming a fin protruding over a substrate;
forming isolation regions on opposing sides of the fin, wherein the fin protrudes above an upper surface of the isolation regions distal from the substrate;
forming a conformal oxide layer over an upper surface of the fin and along sidewalls of the fin;
forming a non-conformal oxide layer over the upper surface of the fin and along the sidewalls of the fin by performing an anisotropic oxide deposition process, wherein the non-conformal oxide layer extends continuously from a first sidewall of the fin to a second opposing sidewall of the fin, wherein the non-conformal oxide layer extends continuously from the upper surface of the fin to the isolation regions; and
forming a gate electrode over the fin, wherein the conformal oxide layer and the non-conformal oxide layer are between the fin and the gate electrode.

### Claim 2 (depends on 1)

The method of claim 1, wherein the non-conformal oxide layer has a first thickness at the upper surface of the fin and has a second thickness at the sidewalls of the fin, wherein the first thickness is larger than the second thickness.

### Claim 3 (depends on 2)

The method of claim 2, further comprising, after forming the gate electrode:
forming source/drain regions over the fin on opposing sides of the gate electrode;
forming a dielectric layer over the fin, over the source/drain regions, and around the gate electrode;
removing the gate electrode, the non-conformal oxide layer, and the conformal oxide layer to form a gate trench in the dielectric layer; and
forming a replacement gate structure in the gate trench over the fin.

### Claim 4 (depends on 1)

The method of claim 1, wherein the conformal oxide layer contacts and extends along the non-conformal oxide layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the conformal oxide layer is formed over the upper surface of the fin and along the sidewalls of the fin before the non-conformal oxide layer is formed.

### Claim 6 (depends on 1)

The method of claim 1, wherein the non-conformal oxide layer is formed over the upper surface of the fin and along the sidewalls of the fin before the conformal oxide layer is formed.

### Claim 7 (depends on 1)

The method of claim 1, wherein performing the anisotropic oxide deposition process comprises performing a plurality of deposition cycles, wherein each of the plurality of deposition cycles is performed by:
supplying, between a first time instant and a second time instant, a silicon precursor to a process chamber for the anisotropic oxide deposition process;
supplying an oxygen gas to the process chamber between the first time instant and a third time instant, wherein the second time instant is between the first time instant and the third time instant; and
activating, between a fourth time instant and a fifth time instant, the oxygen gas into a plasma by turning on a radio frequency (RF) power source, wherein the fourth time instant and the fifth time instant are between the second time instant and the third time instant.

### Claim 8 (depends on 7)

The method of claim 7, wherein the RF power source is turned on continuously between the fourth time instant and the fifth time instant.

### Claim 9 (depends on 7)

The method of claim 7, wherein the RF power source is turned on and off alternately between the fourth time instant and the fifth time instant.

### Claim 10 (depends on 7)

The method of claim 7, wherein forming the conformal oxide layer comprises performing a thermal oxidization process.

### Claim 11 (depends on 10)

The method of claim 10, wherein the thermal oxidization process is an in-situ steam generation (ISSG) process or a rapid thermal oxidization (RTO) process.

### Claim 12

A method comprising:
forming a fin protruding over a substrate;
performing an anisotropic plasma treatment to convert a first exterior portion of the fin along an upper surface of the fin and a second exterior portion of the fin along sidewalls of the fin into a non-conformal oxide layer, wherein the first exterior portion is thicker than the second exterior portion; and
forming a gate electrode over the fin, wherein the non-conformal oxide layer is between the fin and the gate electrode.

### Claim 13 (depends on 12)

The method of claim 12, further comprising before forming the gate electrode, forming a conformal oxide layer along the upper surface of the fin and along the sidewalls of the fin.

### Claim 14 (depends on 13)

The method of claim 13, wherein a first portion of the conformal oxide layer along the sidewalls of the fin physically contacts a second portion of the non-conformal oxide layer along the sidewalls of the fin.

### Claim 15 (depends on 13)

The method of claim 13, wherein the non-conformal oxide layer is formed along the upper surface of the fin and along the sidewalls of the fin before the conformal oxide layer is formed.

### Claim 16 (depends on 12)

The method of claim 12, wherein performing the anisotropic plasma treatment comprises:
supplying an oxygen gas to a process chamber for the anisotropic plasma treatment;
while the oxygen gas is being supplied to the process chamber, turning on a radio frequency (RF) power source for a first period of time to activate the oxygen gas into a plasma; and
turning off the RF power source after the first period of time elapses.

### Claim 17

A method comprising:
forming a fin protruding above a substrate;
forming a non-conformal gate dielectric layer over a top surface of the fin and along sidewalls of the fin, wherein the non-conformal gate dielectric layer has a first thickness over the top surface of the fin and has a second thickness along the sidewalls of the fin, the first thickness being different from the second thickness;
forming a dummy gate electrode over the fin and over the non-conformal gate dielectric layer;
forming a dielectric layer over the fin around the dummy gate electrode;
removing the dummy gate electrode and the non-conformal gate dielectric layer under the dummy gate electrode to form an opening in the dielectric layer; and
forming a replacement gate structure in the opening.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first thickness is larger than the second thickness.

### Claim 19 (depends on 18)

The method of claim 18, further comprising, before forming the dummy gate electrode, forming a conformal gate dielectric layer over the top surface of the fin and along the sidewalls of the fin, wherein the method further comprises removing the conformal gate dielectric layer before forming the replacement gate structure.

### Claim 20 (depends on 19)