# US 2025/0096421 A1 · Cylindrical lithium-ion cells with silicon-carbon composite anodes and a fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096421 A1
- Document ID: US20250096421A1
- Status: Published application
- Kind: A1
- Application number: 18/441,586
- Filed: 2024-02-14
- Published: 2025-03-20
- Earliest claimed: 2023-09-15
- Assignees: Rincell Corporation
- Applicants: Rincell Corporation
- Inventors: Jignesh Parikh; Jagjit Nanda; Lasantha Korala
- Web page: https://patentgrep.com/patent/US20250096421A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 50/469: tubular or cylindrical
- H01M 4/0435: {Rolling or calendering}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/362: {Composites}
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/622: {being polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0567: characterised by the additives
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 50/417: Polyolefins
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0065: Solid electrolytes
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed is a cylindrical lithium-ion cell with energy density of greater than 300 Wh/kg and greater than 850 Wh/L, and improved cycle life, charge/discharge rate, storage, and safety performances across a wide temperature range (−40° C. to +60° C.). The cylindrical lithium-ion cell includes a densified anode electrode and a densified cathode electrode separated by two separator layers (together termed as an electrode stack). The electrode stack is spirally wound and is infused with an electrolyte formulation. The electrode stack has less than or equal to 3% stack-level expansion at fully charged state. The densified anode electrode comprises a composite anode electrode active material with a predefined ratio of 52.6-100% silicon-carbon such that SixCy; x+y=1, where x ranges between 0.45-0.55 and 0-47.4% graphite, and fabricated with an anode electrode formulation and a fabrication method.

## Claims

### Claim 1

A cylindrical lithium-ion cell, comprising:
a densified anode electrode;
a densified cathode electrode;
two separator layers sandwiched between the densified anode electrode and the densified cathode electrode;
an electrolyte infiltrated into the densified anode electrode, the densified cathode electrode and the two separator layers, wherein the electrolyte facilitates movement of ions between cathode and anode; and
a cylindrical metal housing that houses the densified anode electrode, the densified cathode electrode, the two separator layers and the electrolyte,
wherein the densified anode electrode is prepared according to an anode electrode formulation comprising a composite anode electrode active material, a conductive additive mixture and a binder mixture,
wherein the composite anode electrode active material comprises a predefined ratio of 52.6-100% silicon-carbon composite SixCy; x+y=1, with x ranging between 0.45-0.55, and 0-47.4% graphite,
wherein the binder mixture is composed of 0-25% polyacrylic acid (PAA), 2.5-25% styrene-butadiene rubber (SBR), 2.5-25% carboxymethyl cellulose (CMC), and 0-25% alginate,
wherein the conductive additive mixture encompasses 0-25% graphene, 0-25% single-wall carbon nanotubes (CNT), and 0-50% carbon black,
the cylindrical lithium-ion cell has an energy density of greater than 300 Wh/kg and greater than 850 Wh/L and the electrode stack has ≤3% stack-level expansion at fully charged state.

### Claim 2 (depends on 1)

The cylindrical lithium-ion cell of claim 1, wherein the densified cathode comprises a mixture of 25-50% lithium nickel manganese cobalt oxide LiNixMnyCo1-x-yO2, 0.9<x<1 and 50-75% LiNixMnyCo1-x-yO2, 0.8<x<0.9 as active materials and coat density of >3.5 mg/cm3.

### Claim 3 (depends on 1)

The cylindrical lithium-ion cell of claim 1, wherein the two separator layers include inorganic coatings, wherein the inorganic coatings consist of ceramic or boehmite.

### Claim 4 (depends on 1)

The cylindrical lithium-ion cell of claim 1, wherein the electrolyte has conductivity >10.5 mS/cm at 25° C. and comprises a composition of a salt mixture of lithium salt, organic solvents, and salt-type additives to generate a stable solid electrolyte interface (SEI) designed for silicon anode material that undergoes substantial volume changes during cycling.

### Claim 5 (depends on 1)

The cylindrical lithium-ion cell of claim 1, wherein the cylindrical lithium-ion cell is an 18650-form factor cell with a discharge capacity of ≥4.1 Ah at 0.2 C discharge rate when discharge from 4.2 V to 2.5 V.

### Claim 6 (depends on 5)

The cylindrical lithium-ion cell of claim 5, wherein a discharge capacity yield at 3 C discharge rate is >87% when discharge from 4.2 V to 2.5 V.

### Claim 7 (depends on 5)

The cylindrical lithium-ion cell of claim 5, wherein the 18650-form factor cell can be charged at 3 C rate allowing 0% to 80% charge in less than 20 minutes.

### Claim 8 (depends on 5)

The cylindrical lithium-ion cell of claim 5, wherein the 18650-form factor cell can be cycled between lower and upper voltage of 2.5 V and 4.2 V, and at a charge rate of 2 C for >500 cycles before reaching the discharge capacity yield of 80% at 0.2 C discharge rate.

### Claim 9 (depends on 5)

The cylindrical lithium-ion cell of claim 5, wherein the 18650-form factor cell can be discharged at −40° C. at 0.2 C rate with capacity yield of >40% in the voltage window of 4.2 V to 2.5 V.

### Claim 10 (depends on 1)

The cylindrical lithium-ion cell of claim 1, wherein the cylindrical lithium-ion cell is a 21700-form factor cell with a discharge capacity of ≥5.8 Ah at 0.2 C discharge rate when discharge from 4.2 V to 2.5 V.

### Claim 11 (depends on 10)

The cylindrical lithium-ion cell of claim 10, wherein a discharge capacity yield at 3 C discharge rate is >87% when discharge from 4.2 V to 2.5 V.

### Claim 12 (depends on 10)

The cylindrical lithium-ion cell of claim 10, wherein the 21700-form factor cell can be charged at 3 C rate allowing 0% to 80% charge in less than 20 minutes.

### Claim 13 (depends on 10)

The cylindrical lithium-ion cell of claim 10, wherein the 21700-form factor cell can be cycled between lower and upper voltage of 2.5 V and 4.2 V, and at a charge rate of 2 C for >500 cycles before reaching the discharge capacity yield of 80% at 0.2 C discharge rate.

### Claim 14 (depends on 10)

The cylindrical lithium-ion cell of claim 10, wherein the 21700-form factor cell can be discharged at −40° C. at 0.2 C rate with capacity yield of >40% in the voltage window of 4.2 V to 2.5 V.

### Claim 15

A method for fabricating a densified anode electrode for a cylindrical lithium-ion cell, the method comprising:
preparing an anode electrode formulation comprising a composite anode electrode active material, a conductive additive mixture and a binder mixture;
preparing an anode electrode slurry with uniform dispersion of active materials, conductive additives, and binders according to the anode electrode formulation in water via utilization of industrial planetary mixers;
wherein the anode electrode formulation includes 93-95.9% of the composite anode electrode active material, the composite anode electrode active material including a predefined ratio of 52.6-100% silicon-carbon composite SixCy; x+y=1, with x ranging between 0.45-0.55, and 0-47.4% graphite;
wherein the anode electrode formulation includes 0.1-1% of the conductive additive mixture, the conductive additive mixture comprising graphene, single-wall carbon nanotubes (CNT), and carbon black, and combinations thereof;
wherein the anode electrode formulation includes 4-6% of the binder mixture comprises, the binders mixture comprising polyacrylic acid (PAA), styrene-butadiene rubber (SBR), carboxymethyl cellulose (CMC), alginate, and combinations thereof;
Coating the anode electrode slurry on both side of a current collector foil using slot-die coating;
oven drying the coating to form a porous anode electrode; and
performing a calendaring process for obtaining a densified anode electrode utilizing calendaring machines equipped with hydraulic servo type gap adjustment and double pressing.

### Claim 16 (depends on 15)

The method of claim 15, wherein the anode electrode slurry comprises dispersion of active materials, conductive additives, and binders according to the anode electrode formulation in water via utilization of industrial planetary mixers in the sequence of making binder solution (5-8% solid) and then adding/mixing of conductive additives and adjusting the PH to 8-10 followed by adding/mixing active material (35-40% solid) for minimizing the occurrence of agglomerates and obtaining appropriate rheological properties for slot-die coating and drying at >15 m/min.

### Claim 17 (depends on 16)

The method of claim 16, wherein loading of the densified anode electrode is at 3-8 mg/cm2.

### Claim 18 (depends on 15)

The method of claim 15, wherein the calendaring process employs a double-sided coated electrode rolls on a calendaring machine equipped with a constant pressure and gap adjustment mode.

### Claim 19 (depends on 18)

The method of claim 18, wherein the calendaring process produces the densified anode electrode with a density of 1.6-1.75 g/cm3 and porosity in the range of 25 to 30%.