# US 2025/0096414 A1 · Coating slurry, separator, preparation method for separator and battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096414 A1
- Document ID: US20250096414A1
- Status: Published application
- Kind: A1
- Application number: 18/961,298
- Filed: 2024-11-26
- Published: 2025-03-20
- Earliest claimed: 2022-05-27
- Assignees: Shenzhen Senior Technology Material Co., Ltd.; Senior Material Holding Company (Europe) AB
- Applicants: Shenzhen Senior Technology Material Co., Ltd.; Senior Material Holding Company (Europe) AB
- Inventors: Dandan YANG; Xiang PING; Huizhen HUANG; Yulin LIN
- Web page: https://patentgrep.com/patent/US20250096414A1

## CPC

- C09D 127/16: Homopolymers or copolymers of vinylidene fluoride
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- C09D 7/20: Diluents or solvents
- C09D 7/61: inorganic
- C09D 7/68: {Particle size between 100-1000 nm}
- C09D 179/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- H01M 10/052: Li-accumulators
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/417: Polyolefins
- H01M 50/42: Acrylic resins
- H01M 50/426: Fluorocarbon polymers
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/449: having a layered structure
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- C08K 5/17: Amines; Quaternary ammonium compounds
- C08K 5/45: Heterocyclic compounds having sulfur in the ring
- Y02E 60/10: Energy storage using batteries
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application provides a coating slurry, a separator, a preparation method, and a battery. Main components of the coating slurry include a solvent, an ultra-high heat-resistant polymer resin binder, an auxiliary binder, a cross-linking agent, and an inorganic filler. According to the present application, the heat resistance and breakage temperature of the separator are successfully improved at a low cost by using a simple formula, thereby greatly improving the safety of a battery.

## Claims

### Claim 1

A coating slurry, wherein main components of the coating slurry comprise a solvent, an ultra-high heat-resistant polymer resin binder, an auxiliary binder, a cross-linking agent and an inorganic filler.

### Claim 2 (depends on 1)

The coating slurry according to claim 1, wherein a melting point of the ultra-high heat-resistant polymer resin binder is 200° C. or more, an addition amount of the ultra-high heat-resistant polymer resin binder is 1-60 wt %, and the ultra-high heat-resistant polymer resin binder is selected from one or two of polyimide, ether anhydride polyimide, fluoroanhydride polyimide, ketone anhydride polyimide, bismaleimide oligomer, and alkenyl-terminated polyimide oligomer.

### Claim 3 (depends on 1)

The coating slurry according to claim 1, wherein an addition amount of the auxiliary binder is 1-20 wt %, and the auxiliary binder is selected from one or more of acrylate polymer, polyacrylic acid, polyurethane acrylate, polysiloxane methacrylate, polyvinylidene fluoride homopolymer, vinylidene fluoride-hexafluoropropylene copolymer, and polyvinylidene fluoride-tetrafluoroethylene-propylene terpolymer.

### Claim 4 (depends on 1)

The coating slurry according to claim 1, wherein an addition amount of the cross-linking agent is 0.001-6 wt %, and the cross-linking agent is selected from one or more of diethylenetriamine, ethylenediamine, 3,3′-dichloro-4,4′-diaminodiphenylmethane, m-phenylenediamine, diaminodiphenylmethane, isopropyl thioxanthone, benzophenone, and ethyl p-dimethylaminobenzoate.

### Claim 5 (depends on 1)

The coating slurry according to claim 1, wherein an addition amount of the inorganic filler is 1-70 wt %, and a particle diameter of the inorganic filler is 0.3-0.8 μm.

### Claim 6 (depends on 5)

The coating slurry according to claim 5, wherein the inorganic filler is selected from one or more of Al2O3, SiO2, TiO2, ZrO2, MgO, CaO, AlOOH, and SiC.

### Claim 7 (depends on 1)

The coating slurry according to claim 1, wherein the coating slurry is an organic-solvent coating slurry, and a solid content thereof is 7-20 wt %.

### Claim 8 (depends on 1)

The coating slurry according to claim 1, wherein the solvent is N-methylpyrrolidone.

### Claim 9 (depends on 1)

A separator, comprising the coating slurry according to claim 1 and a substrate, wherein the coating slurry is coated on at least one surface of the substrate and subjected to ultraviolet light radiation with set energy and set wavelength, to obtain an ultraviolet cross-linked separator.

### Claim 10 (depends on 9)

The separator according to claim 9, wherein a wavelength of ultraviolet light used is in a range of 210 nm-420 nm, an ultraviolet cross-linking time is 0.001 s-10 s, and a radiation light intensity is above 50 mj/cm2.

### Claim 11 (depends on 9)

The separator according to claim 9, wherein a thickness of the substrate is 5-20 μm.

### Claim 12 (depends on 9)

The separator according to claim 9, wherein the substrate is any one of polyolefin microporous separator, polyimide microporous separator, nonwoven separator, multilayer composite separator, ceramic coated separator, polymer coated separator.

### Claim 13 (depends on 1)

A separator, comprising a substrate and a coating layer located on at least one surface of the substrate, wherein the coating layer is formed by the coating slurry according to claim 1, and the separator has a breakage temperature greater than 180° C. and a breakdown voltage greater than 2.1 KV, and the breakdown voltage per unit thickness is greater than 5.1 KV/mil.

### Claim 14 (depends on 13)

The separator according to claim 13, wherein the breakage temperature of the separator is greater than 210° C. in a machine direction, and the breakage temperature of the separator is greater than 190° C. in a transverse direction.

### Claim 15 (depends on 9)

A preparation method for the separator according to claim 9, comprising the following steps:
S1, preparing a slurry: adding no more than 60 wt % of ultra-high heat-resistant polymer resin binder and 1-20 wt % of auxiliary binder into a solvent; after being fully dissolved, adding 1-70 wt % of inorganic filler and dispersing them evenly to obtain a premixed slurry; adding a cross-linking agent into a solvent and completely dissolving it to obtain a cross-linking agent solution; and adding the cross-linking agent solution into the premixed slurry, wherein an amount of the cross-linking agent is 0.001-6 wt % of a solid content of the premixed slurry, so as to obtain a slurry;
S2, coating: coating the slurry prepared above on at least one surface of a substrate;
S3, phase transformation: immersing the separator obtained after coating in a coagulation tank containing a mixed solution of a first solvent and a non-solvent to perform phase transformation;
S4, drying: washing and drying a product obtained in the above step S3, to obtain a composite separator;
S5, ultraviolet cross-linking: subjecting the composite separator to an ultraviolet light radiation for inducing a cross-linking reaction, to obtain an ultraviolet cross-linked composite separator.

### Claim 16 (depends on 15)

The preparation method according to claim 15, wherein a wavelength of ultraviolet light used is in a range of 210 nm-420 nm, an ultraviolet cross-linking time is 0.001 s-10 s, and a radiation light intensity is above 50 mj/cm2.

### Claim 17 (depends on 15)

The preparation method according to claim 15, wherein a ratio of the first solvent is 20-30 wt % based on a total mass of the first solvent and the non-solvent.

### Claim 18 (depends on 15)

The preparation method according to claim 15, wherein the step S1 further comprises adding an ultra-high heat-resistant polymer resin binder and an auxiliary binder to NMP solvent, and stirring continuously for 12 h-24 h at a temperature of 50-70° C. to obtain a premixed slurry.

### Claim 19 (depends on 9)

A battery, comprising a separator, a positive electrode, a negative electrode and an electrolyte, wherein the separator is the separator according to claim 9.