# US 2025/0096373 A1 · Cell pouch for secondary battery and its manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096373 A1
- Document ID: US20250096373A1
- Status: Published application
- Kind: A1
- Application number: 18/535,670
- Filed: 2023-12-11
- Published: 2025-03-20
- Earliest claimed: 2023-09-14
- Assignees: Dongwon Systems Corporation
- Applicants: Dongwon Systems Corporation
- Inventors: Eui Hwan SONG; Sung Gi YOON; Jong An KIM; Gyu Woon JUNG; Hyun Ah LEE; Seung Hyeon YEON
- Web page: https://patentgrep.com/patent/US20250096373A1

## CPC

- H01M 50/129: with two or more layers of only organic material
- H01M 50/105: Pouches or flexible bags
- H01M 50/121: Organic material
- H01M 50/124: having a layered structure
- H01M 50/126: comprising three or more layers
- H01M 50/131: characterised by physical properties, e.g. gas permeability, size or heat resistance
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

In a secondary battery, a cell pouch for a secondary battery according to the present invention comprises an inner resin layer, a barrier layer, and an outer resin layer, wherein the inner resin layer, the barrier layer, and the outer resin layer are sequentially laminated, wherein a content ratio of PER (Propylene Ethylene Rubber) in the inner resin layer is 10% or less. According to the present invention, the electrolyte peel strength of the secondary battery cell is improved to ensure excellence and reliability, as well as it is possible to use a cell pouch for a secondary battery with excellent conditions such as an electrolyte peeling strength of 1,000 (gf/15 mm) or more, due to the property, in which the electrolyte peel strength of the secondary battery cell is inversely proportional to the content ratio of PER in the inner resin layer and is proportional to the length of PER.

## Claims

### Claim 1

A cell pouch for a secondary battery comprising:
an inner resin layer;
a barrier layer; and
an outer resin layer,
wherein the inner resin layer, the barrier layer, and the outer resin layer are sequentially laminated,
wherein a content ratio of Propylene Ethylene Rubber (PER) in the inner resin layer is 10% or less.

### Claim 2 (depends on 1)

The cell pouch of claim 1, wherein a length of the PER of the inner resin layer is 0.3 μm or more, or the length of the PER compared to the content ratio of the PER is 3.0 (μm/%) or more.

### Claim 3 (depends on 1)

The cell pouch of claim 1, wherein an electrolyte peeling strength of the inner resin layer is 1,000 (gf/15 mm) or more.

### Claim 4 (depends on 1)

The cell pouch of claim 1, wherein the outer resin layer includes a first outer resin layer and a second outer resin layer sequentially laminated in the outer resin layer.

### Claim 5 (depends on 4)

The cell pouch of claim 4 further comprises,
a first surface treatment layer formed between the inner resin layer and the barrier layer; and
a second surface treatment layer formed between the barrier layer and the first outer resin layer.

### Claim 6 (depends on 5)

The cell pouch of claim 5 further comprises,
a first adhesive layer formed between the second surface treatment layer and the first outer resin layer; and
a second adhesive layer formed between the first outer resin layer and the second outer resin layer.

### Claim 7

A method for manufacturing a cell pouch for a secondary battery comprising:
placing an inner resin layer;
placing a barrier layer above the inner resin layer; and
placing the outer resin layer above the barrier layer,
wherein a content ratio of Propylene Ethylene Rubber (PER) of the inner resin layer is 10% or less.

### Claim 8 (depends on 7)

The method of claim 7, wherein a length of PER of the inner resin layer is 0.3 μm or more, or a length of the PER compared to a content ratio of the PER is 3.0 (μm/%) or more.

### Claim 9 (depends on 7)

The method of claim 7, wherein the outer resin layer includes a first outer resin layer and a second outer resin layer sequentially laminated in the outer resin layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein a first surface treatment layer is formed between the inner resin layer and the barrier layer, and a second surface treatment layer is formed between the barrier layer and the first outer resin layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein a first adhesive layer is formed between the second surface treatment layer and the first outer resin layer, and a second adhesive layer is formed between the first outer resin layer and the second outer resin layer.