# US 2025/0096329 A1 · Self-forming solid state batteries and self-healing solid electrolytes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096329 A1
- Document ID: US20250096329A1
- Status: Published application
- Kind: A1
- Application number: 18/968,877
- Filed: 2024-12-04
- Published: 2025-03-20
- Earliest claimed: 2017-06-09
- Assignees: The Regents of the University of California
- Applicants: The Regents of the University of California
- Inventors: Ping Liu; Byoung-Sun Lee; Xing Xing
- Web page: https://patentgrep.com/patent/US20250096329A1

## CPC

- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/40: Alloys based on alkali metals
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/587: for inserting or intercalating light metals
- H01M 10/052: Li-accumulators
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 10/0562: Solid materials
- H01M 10/058: Construction or manufacture
- H01M 2300/0017: Non-aqueous electrolytes
- H01M 2300/0065: Solid electrolytes
- H01M 2300/0082: Organic polymers
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Compositions, manufacturing processes, articles of manufacture, and structures/batteries for self-forming batteries and self-healing solid electrolytes are disclosed. Example embodiments include a self-forming battery. The battery may include a first electrode material and a second electrode material. Assembly of the two electrode materials may result in a chemical reaction that forms an electrolyte layer between the two electrode materials.

## Claims

### Claim 1

A method for producing a self-forming battery, the method comprising:
exposing a metal to a solution of an oxidant for a period of time;
rendering the metal free from solvents; and
attaching the metal to a conducting current collector.

### Claim 2 (depends on 1)

The method of claim 1, wherein the conducting current collector comprises at least one of Ti, Al, and C.

### Claim 3 (depends on 1)

The method of claim 1, further comprising obtaining a structure comprising the metal and an electrolyte, wherein the structure is used in combination with a cathode.

### Claim 4 (depends on 1)

The method of claim 1, further comprising exposing the metal with a thermal treatment comprising an electrochemical treatment where a cyclic current is applied to promote electrolyte layer growth.

### Claim 5 (depends on 1)

The method of claim 1, wherein the metal comprises a lithium (Li) metal.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solution comprises xLi2S1+y:P2S5, where x ranges from 1 to 5, and y ranges from 0 to 7.

### Claim 7 (depends on 6)

The method of claim 6, wherein x ranges from 7/3 to 3, and y ranges from 0 to 0.5.

### Claim 8 (depends on 1)

The method of claim 1, wherein the solvents comprise at least one of dimethyl ether, diethyl ether, dimethoxy ethane (DME), tetra ethylene glycol dimethyl ether (TEGDME) and diethylene glycol dimethyl ether (DEGDME).

### Claim 9 (depends on 1)

The method of claim 1, wherein the period of time comprises at least 5 days.