# US 2025/0096328 A1 · Method for manufacturing secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096328 A1
- Document ID: US20250096328A1
- Status: Published application
- Kind: A1
- Application number: 18/962,444
- Filed: 2024-11-27
- Published: 2025-03-20
- Earliest claimed: 2019-05-09
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Sung Tae KIM; Nak Gi SUNG; Joon Sup KANG
- Web page: https://patentgrep.com/patent/US20250096328A1

## CPC

- H01M 10/058: Construction or manufacture
- G01R 31/3865: {related to manufacture, e.g. testing after manufacture}
- G01R 31/388: involving voltage measurements
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/446: {Initial charging measures}
- G01R 31/392: Determining battery ageing or deterioration, e.g. state of health
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing a secondary battery includes a formation step for charging an assembled secondary battery to a state of charge (SOC) of 45% to 65%; an aging step for aging the secondary battery for which the formation has been completed; and a low voltage testing step for measuring the change in voltage value, wherein, in the low voltage testing step, a voltage value is measured in an SOC interval of 30% or lower. Since an SEI coating is stably formed in the method for manufacturing a secondary battery, charging time is shortened and thus the secondary battery can be mass-produced. In addition, since a low voltage test is performed in an interval in which the voltage change rate per capacity of a negative electrode is high, a low voltage defect due to non-uniformity of the formation process can be detected in the method for manufacturing the secondary battery.

## Claims

### Claim 1

A method for manufacturing a secondary battery, the method comprising:
a formation step of charging an assembled secondary battery to state of charge (SOC) 45% to 65% to provide a formed secondary battery;
an aging step of aging the formed secondary battery in the formation step to provide the secondary battery; and
a low voltage test step of measuring a change in a voltage value of the secondary battery,
wherein in the low voltage test step, the voltage value is measured in a section of SOC 30% or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the low voltage test step includes sorting out a defective secondary battery from a voltage drop amount.

### Claim 3 (depends on 1)

The method of claim 1, wherein, in the low voltage test step, a voltage drop amount is the voltage drop amount in a section of SOC 30% or less.

### Claim 4 (depends on 1)

The method of claim 1, wherein, in the formation step, charging and pressurizing of the assembled secondary battery are simultaneously performed.

### Claim 5 (depends on 1)

The method of claim 1, wherein the formation step is performed at a temperature of 30° C. to 65° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the aging step comprises a high temperature aging step, in which the formed secondary battery is stabilized at a temperature above 60° C.

### Claim 7 (depends on 1)

The method of claim 1, further comprising a room temperature aging step at a temperature of 20° C. to 30° C.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
a degassing step after the aging step, and
a full charge and full discharge step.

### Claim 9 (depends on 8)

The method of claim 8, further comprising a shipping charge step after the full charge and full discharge step.

### Claim 10 (depends on 1)

The method of claim 1, further comprising a pre-aging step of aging the assembled secondary battery at room temperature, before the formation step.