# US 2025/0096316 A1 · Wound-type all-solid-state lithium ion secondary battery and manufacturing method of wound-type all-solid-state lithium ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096316 A1
- Document ID: US20250096316A1
- Status: Published application
- Kind: A1
- Application number: 18/963,549
- Filed: 2024-11-28
- Published: 2025-03-20
- Earliest claimed: 2022-06-01
- Assignees: FUJIFILM Corporation; Institute of Science Tokyo
- Applicants: FUJIFILM Corporation; Institute of Science Tokyo
- Inventors: Yosuke SHIRATORI; Shintaro YASUI; Yasuharu SHIRAISHI; Kengo SAITO; Kenta WATANABE; Akihiro TAKAHASHI
- Web page: https://patentgrep.com/patent/US20250096316A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 2300/0068: inorganic
- H01M 2300/0071: Oxides
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a wound-type all-solid-state lithium ion secondary battery including a laminate in which a positive electrode layer, a solid electrolyte layer, and a negative electrode layer are arranged in this order, the laminate being wound around a core material, in which the solid electrolyte layer contains an amorphous solid electrolyte which contains a lithium-containing oxide containing Li, B, and O and a lithium salt, and in the amorphous solid electrolyte, a value of a ratio of a content of the lithium salt to a content of the lithium-containing oxide is 0.001 to 1.5 in terms of a molar ratio; and a manufacturing method of the wound-type all-solid-state lithium ion secondary battery.

## Claims

### Claim 1

A wound-type all-solid-state lithium ion secondary battery comprising:
a laminate in which a positive electrode layer, a solid electrolyte layer, and a negative electrode layer are arranged in this order, the laminate being wound around a core material,
wherein the solid electrolyte layer contains an amorphous solid electrolyte which contains a lithium-containing oxide containing Li, B, and O and a lithium salt, and in the amorphous solid electrolyte, a value of a ratio of a content of the lithium salt to a content of the lithium-containing oxide is 0.001 to 1.5 in terms of a molar ratio.

### Claim 2 (depends on 1)

The wound-type all-solid-state lithium ion secondary battery according to claim 1,
wherein, in the amorphous solid electrolyte, a value of a ratio of a content of water to the content of the lithium-containing oxide is 12 or less in terms of a molar ratio.

### Claim 3 (depends on 2)

The wound-type all-solid-state lithium ion secondary battery according to claim 2,
wherein, in the amorphous solid electrolyte, the value of the ratio of the content of the water to the content of the lithium-containing oxide is 1 to 12 in terms of a molar ratio.

### Claim 4 (depends on 1)

The wound-type all-solid-state lithium ion secondary battery according to claim 1,
wherein the lithium-containing oxide includes Li2+xB4+yO7+z,
where −0.3<x≤0.3, −0.3<y<0.3, and −0.3<z<0.3.

### Claim 5 (depends on 1)

The wound-type all-solid-state lithium ion secondary battery according to claim 1,
wherein the lithium salt is represented by Formula (1),
LiN(Rf1SO2)(Rf2SO2) Formula (1)
in the formula, Rf1 and Rf2 each independently represent a halogen atom or a perfluoroalkyl group.

### Claim 6 (depends on 1)

The wound-type all-solid-state lithium ion secondary battery according to claim 1,
wherein, in the amorphous solid electrolyte, in a case where a molar amount of B is set to 4.00, a molar amount of Li is 1.58 to 3.49, a molar amount of O is 6.23 to 25.00, and molar amounts of elements other than B, Li, and O are each 0.001 to 10.00.

### Claim 7 (depends on 1)

The wound-type all-solid-state lithium ion secondary battery according to claim 1,
wherein the lithium-containing oxide is a lithium-containing oxide subjected to a mechanical milling treatment.

### Claim 8

A wound-type all-solid-state lithium ion secondary battery comprising:
a laminate in which a positive electrode layer, a solid electrolyte layer, and a negative electrode layer are arranged in this order, the laminate being wound around a core material,
wherein the solid electrolyte layer contains an amorphous solid electrolyte containing Li, B, and O, and in the amorphous solid electrolyte, in a case where a molar amount of B is set to 4.00, a molar amount of Li is 1.58 to 3.49, a molar amount of O is 6.23 to 25.00, and molar amounts of elements other than Li, B, and O are each 0.001 to 10.00.

### Claim 9 (depends on 1)

A manufacturing method of the wound-type all-solid-state lithium ion secondary battery according to claim 1, comprising:
performing formation of the laminate under a condition in which the solid electrolyte layer is brought into contact with moisture.

### Claim 10 (depends on 8)

A manufacturing method of the wound-type all-solid-state lithium ion secondary battery according to claim 8, comprising:
performing formation of the laminate under a condition in which the solid electrolyte layer is brought into contact with moisture.